Abstract
Abstract H2S corrosion behaviors of P110, Fe-Mn-Al, and Fe-Mn-Cr-Ni high-Mn steels were analyzed according to ion-selectivity of corrosion products. At 60 oC and 80 oC, cation-selective troilite restrain diffusion of corrosive ions to the substrate. The corrosion rates were low, and uniform corrosion occurred. At 100 oC and 205 oC, anion-selective pyrrhotite caused accumulation of Cl− between corrosion scale and substrate. Corrosion rates were high and localized corrosion happened. Crystal atom stacking models of iron sulfides were built, and the adsorption energy of ions on the exposed surface was calculated to discuss the ion-selectivity mechanism. The effect of alloy elements on corrosion behavior was analyzed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Metallurgical Processes and Thermodynamics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (53)
Show source-provided references
1. Kane · 1999
2. Role of sulfate-reducing bacteria in corrosion of mild steel: a review10.1080/08927019509378271 ↗
3. Mechanism of (Mg, Al, Ca)-oxide inclusion-induced pitting corrosion in 316L stainless steel exposed to sulphur environments containing chloride ion10.1016/j.corsci.2012.09.044 ↗
4. Chemistry of iron sulfides10.1021/cr0503658 ↗
5. Review of recent progress in the study of corrosion products of steels in a hydrogen sulphide environment10.1016/j.corsci.2018.05.002 ↗
6. Investigations of the diverse corrosion products on steel in a hydrogen sulfide environment10.1016/j.corsci.2014.06.048 ↗
7. Lunar troilite: crystallography10.1126/science.167.3918.621 ↗
8. Inversion twinning in troilite10.2138/am.2006.1999 ↗
9. Sour top of the line corrosion in the presence of acetic acid10.5006/1.3615805 ↗
10. Corrosion of iron in gaseous environments and in gas-saturated aqueous environments10.5006/1.3585068 ↗
11. Polymorphous FeS corrosion products of pipeline steel under highly sour conditions10.1016/j.corsci.2015.09.024 ↗
12. Effect of cation vacancy and crystal superstructure on thermodynamics of iron monosulfides10.1080/17415990600646124 ↗
13. Ordering, incommensuration, and phase transitions in pyrrhotite Part I: a TEM study of Fe7S810.1006/jssc.1996.0235 ↗
14. Structure and magnetism in synthetic pyrrhotite Fe7S8: A powder neutron-diffraction study10.1103/PhysRevB.70.014415 ↗
15. Shape-controlled synthesis of iron sulfide nanostructures via oriented attachment mechanism10.1016/j.jcrysgro.2009.08.023 ↗
16. Nature of sulphides and their corrosive effect on ferrous metals: a review10.1179/000705975798320701 ↗
17. Initiation and developmental stages of steel corrosion in wet H2S environments10.1016/j.corsci.2015.01.024 ↗
18. Initial stages of corrosion pits on AISI 1040 steel in sulfide solution analyzed by temporal series micrographs coupled with electrochemical techniques10.1016/j.corsci.2013.04.054 ↗
19. The effect of H2S concentration on the corrosion behavior of carbon steel at 90 ◦C10.1016/j.corsci.2010.02.004 ↗
20. The chemistry of the hydrogen sulfide and iron sulfide systems in natural waters10.1016/0012-8252(87)90046-8 ↗
21. Corrosion of iron in on H2S-CO2-H2O system: corrosion film properties on pure iron10.5006/0010-9312-19.10.354 ↗
22. The influence of hydrogen sulfide on corrosion of iron under different conditions10.1016/S0010-938X(00)00003-2 ↗
23. Corrosion at higher H2S concentrations and moderate temperatures
24. Formation of iron oxide and iron sulfide at high temperature and their effects on corrosion10.1016/j.corsci.2018.02.045 ↗
