journal article·2012-01

Oxidation of Fe–Si, Fe–Al and Fe–Si–Al alloys in CO2–H2O gas at 800°C

Huan Li, Jianqiang Zhang, David J. Young

Corrosion Science· Volume 54
Publisher page

Abstract

Abstract Binary Fe–(1, 2, 3)Si and Fe–(2, 4, 6)Al, and ternary Fe–(2, 3)Si–(4, 6)Al alloys (all in wt%) were oxidised in Ar–20% CO2, with and without H2O, at 800 °C. All binary alloys except Fe–6Al, in all gases, formed a thin outer layer of Fe3O4, an intermediate Fe3O4 + FeO layer, an inner FeO + Fe2SiO4 (or FeAl2O4) layer and internally precipitated SiO2 (or FeAl2O4). Ternary alloys and Fe–6Al developed a protective Al2O3 layer beneath Fe2O3 in Ar–20% CO2. Water vapour affected ternary alloy oxidation only slightly, but Fe–6Al oxidized internally in high H2O-content gas, and its scale was non-protective.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Catalytic Processes in Materials Science · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. Carburisation of ferritic Fe–Cr alloys by low carbon activity gases10.1016/j.corsci.2011.05.013 ↗
2. Scale formation mechanisms of martensitic steels in high CO2/H2O-containing gases simulating oxyfuel environments10.3184/096034009X438185 ↗
3. Carburization of Fe–Cr alloys during oxidation in dry carbon dioxide10.1149/1.2426622 ↗
4. Internal oxidation and carburisation of heat-resistant alloys10.1016/S0010-938X(02)00182-8 ↗
5. High-temperature corrosion of Cr2O3-forming alloys in CO–CO2–N2 atmospheres10.1007/BF01052021 ↗
6. High-temperature corrosion and creep of Ni-Cr-Fe alloys in carburizing and oxidizing environments10.1007/BF00612086 ↗
7. Corrosion resistance of a high-silicon alloy in metal-dusting environments10.1007/s11085-007-9052-3 ↗
8. Einfluß von wasserdampf und kohlendioxyd auf die oxydation von eisen-silicium-legierungen in sauerstoff bei temperaturen von 750 bis 1050°C10.1002/maco.19650160806 ↗
9. The influence of silicon on the oxidation properties of iron10.1016/S0010-938X(74)80032-6 ↗
10. Oxidation of iron–silicon alloys10.1007/BF00659276 ↗
11. Non-protective and protective scaling of a commercial 1.75% silicon–iron alloy in the range 800–1000°C10.1016/S0010-938X(65)90189-7 ↗
12. The oxidation of dilute iron–silicon alloys ([Si]⩽1%) in carbon dioxide10.1016/0010-938X(82)90070-1 ↗
13. High-temperature oxidation of Fe–Si alloys in Ar–H2O atmospheres10.2355/tetsutohagane1955.77.1_123 ↗
14. Effect of water vapor on the oxidation behavior of Fe–1.5Si in air at and 1273K10.1023/A:1010353729663 ↗
15. Effect of small amounts of manganese on oxidation behavior of a 3-percent silicon–iron alloy in water–hydrogen atmospheres10.1016/S0010-938X(77)80011-5 ↗
16. Transition from external to internal oxidation in iron–silicon alloy as a function of oxygen potential of ambient atmosphere10.1016/0036-9748(76)90191-5 ↗
17. The formation of protective films on iron–silicon alloys10.1016/0010-938X(79)90012-X ↗
18. The oxidation of iron–aluminum alloys from 450 to 90010.1149/1.2408222 ↗
19. Observations of nodule growth during the oxidation of pure binary iron–aluminum alloys10.1007/BF00666643 ↗
20. Oxidation properties of Fe–Al alloys (1.5–5 a/o Al) in oxygen at 1173K10.1149/1.2108526 ↗
21. The oxidation of iron–aluminum alloys10.1007/BF00665045 ↗
22. Competitive effect of water vapor, oxygen on the oxidation of Fe–5 wt.% Al alloy at 1073K10.1023/A:1010372711563 ↗
23. The high-temperature oxidation resistance of iron–silicon–aluminum10.1007/BF00618248 ↗
24. H. Li, J. Zhang, D.J. Young, Oxidation of Fe–Si alloys in CO2–H2O atmospheres, Mater. High Temp., in press.
25. A model for mild steel oxidation in CO210.1007/BF00610578 ↗
26. Birks · 2006
27. Thermodynamics of the system iron–aluminum–oxygen between 1073 and 1573K10.1007/BF02670873 ↗
28. On the mechanism and kinetics of the scaling of iron
29. The kinetics of wustite scale formation on iron10.1016/0001-6160(60)90006-7 ↗
30. Reaktionstypen bei der oxydation von legierungen
31. The transition from internal to external oxidation and the formation of interruption bands in silver–indium alloys10.1016/0001-6160(61)90103-1 ↗
32. Solubility and interstitial migration of oxygen in b.c.c
33. 2004
34. Young · 2008
35. Iron–aluminium alloys: a review of their oxidation behaviour
36. The mechanism of the high-temperature oxidation of iron–chromium alloys in water vapor10.1149/1.2425963 ↗
37. Einfluss von wasserdampf und kohlendioxyd auf die oxydation von eisen in sauerstoff bei hohen temperature10.1016/S0010-938X(65)90500-7 ↗
38. The effect of water vapor on selective oxidation of Fe–Cr alloys10.1007/s11085-007-9090-x ↗
39. A theoretical analysis of the oxidation of Fe–Si alloys10.1016/0010-938X(82)90071-3 ↗
40. Oxygen potential distribution during disappearance of the internal oxidation zone formed in the steam oxidation of Fe–9Cr–0.26Si ferritic steel at 973 K10.3184/096034005782750545 ↗
41. Formation and disappearance of an internal oxidation zone in the initial stage of the steam oxidation of Fe–9Cr–0.26Si ferritic-steel10.3184/096034003782748964 ↗
42. Effect of oxide volatilization on oxidation kinetics of Cr and Fe–Cr alloys10.1149/1.2424115 ↗
43. Passivity and inhibition during the oxidation of metals at elevated temperatures10.1016/S0010-938X(65)80003-8 ↗
44. S.W. Guan, J. Corkum, W. Smeltzer, Oxidation behavior of Fe–Al–Si alloys at 1073 and 1173K, in: Y. Saito, B. Önay, T. Maruyama (Eds.), High Temperature Corrosion of Advanced Materials and Protective Coatings, North Holland, 1992, pp. 75–82.10.1016/B978-0-444-88970-6.50013-0 ↗
45. The influence of alloying elements on the development and maintenance of protective scales10.1007/BF01046725 ↗
46. Batlin · Atom. Svarka. · 1982 · 1 · 70