Interfacial modification and cyclic ablation behaviors of a SiC/ZrB2-SiC/SiC triple-layer coating for C/SiC composites at above 2000 °C
Source abstract
Abstract
Abstract A SiC/ZrB2-SiC/SiC triple-layer coating was fabricated successively by chemical vapor deposition (CVD), slurry brushing-sintering and CVD for C/SiC composites. To enhance the cyclic ablation resistance, a pre-oxidation treatment on the inner SiC layer was performed. The bonding strength of the coating with pre-oxidation at 1600 °C is significantly improved to 32 MPa, 77.8 % greater than that of the untreated specimen. The coating can endure 5 ablation cycles from 2050 °C to room temperature without peeling off and displays a small spalling area of 18 mm2 after 6 cycles. The cyclic ablation mechanisms are discussed in detail.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Mechanical behavior of C/SiC T-section under pulling load10.1016/j.jmst.2019.04.040 ↗
2. Tribological behavior of C/C-SiC composites-a review10.1007/s40145-015-0171-z ↗
3. Long-term oxidation behaviors of C/SiC composites with a SiC/UHTC/SiC three-layer coating in a wide temperature range10.1016/j.corsci.2018.10.017 ↗
4. ZrB2 coating for the oxidation protection of carbon fiber reinforced silicon carbide matrix composites10.1016/j.vacuum.2013.03.009 ↗
5. A multilayer coating of dense SiC alternated with porous Si-Mo for the oxidation protection of carbon/carbon silicon carbide composites10.1016/j.carbon.2007.10.035 ↗
6. Oxidation behavior of 2D C/SiC composites coated with multi-layer SiC/Si-B-C/SiC coatings under wet oxygen atmosphere10.1016/j.apsusc.2015.06.153 ↗
7. Ablation behavior of rare earth La-modified ZrC coating for SiC-coated carbon/carbon composites under an oxyacetylene torch10.1016/j.corsci.2015.11.030 ↗
8. A WSi2-HfB2-SiC coating for ultralong-time anti-oxidation at 1973K10.1016/j.corsci.2018.11.007 ↗
9. Ablation resistance of ZrC-MoSi2/ZrC-SiC double-layered coating in a plasma flame10.1016/j.corsci.2018.10.006 ↗
10. Thermal cycling and reactivity of a MoSi2/ZrO2 composite designed for self-healing thermal barrier coatings10.1016/j.matdes.2016.01.054 ↗
11. A multilayer coating of dense SiC alternated with porous Si-Mo for the oxidation protection of carbon/carbon silicon carbide composites10.1016/j.carbon.2007.10.035 ↗
12. Microstructure, oxidation protection and failure mechanism of Yb2SiO5/LaMgAl11O19 coating deposited on C/SiC composites by atmospheric plasma spraying10.1016/j.corsci.2012.05.020 ↗
13. Oxidation behavior of 2D C/SiC composites coated with multi-layer SiC/Si-B-C/SiC coatings under wet oxygen atmosphere10.1016/j.apsusc.2015.06.153 ↗
14. Si-Mo-SiO2 oxidation protective coatings prepared by slurry painting for C/C-SiC composites10.1016/j.surfcoat.2008.04.047 ↗
15. Oxidation behavior of oxidation protective coatings for PIP-Cf/SiC composites at 1500C10.1016/j.ceramint.2011.06.063 ↗
16. Oxidation protective silicon carbide coating for C/SiC composite modified by a chromium silicide–chromium carbide outer layer10.1016/j.msea.2015.07.081 ↗
17. Microstructure and anti-oxidation properties of Yb2Si2O7/SiC bilayer coating for C/SiC composites10.1016/j.ceramint.2019.08.132 ↗
18. Oxidation behavior of two-dimensional C/SiC modified with self-healing Si–B–C coating in static air10.1016/j.corsci.2012.08.003 ↗
19. Mechanisms governing the failure modes of dense vertically cracked thermal barrier coatings10.1016/j.engfracmech.2017.11.037 ↗
20. An innovative model coupling TGO growth and crack propagation for the failure assessment of lamellar structured thermal barrier coatings10.1016/j.ceramint.2019.09.120 ↗
21. Interface design and HfC additive to enhance the cyclic ablation performance of SiC coating for carbon/carbon composites from 1750 °C to room temperature under vertical oxyacetylene torch10.1016/j.corsci.2017.04.014 ↗
22. The effects of carbon/carbon composites blasting treatment and modifying SiC coatings with SiC/ZrB2 on their oxidation and cyclic ablation performances10.1016/j.corsci.2018.06.008 ↗
23. Enhanced bonding strength and thermal cycling performance of MoSi2-CrSi2-SiC-Si coating for carbon/carbon composites by surface modification via blasting treatment10.1016/j.ceramint.2016.06.008 ↗
24. Bonding strength, thermal shock and oxidation resistance of interlocking (Zr,Hf)C-SiC/SiC double-layer coating for C/C composites10.1016/j.surfcoat.2017.02.072 ↗
25. Effect of oxygen plasma treatment on bonding strength of epoxy coating on steel substrate10.1016/j.porgcoat.2019.02.011 ↗
26. Microstructure and oxidation resistant behavior of Er2Si2O7 and Er2Si2O7/LaMgAl11O19 coatings deposited on Cf/SiC composites by APS at 1723 K
27. Bond stability and oxidation resistance of BSAS-based coating on C/SiC composites10.1016/j.surfcoat.2016.10.080 ↗
28. Fabrication and characterization of C/SiC composites with large thickness, high density and near-stoichiometric matrix by heaterless chemical vapor infiltration10.1016/j.msea.2007.02.037 ↗
29. Interfacial egregation, pore formation, and scale adhesion on NiAl Alloys10.1007/s11085-005-1954-3 ↗
30. Preparation and properties of porous mullite ceramics with high closed porosity and high strength from fly ash via reaction synthesis process10.1016/j.jallcom.2019.06.272 ↗
31. Phase diagrams for ceramists
32. Thermodynamic modeling of the Al2O3-B2O3-SiO2 system10.1016/j.jnoncrysol.2009.06.036 ↗
33. Oxidation and ablation resistance of ZrB2-SiC-Si/B-modified SiC coating for carbon/carbon composites10.1016/j.corsci.2012.10.041 ↗
34. Effect of heat flux on ablation behavior and mechanism of C/C-ZrB2-SiC composite under oxyacetylene Torch Flame10.1016/j.corsci.2013.04.052 ↗