25. Corrosion behavior of mild steel in sour environment at elevated temperature10.5006/2366 ↗
26. Toward a more fundamental understanding of corrosion processes10.5006/1.3582030 ↗
27. Effect of sulfide films formed on X65 steel surface on hydrogen permeation in H2S environments10.1016/j.ijhydene.2016.10.130 ↗
28. Role of alloyed molybdenum on corrosion resistance of austenitic Ni–Cr–Mo–Fe alloys in H2S–Cl− environments10.1016/j.corsci.2015.05.053 ↗
29. Ion selective properties of rust membranes and protective effect of stable rust layer formed on weathering steel10.3323/jcorr1991.47.186 ↗
30. Iterative minimization techniques for ab initio total-energy calculations: molecular dynamics and conjugate gradients10.1103/RevModPhys.64.1045 ↗
31. Atoms, molecules, solids, and surfaces: applications of the generalized gradient approximation for exchange and correlation10.1103/PhysRevB.46.6671 ↗
32. Ernzerh of M. Generalized gradient approximation made simple10.1103/PhysRevLett.77.3865 ↗
33. The effect of molybdate anion on the ion-selectivity of hydrous ferric oxide files in the chloride solution10.1016/0010-938X(77)90003-8 ↗
34. Nano-scale chemical analysis of rust on a 2% Si-bearing low alloy steel exposed in a coastal environment10.1016/j.corsci.2008.05.022 ↗
35. A review on the mineral chemistry of the non-stoichiometric iron sulphide, Fe1-xS (0≤x≤0.125): polymorphs, phase relations and transitions, electronic and magnetic structures10.1080/01411590500185542 ↗
36. Investigation of the iron-sulfide phase transformation in nanoscale10.1021/cg500333p ↗
37. Initial oxygen incorporation in the prismatic surfaces of troilite FeS10.1021/acs.jpcc.8b02774 ↗
38. Corrosion and deposition during the exposure of carbon steel to hydrogen sulphide-water solutions10.1016/0010-938X(80)90101-8 ↗
39. Computational investigation of FeS2 surfaces and prediction of effects of sulfur environment on stabilities10.1021/jp100578n ↗
40. Dzade · 2014
41. High-pressure and high-temperature polymorphism of iron sulfide (FeS)10.1107/S0567740882007523 ↗
42. Refinement of 3C pyrrhotite, Fe7S810.1107/S0567740879004532 ↗
43. The ion passing selectivity of CO2 corrosion scale on N80 tube steel
44. Role of copper and aluminum on the corrosion behavior of austenitic Fe–Mn–C TWIP steels in aqueous solutions and the related hydrogen absorption10.1016/j.corsci.2014.02.018 ↗
45. Development of superior corrosion resistance 3%Cr steels for downhole applications
46. Effect of Cl− accumulation on corrosion behavior of steels in H2S/CO2 methyldiethanolamine (MDEA) gas sweetening aqueous solution10.1016/j.jngse.2016.02.055 ↗
47. The effects of anions on the behaviour of scratched iron electrodes in aqueous solutions10.1016/0010-938X(80)90145-6 ↗
48. Comparison of corrosion behaviour of low-alloy pipeline steel exposed to H2S/CO2-saturated brine and vapour-saturated H2S/CO2 environments10.1016/j.electacta.2017.02.114 ↗
49. Corrosion inhibition effects of metal cations on SUS304 in 0.5 M Cl− aqueous solution10.1016/j.corsci.2018.06.028 ↗
50. Corrosion of low alloy steel and stainless steel in supercritical CO2/H2O/H2S systems10.1016/j.corsci.2016.06.003 ↗
51. Passivity breakdown of 316L stainless steel during potentiodynamic polarization in NaCl solution10.1016/j.corsci.2016.06.011 ↗
52. The role of chloride ions in pitting of carbon steel studied by the statistical analysis of electrochemical noise10.1016/S0169-4332(99)00328-1 ↗
53. Kinetics of iron sulfide and mixed iron sulfide/carbonate scale precipitation in CO2/H2S corrosion