Abstract
The influence of chloride deposition on the formation, evolution and barrier properties of the patina formed on Cu5Zn5Al1Sn used for architectural cladding is explored via long-term marine field exposures and laboratory investigations. The presence of Cu2O, ZnO, Al2O3 and SnO2 within the inner part of the patina and intercalation of SnO2, Zn5(CO3)2(OH)6, Zn6Al2(OH)16CO3·4H2O, Zn5(OH)8Cl2·H2O within its outer part, predominantly composed of Cu2(OH)3Cl, significantly reduce the chloride-induced corrosion compared with Cu metal. The intercalation of zinc-rich corrosion products within the patina and not at the top-surface explain their marginal influence on the runoff process that mainly occurs at the outmost surface.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metallurgy and Material Science · Corrosion Behavior and Inhibition · Nanoporous metals and alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (70)
Show source-provided references
1. Atmospheric corrosion of copper and the colour, structure and composition of natural patinas on copper10.1016/j.corsci.2005.09.011 ↗
2. Copper patinas formed in the atmosphere-II. A qualitative assessment of mechanisms10.1016/0010-938X(87)90053-9 ↗
3. Atmospheric corrosion of copper in a rural atmosphere10.1149/1.2048399 ↗
4. Some aspects of the atmospheric corrosion of copper in the presence of sodium chloride10.1149/1.1838422 ↗
5. In situ studies of the initial atmospheric corrosion of copper influence of humidity, sulfur dioxide, ozone, and nitrogen dioxide10.1149/1.1393566 ↗
6. The evolution of outdoor copper patina10.1016/S0010-938X(01)00081-6 ↗
7. Copper and copper alloys
8. Corrosion and runoff rates of Cu and three Cu-alloys in marine environments with increasing chloride deposition rate10.1016/j.scitotenv.2013.11.080 ↗
9. Corrosion-induced copper runoff from naturally and pre-patinated copper in a marine environment10.1016/j.corsci.2006.04.004 ↗
10. A survey of argentinean atmospheric corrosion: II—Copper samples10.1016/S0010-938X(96)00150-3 ↗
11. Effect of carbon dioxide on sodium chloride-induced atmospheric corrosion of copper10.1149/1.2098327 ↗
12. Mechanistic studies of corrosion product flaking on copper and copper-based alloys in marine environments10.1016/j.corsci.2014.03.028 ↗
13. The characterization of a corroded egyptian bronze statue and a study of the degradation phenomena
14. A review of copper chlorides and related salts in bronze corrosion and as painting pigments10.1179/sic.2000.45.1.39 ↗
15. Chase · 1994
16. Electrochemical and spectroscopic characterizations of patinas formed on an archaeological bronze coin10.1016/j.electacta.2005.01.050 ↗
17. The characterization of Sn-based corrosion products in ancient bronzes: a Raman approach10.1002/jrs.4037 ↗
18. Initial oxidation of brass induced by humidified air10.1016/j.apsusc.2011.09.080 ↗
19. Atmospheric corrosion of brass in outdoor applications: patina evolution, metal release and aesthetic appearance at urban exposure conditions10.1016/j.scitotenv.2011.09.083 ↗
20. The protective nature of passivation films on zinc: wetting and surface energy10.1016/j.corsci.2004.01.001 ↗
21. The protective role of hydrozincite during initial corrosion of a Cu40Zn alloy in chloride-containing laboratory atmosphere10.1016/j.corsci.2015.10.027 ↗
22. The corrosion of nickel-aluminium bronzes in seawater—I. Protective layer formation and the passivation mechanism10.1016/0010-938X(93)90017-B ↗
23. The corrosion of nickel-aluminium bronzes in seawater—II. The corrosion mechanism in the presence of sulphide pollution10.1016/0010-938X(93)90018-C ↗
24. Tarnishing and Cu ion release in selected copper-base alloys: implications towards antimicrobial functionality10.1016/j.electacta.2015.04.001 ↗
25. The fate of copper during corrosion of Cu-5Zn-5Al-1Sn (89% Cu 5% Zn, 5% Al, 1% Sn) compared to copper in cynthetic perspiration solution10.5006/1885 ↗
26. Corrosion of cu-5Zn-5Al-1Sn (89% Cu, 5% Zn, 5% Al, 1% Sn) compared to copper in synthetic perspiration during cyclic wetting and drying: the fate of copper10.5006/2063 ↗
27. The golden alloy Cu-5Zn-5Al-1Sn: a multi-analytical surface characterization10.1016/j.corsci.2017.11.014 ↗
28. 2012
29. Atmospheric corrosion of Galfan coatings on steel in chloride-rich environments10.1016/j.corsci.2013.03.025 ↗
30. Effect of sodium chloride particles on the atmospheric corrosion of pure copper10.5006/1.3299244 ↗
31. A comparison between corrosion rates and runoff rates from new and aged copper and zinc as roofing material10.1023/A:1017547903442 ↗
32. 2012
33. 2012
