journal article·2008-09

Material characterization and corrosion performance of nickel electroplated in supercritical CO2 fluid

Sung-Ting Chung, Hsien-Chung Huang, Szu-Jung Pan, Wen-Ta Tsai, Pee-Yew Lee, Chung-Hsin Yang, Mau-Bin Wu

Corrosion Science· Volume 50· Issue 9
Publisher page

Abstract

Abstract The surface roughness, microhardness, crystal structure and corrosion performance of nickels electroplated at atmospheric pressure and in supercritical CO 2 fluid, respectively, are compared. The experimental results showed that nickel electroplated in the latter case exhibited a lower surface roughness and a higher hardness. In HCl solution, the nickel deposited in supercritical CO 2 fluid had a lower anodic current density and a higher polarization resistance. The advantage of emulsified supercritical CO 2 fluid for electroplating was demonstrated.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electrodeposition and Electroless Coatings · Corrosion Behavior and Inhibition · Injection Molding Process and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Dennis · 1993
2. Schlesinger · 1987
3. Improving the throwing power of nickel electroplating baths10.1016/S0254-0584(97)02070-1 ↗
4. Effect of frequency on properties of film in Cu electroplating using square pulse plating
5. Pulse electrodeposition of nanocrystalline nickel using ultra narrow pulse width and high peak current density10.1016/S0257-8972(03)00014-8 ↗
6. Kinetics of electroplating process of nano-sized ceramic particle/Ni composition10.1016/S0254-0584(01)00564-8 ↗
7. Application of emulsion of dense carbon dioxide in electroplating solution with nonionic surfactants for nickel electroplating10.1016/S0257-8972(03)00734-5 ↗
8. The effects of dense carbon dioxide on nickel plating using emulsion of carbon dioxide in electroplating solution10.1016/j.surfcoat.2003.07.006 ↗
9. New electroplating method of nickel in emulsion of supercritical carbon dioxide and electroplating solution to enhance uniformity and hardness of plated film10.1016/j.tsf.2003.09.072 ↗
10. Electroplating in CO2-in-water and water-in-CO2 emulsions using a nickel electroplating solution with anionic fluorinated surfactant10.1016/j.surfcoat.2004.01.009 ↗
11. Nano-grain structure of nickel films prepared by emulsion plating using dense carbon dioxide10.1016/j.surfcoat.2004.03.014 ↗
12. Nano-grain deposition via an electroplating reaction in an emulsion of dense carbon dioxide in a nickel electroplating solution using nonionic fluorinated surfactant10.1016/j.surfcoat.2004.04.087 ↗
13. Three-phase catalytic hydrogenation of α-methylstyrene in supercritical carbon dioxide10.1016/S0896-8446(02)00092-X ↗
14. Kinetic experiments and modeling of a three-phase catalytic hydrogenation reaction in supercritical CO210.1016/S0920-5861(98)00390-3 ↗
15. Electroplating of nanostructured nickel in emulsion of supercritical carbon dioxide in electrolyte solution10.1246/cl.2002.1086 ↗
16. Microstructural evolution in pulse plated nickel electrodeposits10.1016/S0257-8972(96)02928-3 ↗
17. Controlling the surface texture of nickel for hightemperature oxidation inhibition10.1016/S0010-938X(98)00146-2 ↗
18. On texture formation of nickel electrodeposits10.1023/A:1018429013660 ↗
19. Mass-transport effects on texture formation of nickel electrodeposits10.1016/S0254-0584(00)00313-8 ↗
20. Preferred orientations in nickel electrodeposits I. The mechanism of development of textures in nickel electrodeposits10.1016/S0022-0728(63)80152-7 ↗
21. The deformation and ageing of mild steel: III Discussion of results10.1088/0370-1301/64/9/303 ↗
22. The cleavage strength of polycrystals
23. On the interpretation of corrosion processes through the superposition of electrochemical partial processes and on the potential of mixed electrodes