journal article·2020-06

Enhanced oxidation and corrosion inhibition of 1Cr11Ni2W2MoV stainless steel by nano-modified silicone-based composite coatings at 600°C

Yao Du, Cheng Wang, Lanlan Yang, Shenglong Zhu, Fuhui Wang

Corrosion Science· Volume 169
Publisher page

Abstract

Abstract Silicone-based composite coatings modified by ZrO2 nanoparticles were applied on the 1Cr11Ni2W2MoV steel. Their oxidation and corrosion performances were evaluated in air and an environment containing solid NaCl and water vapor at 600 °C, respectively. The coating with 20 wt.% ZrO2 exhibited better oxidation resistance than those with 10 and 30 wt.% ZrO2, while the coating with 20 or 30 wt.% ZrO2 exhibited better resistance against the corrosion induced by water vapor and solid NaCl deposits than those with 10 wt.% ZrO2.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Corrosion Behavior and Inhibition · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (59)

Show source-provided references
1. High temperature oxidation behavior of silicon carbide-carbon coated nanostructured ferritic alloy composites in air + water vapor environment10.1016/j.corsci.2018.05.008 ↗
2. Effect of water vapour on the oxidation of Fe-13Cr-5Ni martensitic alloy at 973 K10.1016/j.corsci.2012.04.008 ↗
3. Study on corrosion kinetics of 310H in different simulated MSW combustion environment, the influence of SO2 and H2O on NaCl assisted corrosion10.1016/j.corsci.2019.04.013 ↗
4. Initial oxidation mechanisms of stainless steel Sanicro 28 (35Fe27Cr31Ni) exposed to KCl, NaCl, and K2CO3 under dry and humid conditions at 535 °C10.1016/j.corsci.2019.04.010 ↗
5. KCl Induced corrosion of a 304-type austenitic stainless steel at 600°C, the role of potassium10.1007/s11085-005-5704-3 ↗
6. Oxidation behavior of Fe-20Cr-25Ni-Nb austenitic stainless steel in high-temperature environment with small amount of water vapor10.1016/j.corsci.2018.09.016 ↗
7. Corrosion behavior of a sputtered K38G nanocrystalline coating with a solid NaCl deposit in wet oxygen at 600 to 700°C10.1023/A:1016072726338 ↗
8. Effect of water drops on the oxidation mechanisms of a ceria coated nickel-based superalloy10.1016/j.corsci.2012.11.010 ↗
9. NaCl induced corrosion of Ti-6Al-4V alloy at high temperature10.1016/j.corsci.2016.04.016 ↗
10. Synergistic corrosion behavior of coated Ti60 alloys with NaCl deposit in moist air at elevated temperature10.1016/j.corsci.2007.06.007 ↗
11. Oxidation and H2O/NaCl-induced corrosion behavior of sputtered Ni-Si coatings on Ti6A14V at 600-650 degrees C10.1016/j.surfcoat.2007.02.022 ↗
12. The effect of Hf on the oxidation and corrosion behavior of Ti0.7Al0.3N coating prepared by arc-ion plating10.1007/s11085-008-9129-7 ↗
13. Comparison of the oxidation behavior of a zirconium nitride coating in water vapor and air at high temperature10.1016/j.corsci.2018.04.015 ↗
14. Synergistic effect of NaCl and water vapor on the corrosion of 1Cr-11Ni-2W-2Mo-V steel at 500 - 700°C10.1023/A:1018854202982 ↗
15. Self-healing mechanisms in smart protective coatings: a review10.1016/j.corsci.2018.08.005 ↗
16. Degradation behaviour of a composite material for thermal protection systems, part I experimental characterization10.1023/A:1004399923891 ↗
17. The degradation of silicone coatings in high temperature atmospheres10.1108/00035599810236504 ↗
18. The thermogravimetric analysis of some polysiloxanes10.1016/S0141-3910(97)00135-3 ↗
19. Synthesis and characterization of a silicone resin with silphenylene units in Si-O-Si backbones10.1002/app.30635 ↗
20. Comparative study of micro-and nano-structured coatings for high-temperature oxidation in steam atmospheres10.1007/s11085-013-9447-2 ↗
21. Thermal stability of organofunctional polysiloxanes10.1016/j.tca.2013.04.032 ↗
22. Study on the synthesis and application of silicone resin containing phenyl group10.1007/s10971-015-3752-y ↗
23. Synthesis, characterization and ceramic conversion studies of borosiloxane oligomers from phenyltrialkoxysilanes10.1007/s10904-010-9380-7 ↗
24. Synthesis and properties of poly(tetramethyl-1,6- silpyrenylenesiloxane) derivative with phenyl groups on pyrenylene moiety10.1007/s00289-011-0639-0 ↗
25. Synthesis and thermal characterization of novel adamantane-based polysiloxan10.1016/j.polymer.2008.04.053 ↗
