Isothermal oxidation of the Ti2AlC MAX phase coatings deposited by kerosene-fuelled HVOF spray
Source abstract
Abstract
Abstract Isothermal oxidation of 100 μm Ti2AlC coatings deposited by kerosene-fuelled high velocity oxy-fuel spray have been carried out between 200 and 1000 °C for 5 h at 200 °C intervals. The development of coating’s crystalline phase, surface morphology and cross-sectional microstructure with respect to oxidation temperature has been investigated by X-ray diffraction with Rietveld phase analysis, optical microscope and scanning electron microscope. The coating maintained its phase composition and morphology till 400 °C, but was severely oxidized at 600 °C and above. A good temperature window for Ti2AlC would be below 1000 °C and avoid direct oxidation at 600 °C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: MXene and MAX Phase Materials · Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Layered machinable ceramics for high temperature applications10.1016/S1359-6462(96)00418-6 ↗
2. The Mn+1AXn phases: a new class of solids; thermodynamically stable nanolaminates10.1016/S0079-6786(00)00006-6 ↗
3. Processing and characterization of Ti2AlC, Ti2AlN, and Ti2AlC0.5N0.510.1007/s11661-006-0243-3 ↗
4. The Mn+1AXn phases: materials science and thin-film processing10.1016/j.tsf.2009.07.184 ↗
5. High-temperature oxidation behavior of Ti2AlC in air10.1023/A:1023092027697 ↗
6. Investigations on radiation tolerance of Mn+1AXn phases: study of Ti3SiC2, Ti3AlC2, Cr2AlC, Cr2GeC, Ti2AlC, and Ti2AlN10.1111/jace.13450 ↗
7. Cold spray deposition of Ti2AlC coatings for improved nuclear fuel cladding10.1016/j.jnucmat.2015.06.028 ↗
8. Ti2AlC coatings deposited by high velocity oxy-fuel spraying10.1016/j.surfcoat.2008.06.184 ↗
9. Microindentation and inverse analysis to characterize elastic-plastic properties for thermal sprayed Ti2AlC and NiCoCrAlY10.1007/s11666-009-9310-9 ↗
10. Microstructure of high velocity oxy-fuel sprayed Ti2AlC coatings10.1007/s10853-010-4263-4 ↗
11. Annealing of thermally sprayed Ti2AlC coatings10.1111/j.1744-7402.2010.02569.x ↗
12. In situ diffraction study of thermal decomposition in maxthal Ti2AlC10.1016/j.jallcom.2010.09.019 ↗
13. Cold spraying of Ti2AlC max-phase coatings10.1007/s11666-012-9843-1 ↗
14. Thermally sprayed Ti3SiC2 and Ti2AlC MAX-phase coatings
15. Kinetic aspects of Ti2AlC MAX phase oxidation10.1007/s11085-015-9526-7 ↗
16. Probing the oxidation behavior of Ti2AlC MAX phase powders between 200 and 1000 °C10.1016/j.jeurceramsoc.2016.08.004 ↗
17. Plasma spray of Ti2AlC MAX phase powders: effects of process parameters on coatings’ properties10.1016/j.surfcoat.2017.07.006 ↗
18. Kerosene-fuelled High velocity oxy-fuel (HVOF) spray of Ti2AlC MAX phase powders10.1016/j.jallcom.2017.11.157 ↗
19. Long-term oxidation of Ti2AlC in air and water vapor at 1000–1300 °C temperature range10.1149/2.052202jes ↗
20. Fauchais · 2014
21. Cold-spray deposition of Ti2AlC coatings10.1016/j.vacuum.2013.01.023 ↗
22. Oxidation of Ti2AlC bulk and spray deposited coatings10.1016/j.corsci.2010.08.004 ↗
23. Intermediate-temperature oxidation behavior of Ti2AlC in air10.1557/JMR.2002.0431 ↗
24. Microstructural evolution during high-temperature oxidation of Ti2AlC ceramics10.1016/j.actamat.2011.03.035 ↗
25. Oxidation of Tin+1AlXn (n = 1–3 and x = C, N) - II. Experimental results10.1149/1.1380256 ↗
26. Oxidation behavior of Ti3AlC2 powders in flowing air10.1039/b203644d ↗
27. Oxidation behavior of Ti3AlC2 at 1000–1400 °C in air10.1016/S0010-938X(02)00177-4 ↗
28. Oxidation of TiC at Low temperatures10.1007/BF01107214 ↗
29. Microstructure and residual stress of alumina scale formed on Ti2AlC at high temperature in air10.1007/s11085-007-9063-0 ↗
30. A critical review of the oxidation of Ti2AlC, Ti3AlC2 and Cr2AlC in air10.1080/21663831.2013.806364 ↗
31. Phase stability and initial low-temperature oxidation mechanism of Ti2AlC thin films10.1016/j.jeurceramsoc.2012.09.003 ↗
32. Oxidation behaviour of Ti-Al-C films composed mainly of a Ti2AlC phase10.1016/j.corsci.2011.05.033 ↗
33. Oxidation of Tin+1AlXn (n = 1–3 and X = C, N) - I. Model10.1149/1.1380255 ↗
34. High temperature healing of Ti2AlC: on the origin of inhomogeneous oxide scale10.1016/j.scriptamat.2011.03.031 ↗
35. Oxidation-induced crack healing in Ti3AlC2 ceramics10.1016/j.scriptamat.2007.09.006 ↗
36. Microstructural evolution during high-temperature oxidation of spark plasma sintered Ti2AlN ceramics10.1016/j.actamat.2011.11.010 ↗
37. TEM study of the initial oxide scales of Ti2AlC10.1016/j.actamat.2011.04.058 ↗
38. Phase stability of Ti2AlC upon oxygen incorporation: a first-principles investigation10.1103/PhysRevB.81.024111 ↗