Oxidation behavior of 9Cr-4.5Al ODS steel in 600 °C supercritical water and the effect of pre-oxidation
Source abstract
Abstract
Abstract The oxidation behavior of a 9Cr-4.5Al ODS steel in 600℃ supercritical water with 200 ppb dissolved oxygen was investigated with and without a pre-oxidation heat treatment. In general, results suggest that all samples follow the “available space model” oxidation mechanism as exposure time is extended. Based on the microstructural analysis, it is found that a thin alumina layer formed by pre-oxidation treatment is initially protective up to approximately 100 h. However, this passive film becomes ineffective due to the existence of M23C6 (M = Cr, Fe) and the insufficient content of Al or/and Cr in the steel.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Fusion materials and technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. Oxide dispersion-strengthened/ferrite-martensite steels as core materials for generation IV nuclear reactors
2. Development of next generation tempered and ODS reduced activation ferritic/martensitic steels for fusion energy applications10.1088/1741-4326/57/9/092005 ↗
3. Corrosion and stress corrosion cracking in supercritical water10.1016/j.jnucmat.2007.05.017 ↗
4. Corrosion of ferritic–martensitic steel HT9 in supercritical water10.1016/j.jnucmat.2006.07.010 ↗
5. Corrosion behavior of oxide dispersion strengthened ferritic steels in supercritical water10.1016/j.jnucmat.2017.01.014 ↗
6. Oxidation of 9Cr oxide dispersion strengthened steel exposed in supercritical water10.1016/j.jnucmat.2007.05.018 ↗
7. Oxidation of ferritic–martensitic alloys T91, HCM12A and HT-9 in supercritical water10.1016/j.jnucmat.2007.05.023 ↗
8. Influence of exposure pressure on oxidation behavior of the ferritic–martensitic steel in steam and supercritical water10.1007/s11085-016-9624-1 ↗
9. Effect of water density/pressure on the corrosion behavior of 304 and 310 stainless steels10.1007/s11085-017-9812-7 ↗
10. Corrosion behavior of Alloy 625 in supercritical water environments10.1016/j.pnucene.2011.12.015 ↗
11. Corrosion behavior of Alloy 690 in aerated supercritical water10.1016/j.corsci.2012.10.001 ↗
12. Long-term thermal stability of nanoclusters in ODS-Eurofer steel: an atom probe tomography study10.1016/j.jnucmat.2017.05.027 ↗
13. Microstructure characterization and strengthening mechanisms of oxide dispersion strengthened (ODS) Fe-9% Cr and Fe-14% Cr extruded bars10.1016/j.jnucmat.2017.07.060 ↗
14. Microstructure characteristic and mechanical property of transformable 9Cr-ODS steel fabricated by spark plasma sintering10.1016/j.matdes.2017.06.063 ↗
15. Improvement of 9Cr-ODS martensitic steel properties by controlling excess oxygen and titanium contents10.1016/j.jnucmat.2004.04.043 ↗
16. Production and properties of nano-scale oxide dispersion strengthened (ODS) 9Cr martensitic steel claddings10.2355/isijinternational.43.2038 ↗
17. Corrosion properties of oxide dispersion strengthened steels in super-critical water environment10.1016/j.jnucmat.2004.04.040 ↗
18. Transmission electron microscopy of oxide development on 9Cr ODS steel in supercritical water10.1016/j.jnucmat.2009.03.032 ↗
19. Development of Al added high-Cr ODS steels for fuel cladding of next generation nuclear systems10.1016/j.jnucmat.2010.12.300 ↗
20. Study of the corrosion behavior of a 18Cr-oxide dispersion strengthened steel in supercritical water10.1016/j.corsci.2012.08.021 ↗
21. Mapping of 475°C embrittlement in ferritic Fe–Cr–Al alloys10.1016/j.scriptamat.2010.08.015 ↗
22. α′ precipitation in neutron-irradiated Fe–Cr alloys10.1016/j.scriptamat.2013.10.001 ↗
23. Irradiation-enhanced α ′ precipitation in model FeCrAl alloys10.1016/j.scriptamat.2016.02.002 ↗
24. Influence of the α–α′ phase separation on the tensile properties of Fe-base ODS PM 2000 alloy10.1016/j.msea.2010.08.083 ↗
25. Accident tolerant FeCrAl fuel cladding: current status towards commercialization
26. Steam oxidation behavior of FeCrAl cladding
27. Oxidation of fuel cladding candidate materials in steam environments at high temperature and pressure10.1016/j.jnucmat.2012.05.007 ↗
28. High temperature oxidation of fuel cladding candidate materials in steam–hydrogen environments10.1016/j.jnucmat.2013.05.047 ↗
29. Development of advanced oxidation resistant steel for ATF clad application
30. Increasing the upper temperature oxidation limit of alumina forming austenitic stainless steels in air with water vapor10.1007/s11085-011-9237-7 ↗
31. Composition, microstructure, and water vapor effects on Internal/External oxidation of alumina-forming austenitic stainless steels10.1007/s11085-009-9161-2 ↗
32. Alloy design strategies for promoting protective oxide-scale formation10.1007/s11837-000-0109-x ↗
33. Metal dusting of alumina-forming creep-resistant austenitic stainless steels10.1007/s11085-011-9279-x ↗
34. Mechanical properties of neutron-irradiated model and commercial FeCrAl alloys10.1016/j.jnucmat.2017.03.038 ↗
35. Design, properties, and weldability of advanced oxidation-resistant FeCrAl alloys10.1016/j.matdes.2017.05.009 ↗
36. A general strategy for the ultrafast surface modification of metals10.1038/ncomms13797 ↗
37. Corrosion behavior of pre-oxidized HR-224 superalloy in supercritical water environment at 700 °C10.1016/j.jnucmat.2018.03.053 ↗
38. Microstructure characterization of Al alloyed 9Cr ODS steels with different Al content10.1002/srin.201800594 ↗
39. Effects of exposure temperature and time on corrosion behavior of a ferritic–martensitic steel P92 in aerated supercritical water10.1016/j.corsci.2014.10.022 ↗
40. Oxidation behavior of ferritic–martensitic and ODS steels in supercritical water10.1016/j.jnucmat.2012.03.009 ↗
41. Bricks · 2006 · 131
42. Chromium-depleted zones and the oxidation process in stainless steels10.1007/BF00612157 ↗
43. Prediction of chromium depleted-zone evolution during aging of Ni–Cr–Fe alloys10.1016/S1359-6454(01)00444-X ↗
44. Formation of M23C6-type precipitates and chromium-depleted zones in austenite stainless steel10.1016/j.scriptamat.2011.06.010 ↗
45. Corrosion and corrosion fatigue behaviors of 9cr steel in a supercritical water condition10.1016/j.msea.2006.05.035 ↗
46. Corrosion behavior of ferritic/martensitic steel P92 in supercritical water10.1016/j.supflu.2009.06.019 ↗
47. Corrosion of ferritic–martensitic steels in steam and supercritical water10.1016/j.jnucmat.2012.09.037 ↗
48. Corrosion behavior of 9–12% Cr ferritic–martensitic steels in supercritical water10.1016/j.corsci.2009.12.032 ↗
49. Boiler materials for ultra-supercritical coal power plants—steamside oxidation10.1361/105994906X108756 ↗
50. 1974