The mechanism of high temperature oxidation of a SmCo-based magnetic alloy

Z. Yang, X. Peng, Q. Feng, Z. Guo, W. Li, F. Wang

Corrosion Science· Volume 61
Publisher page

Abstract

The oxidation of a Sm(CobalFe0.22Cu0.08Zr0.02)(7.5) magnetic alloy in air at 500,600 and 700 degrees C has been studied. The temperature increase greatly promotes the external and internal oxidation. The external scale consists of a thin outer layer of CuO and a thicker inner layer of (Co-x, Fe1-x,)Fe2O4 with distribution of alpha-Fe2O3. Samarium oxide is not seen in the scale but it is mainly internal oxidation product. Breakaway oxidation is observed at higher temperatures. The mechanisms of external and internal oxidation as well as breakaway oxidation are presented, based on detailed compositional and microstructural characterization of the oxidized zone of the alloy. (C) 2012 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnetic Properties of Alloys · Magnetic and transport properties of perovskites and related materials · Metallic Glasses and Amorphous Alloys

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. Micromagnetism and the microstructure of high-temperature permanent magnets10.1063/1.1809250 ↗
2. High-performance permanent magnets10.1007/s001140050755 ↗
3. Recent progress in 2:17-type permanent magnets10.1007/BF02648616 ↗
4. Recent developments in high-temperature permanent magnet materials
5. High-temperature samarium cobalt permanent magnets
6. Application of high temperature magnetic materials10.1109/20.908805 ↗
7. Thermal stability of Sm–TM high temperature magnets at 300–550°C10.1109/20.908773 ↗
8. A new class of Sm–TM magnets for operating temperatures up to 550°C10.1109/20.908807 ↗
9. Surface reaction and Sm depletion at 550°C for high temperature Sm–TM magnets10.1109/20.951225 ↗
10. Prediction of the oxidation behaviour of Sm–Co-based magnets10.1016/j.jmmm.2004.11.408 ↗
11. Corrosion behavior of Sm–Co-based permanent magnets in oxidizing environments10.1109/TMAG.2004.829195 ↗
12. The oxidation of SmCo magnets10.1063/1.2830559 ↗
13. The oxidation morphology of SmCo alloys10.1016/j.jallcom.2009.07.115 ↗
14. The oxidation kinetics of SmCo alloys10.1016/j.jallcom.2008.05.083 ↗
15. Twinning structure in Sm(Co, Fe, Cu, Zr)z permanent magnet10.1016/j.intermet.2010.02.008 ↗
16. The microstructure of sintered Sm(Co0.72Fe0.20Cu0.055Zr0.025)7.5 permanent magnet studied by atom probe10.1016/j.actamat.2003.10.015 ↗
17. Identification of the cell boundary phase in the isothermally aged commercial Sm(Co0.75Fe0.1Cu0.12Zr0.04)7.4 sintered magnet10.1016/j.scriptamat.2005.12.009 ↗
18. A fundamental aspect of the growth process of alumina scale on a metal with dispersion of CeO2 nanoparticles10.1016/j.corsci.2011.02.014 ↗
19. Dislocation and grain boundary diffusion in the growth of α-Fe2O3 whiskers and twinned platelets peculiar to gaseous oxidation10.1038/2181046a0 ↗
20. The growth of hematite blades during the high temperature oxidation of iron10.1007/BF02642408 ↗
21. Intensity anomalies in electron diffraction patterns of CuO’10.1149/1.2781245 ↗
22. CuO Nanowires can be synthesized by heating copper substrates in air10.1021/nl0257519 ↗
23. Wrinkling of α-alumina films grown by thermal oxidation – I. Quantitative studies on single crystals of Fe–Cr–Al alloy10.1016/S1359-6454(98)00133-5 ↗
24. Self-diffusion of iron in iron oxides and the wagner theory of oxidation10.1007/BF03397553 ↗
25. Sur l’oxydation du fer dans l’air dans l’intervalle 400–700°C10.1016/0001-6160(56)90154-7 ↗
26. On the mechanism and kinetics of the scaling of iron
27. The oxidation of high-purity copper–nickel alloys
28. Binnewies · 2002
29. Chemical diffusion in the production of Sm–Co magnet alloys by reduction–diffusion processing10.2320/jinstmet1952.54.1_48 ↗
30. Reaktionstypen bei der oxydation von legierungen
31. A structural and kinetic study of the oxidation of the intermetallic Sm2(Fe, Co)17 compound for permanent magnets10.1016/S0304-8853(97)00148-0 ↗
32. Microstructure and growth kinetics of the fibrous composite subscale formed by internal oxidation of SmCo510.1007/BF02644102 ↗
33. CVM calculation of the ternary system Co–Cu–Fe10.1016/S0925-8388(00)01198-1 ↗
34. Z. Yang, X. Peng, F. Wang, Unpublished work, in preparation.
35. Uber die innere oxydation von metallegierungen10.1016/0001-6160(64)90036-7 ↗
36. The stress and spalling behavior of the oxide scale formed on polycrystalline Ni3Al10.1016/1359-6454(96)00009-2 ↗
37. Cracking and spalling of protective oxide layers10.1016/0921-5093(89)90731-4 ↗
38. Application of fracture mechanics to failure of surface oxide scales10.1179/026708388790331456 ↗
39. The mechanical failure of oxide scales under tensile or compressive load10.1007/BF01352181 ↗
40. Conditions for the initiation of oxide-scale cracking and spallation10.1016/0010-938X(84)90051-9 ↗
41. Discontinuous oxidation and erosion–oxidation of a CeO2-dispersion-strengthened chromium coating10.1016/j.corsci.2010.02.009 ↗
42. Oxidation of a novel CeO2-dispersion-strengthened chromium coating in simulated coal-combustion gases10.1016/j.msea.2006.04.030 ↗
43. Mechanisms of breakaway oxidation and application to a chromia-forming steel10.1023/A:1018855914737 ↗
44. Thermal oxidation kinetics and oxide scale adhesion of Fe–15Cr alloys as a function of their silicon content10.1016/j.actamat.2006.04.023 ↗
45. The oxidation of titanium in oxygen at high temperatures10.1016/0001-6160(60)90170-X ↗