journal article·2018-09

Environmentally assisted degradation of spinodal copper alloy C72900

Roy Johnsen, Torstein Lange, Gaute Stenerud, Jim Stian Olsen

Corrosion Science· Volume 142
Publisher page

Abstract

Abstract In this work, a spinodal Copper alloy – C72900, was tested to investigate the resistance against environmentally assisted degradation. The material was tested according to ISO 15156-3 Level V in sour H2S solution and to cathodic polarization in simulated seawater with stressed samples. The results showed no indications of hydrogen stress cracking under cathodic polarization in seawater. However, cracks up to 3 mm deep were found on the samples exposed to sour H2S environment. Energy Dispersive Spectroscopy showed severe depletion of copper close to the cracks which is associated with selective corrosion. Stress corrosion cracking was the dominating crack mechanism in the ISO 15156-3 Level V test.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Advanced materials and composites · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (42)

Show source-provided references
1. Guidelines for use of copper alloys in seawater
2. CDA Inc seminar technical report 7044-1919
3. 2010
4. Corrosion of Cu-Ni alloys in sulfide-polluted seawater10.5006/1.3316004 ↗
5. Performance advances in copper-nickel-tin spinodal alloys
6. Spinodal copper alloy C72900 – new high strength antifriction alloy system10.1179/1879139511Y.0000000012 ↗
7. Sour service testing of High strength TS temper CuNiSn alloy (UNS C72900)
8. http://www.materion.jp/alloy/tech_lit/toughmet%203AT110.pdf.
9. 2009
10. Hydrogen induced stress cracking of duplex stainless steel under cathodic protection in seawater – historical overview and lessons learned
11. Foinaven super duplex materials crack investigation
12. Avoiding hydrogen embrittlement stress cracking of ferritic austenitic stainless steels under cathodic protection
13. Failure of a subsea super duplex manifold hub by HISC and implications for design
14. A review on hydrogen embrittlement of duplex stainless steels
15. Corrosion evaluation of a High performance Cu-based alloy for seawater applications
16. ASTM G129 Standard Practice for Slow Strain Rate Testing to Evaluate the Susceptibility of Metallic Materials to Environmentally Assisted Cracking.
17. ASTM D1141 Synthetic seawater.
18. The development of very High strength copper alloys with resistance to hydrogen embrittlement and stress corrosion cracking
19. NACE Standard TM0177-2005 Laboratory Testing of Metals for Resistance to Sulfide Stress Cracking and Stress Corrosion Cracking in H2S Environments.
20. 2002
21. NACE TM0198-1998, Slow Strain Rate Test Method for Screening Corrosion-Resistant Alloys for Stress Corrosion Cracking in Sour Oilfield Service.
22. Materion Brush Performance Alloys: Stress Corrosion Cracking in NACE MR0175 Environments of Toughmet Alloys – Final report. Document no.: 15R8T2U-5,2016-11-02. Prepared by DNV GL for Materion Brush Performance Alloys Inc. Not published.
23. ASTM E112 – 13 Standard Test Method for Determining Average Grain Size.
24. DNV RP F112 Design of duplex stainless steel subsea equipment exposed to cathodic protection. October 2008.
25. New improved method for HISC testing of stainless steels under cathodic protection
26. Stenerud · 2015
27. The Cu− Nb (copper-niobium) system10.1007/BF02876162 ↗
28. ASTM · 2015
29. Age hardening in Cu-15Ni-8Sn alloy10.1007/BF02646415 ↗
30. Spinodal decomposition in Cu-9wt% Ni-6wt% Sn—II. A critical examination of mechanical strength of spinodal alloys10.1016/0001-6160(74)90058-3 ↗
31. Relationship between microstructure and mechanical properties of a spinodally decomposing Cu-15Ni-8Sn alloy prepared by spray deposition10.1007/BF02665473 ↗
32. Spinodal decomposition, ordering transformation, and discontinuous precipitation in a Cu–15Ni–8Sn alloy10.1016/S1359-6454(98)00095-0 ↗
33. On the discontinuous precipitation reaction and solute redistribution in a Cu-15%Ni-8%Sn alloy10.1016/j.matchar.2008.01.007 ↗
34. X-ray diffraction studies of the decomposition and microstructural characterization of cold-worked powders of Cu–15Ni–Sn alloys by Rietveld analysis10.1016/j.jallcom.2003.10.019 ↗
35. Journal of the American Institute for Conservation, JAIC · 1999 · 38 · 18610.1179/019713699806113493 ↗
36. Typical failures of CuNi 90/10 seawater tubing systems and how to avoid them. Technical advisory service
37. Experience with copper nickel alloy tubing, Water boxes and piping in MSM desalination plants
38. Aspects of failure of condenser tubes and their remedial measures at power plants
39. Stress corrosion of α-Brass in an acid sulfate solution
40. Progress toward understanding the stress corrosion problem
41. Electron metallography of chemical attack upon some alloys susceptible to stress corrosion cracking10.5006/0010-9312-19.11.373 ↗
42. The stress corrosion cracking mechanism of alpha-brass in NaNO2 solutions10.1016/0010-938X(88)90103-5 ↗