26. Thermal stability and electrical behavior of polydimethylsiloxane nanocomposites with carbon nanotubes and carbon black fillers10.1177/0021998311412985 ↗
27. Anticorrosive temperature-resistant silicone coatings with compacted mineral fillers
28. Heat-resistant anti-corrosive paint from epoxy-silicone vehicles10.1108/00035599710185476 ↗
29. Study of the oxidation process of metallic pigments in the presence of silicone resin under heating10.1134/S1070427216010031 ↗
30. The degradation of silicone coatings in high temperature atmospheres, Anti-Corros
31. Protective space coatings: a ceramer approach for nanoscale materials10.1016/S0300-9440(03)00135-8 ↗
32. Development of heat-resistant anticorrosion urethane siloxane paints10.1007/s11998-012-9464-0 ↗
33. Termination in anionic polymerization of octamethylcyclotetrasiloxane, formation of stable complexes on active sites10.1002/pol.12005315841 ↗
34. Airborne chloride deposit and its effect on marine atmospheric corrosion of mild steel10.1016/j.corsci.2015.04.015 ↗
35. The thermal degradation behavior of polydimethylsiloxane/montmorillonite nanocomposites10.1016/j.polymdegradstab.2009.04.030 ↗
36. Effects of TriSilanolIsobutyl-POSS on thermal stability of methylsilicone resin10.1016/j.polymdegradstab.2006.04.031 ↗
37. Thermal degradation of polyurethane and polyurethane/expandable graphite coatings10.1016/S0141-3910(01)00177-X ↗
38. Thermal degradation and fire behaviour of novel polyurethanes based on phosphate polyols10.1016/j.polymdegradstab.2014.01.012 ↗
39. Silicone resin applications for ceramic precursors and composites10.3390/ma3063518 ↗
40. Processing of polysiloxane-derived porous ceramics: a review
41. Preparation and characterization of water-based aluminium pigments modified with SiO2 and polymer brushes10.1016/j.corsci.2016.06.014 ↗
42. Influence of various surface treated silica nanoparticles on the electrochemical properties of SiO2/polyurethane nanocoatings10.1016/j.corsci.2011.08.036 ↗
43. Corrosion resistance of lamellar aluminium pigments coated by SiO2 by sol-gel method10.1016/j.corsci.2010.09.012 ↗
44. Deposition behavior of hexamethydisiloxane films based on the FTIR analysis of Si-O-Si and Si-CH3 bonds10.1016/S0040-6090(97)00683-4 ↗
45. Synthesis, thermal and mechanical behavior of a silicon/phosphorus containing epoxy resin10.1002/app.42788 ↗
46. The effect of epoxy-silicone copolymer content on the thermal and mechanical properties of cured epoxy resin modified with siloxane10.1039/C4RA09230A ↗
47. A novel epoxy-functionalized hyperbranched polysiloxane (HPSi) endowing methyl phenyl silicone resin (Si603)/epoxy systems with enhanced compatibility and fire retardancy performance10.1039/C5RA18399E ↗
48. Corrosion inhibition of 304 stainless steel by nano-sized Ti/silicone coatings in an environment containing NaCl and water vapor at 400-600°C10.1023/B:OXID.0000038782.77162.5b ↗
49. Pyrolysis kinetics of highly crosslinked polymethylsiloxane by TGA
50. Microstructural investigation of the breakdown of the protective oxide scale on a 304 steel in the presence of oxygen and water vapour at 600°C10.1016/j.corsci.2005.08.012 ↗
51. The oxidation behaviour of metals and alloys at high temperatures in atmospheres containing water vapour: a review10.1016/j.pmatsci.2007.11.001 ↗
52. Influence of Cr content on the corrosion of Fe-Cr alloys: the synergistic effect of NaCl and water vapor10.1023/A:1023083309041 ↗
53. Mechanical properties and oxidation behavior of a graded (Ti,Al)N coating deposited by arc-ion plating10.1007/s11085-006-9015-0 ↗
54. Breakdown of the protective oxide on 11 % Cr steel at high temperature in the presence of water vapor and oxygen, the influence of chromium vaporization10.1179/mht.2005.008 ↗
55. Corrosion protection by organic coatings: electrochemical mechanism and novel methods of investigation10.1016/S0013-4686(00)00348-0 ↗
56. Corrosion behavior of pure Ti under a solid NaCl deposit in a wet oxygen flow at 600 °C
57. Heterogeneous metal catalysts for oxidation reactions
58. Adsorption and reactions of tetraethoxysilane (TEOS) on clean and water-dosed titanium dioxide (110)10.1021/ja00078a055 ↗
59. Study of γ-alumina surface reactivity: adsorption of water and hydrogen sulfide on octahedral aluminum sites10.1021/jp020145n ↗