34. Simultaneous infrared reflection absorption spectroscopy and quartz crystal microbalance measurements for in situ studies of the metal/atmosphere interface10.1149/1.1837948 ↗
35. Colour measurements on patinas and coating system for outdoor bronze monuments10.1016/j.culher.2006.03.001 ↗
36. Reflectance curves and CIE L* a* b* parameters to describe patina characteristics and corrosion mechanism on bronze alloys
37. Leygraf · 2016
38. A critical review on corrosion and runoff from zinc and zinc-based alloys in atmospheric environments10.5006/2458 ↗
39. Spatial distribution and formation of corrosion products in relation to zinc release for zinc sheet and coated pre-weathered zinc at an urban and a marine atmospheric condition10.1002/maco.201106361 ↗
40. Raman investigation of artificial patinas on recent bronze?part II: urban rain exposure10.1002/jrs.4124 ↗
41. Raman spectroscopy of selected copper minerals of significance in corrosion10.1016/S1386-1425(02)00315-3 ↗
42. Structural characterization of phase transition of Al2O3 nanopowders obtained by polymeric precursor method10.1016/j.matchemphys.2007.02.046 ↗
43. Synthesis and characterization of Ni–Al2O3 composite coatings containing different forms of alumina10.1007/s10800-010-0198-3 ↗
44. Spectral studies of SnO2 nanofibres prepared by electrospinning method10.1016/j.saa.2005.07.007 ↗
45. Combined effects of gaseous pollutants and sodium chloride particles on the atmospheric corrosion of copper10.5006/1.3280618 ↗
46. IR characteristics of hydrotalcite-like compounds10.1007/BF00348744 ↗
47. The effects of synthesis pH and hydrothermal treatment on the formation of zinc aluminum hydrotalcites10.1016/j.jssc.2004.07.010 ↗
48. FT-Raman and FT-IR spectroscopic study of synthetic Mg/Zn/Al-hydrotalcites10.1002/jrs.1244 ↗
49. Corrosion product formation on Zn55Al coated steel upon exposure in a marine atmosphere10.1016/j.corsci.2010.11.004 ↗
50. Thermo-Raman spectroscopy of selected layered double hydroxides of formula Cu6Al2(OH)16CO3 and Zn6Al2(OH)16CO310.1002/jrs.2148 ↗
51. Corrosion behaviour of Zn–Al–Mg coated steel sheet in sodium chloride-containing environment10.1016/j.corsci.2009.06.019 ↗
52. Synthesis and vibrational spectroscopic characterisation of synthetic hydrozincite and smithsonite10.1016/j.poly.2007.07.002 ↗
53. Characterization of corrosion products of Zn and Zn–Mg–Al coated steel in a marine atmosphere10.1016/j.corsci.2014.06.017 ↗
54. Reaction sequences in atmospheric corrosion of zinc
55. Corrosion and corrosion products of hot dipped galvanized steel during long term atmospheric exposure at different sites world-wide10.1016/j.corsci.2017.06.025 ↗
56. Understanding corrosion via corrosion product characterization: II. Role of alloying elements in improving the corrosion resistance of Zn–Al–Mg coatings on steel10.1016/j.corsci.2011.03.016 ↗
57. In situ infrared reflection spectroscopy studies of the initial atmospheric corrosion of Zn–Al–Mg coated steel10.1016/j.corsci.2013.03.005 ↗
58. Initial NaCl-particle induced atmospheric corrosion of zinc—effect of CO2 and SO210.1016/j.corsci.2007.06.005 ↗
59. Formation of NaZn4Cl(OH)6SO4· 6H2O in a marine atmosphere10.1016/0010-938X(93)90082-R ↗
60. Raman and infrared spectroscopic study of the basic copper chloride minerals −implications for the study of the copper and brass corrosion and bronze disease
61. Initial stages of indoor atmospheric corrosion of electronics contact metals in humid tropical climate: tin and nickel10.3989/revmetalm.2007.v43.i2.56 ↗
62. Non-destructive surface analysis applied to atmospheric corrosion of tin10.1002/sia.1281 ↗
63. Evolution of patinas on copper exposed in a suburban area10.1016/j.corsci.2006.05.044 ↗
64. In situ infrared reflection absorption spectroscopy studies of confined zinc surfaces exposed under periodic wet-dry conditions10.1149/1.1359397 ↗
65. The atmospheric corrosion of quaternary bronzes: the leaching action of acid rain10.1016/j.corsci.2008.10.008 ↗
66. Electrochemical evaluation of the corrosion protection of bi-dimensional organic films self-assembled onto brass10.1016/j.electacta.2004.01.058 ↗
67. Quantitative in situ analysis of initial atmospheric corrosion of copper induced by acetic acid10.1149/1.2715315 ↗
68. Critical review: copper runoff from outdoor copper surfaces at atmospheric conditions10.1021/es404410s ↗
69. Impedance spectroscopy: models, data fitting, and analysis10.1016/j.ssi.2004.05.035 ↗
70. Impedance and XPS study of benzotriazole films formed on copper, copper?zinc alloys and zinc in chloride solution10.1016/j.corsci.2008.04.016 ↗