journal article·2021-06

Role of microalloyed Sm in enhancing the corrosion resistance of hot-rolled Mg–8Sn–1Al–1Zn alloy

Jaeho Kwon, Soo-Min Baek, Hoseok Jung, Jong Chan Kim, Si-Young Lee, Sung Soo Park

Corrosion Science· Volume 185
Publisher page

Abstract

Abstract We report that the corrosion resistance of hot-rolled Mg–8Sn–1Al–1Zn alloy was significantly enhanced by Sm microalloying. Corrosion rates, measured after immersion for 72 h in 0.6 M NaCl solution, were found to be 2.7 and 19 mm y−1 for the alloys with and without an addition of 0.02 wt% Sm, respectively. Electrochemical and microstructural analyses revealed that the enhanced corrosion resistance achieved by Sm microalloying is mainly a result of a reduced H2 evolution rate owing to the presence of Al8Fe4Sm particles instead of nobler Al5Fe2 particles, which highly accelerate microgalvanic corrosion in the alloy without Sm microalloying.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Metal and Thin Film Mechanics · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (68)

Show source-provided references
1. Current wrought magnesium alloys: strength and weakness10.1007/s11837-005-0095-0 ↗
2. Magnesium sheet alloys: viable alternatives to steels?10.1179/1743284714Y.0000000596 ↗
3. Corrosion mechanisms of magnesium alloys10.1002/(SICI)1527-2648(199909)1:1<11::AID-ADEM11>3.0.CO;2-N ↗
4. Understanding magnesium corrosion10.1002/adem.200310405 ↗
5. Review of recent developments in the field of magnesium corrosion10.1002/adem.201400434 ↗
6. Fundamentals and advances in magnesium alloy corrosion10.1016/j.pmatsci.2017.04.011 ↗
7. Review of the atmospheric corrosion of magnesium alloys10.1016/j.jmst.2019.05.001 ↗
8. Enhancing plastic deformability of Mg and its alloys–A review of traditional and nascent development10.1016/j.jma.2017.11.001 ↗
9. Development of creep resistant die cast Mg–Sn–Al–Si alloy10.1016/j.msea.2005.09.022 ↗
10. Development of creep resistant Mg alloys10.4028/www.scientific.net/MSF.475-479.521 ↗
11. Compressive creep behavior of as-cast and aging-treated Mg–5wt% Sn alloys10.1016/j.msea.2008.05.006 ↗
12. The microstructure, tensile properties, and creep behavior of AZ91, AS52 and TAS652 alloy10.1016/j.jallcom.2009.12.145 ↗
13. The effect of precipitate state on the creep resistance of Mg–Sn alloys10.1016/j.scriptamat.2010.07.002 ↗
14. Enhanced age hardening response by the addition of Zn in Mg–Sn alloys10.1016/j.scriptamat.2006.04.005 ↗
15. Significant enhancement of the age-hardening response in Mg–10Sn–3Al–1Zn alloy by Na microalloying10.1016/j.scriptamat.2013.01.032 ↗
16. A high-strength Mg–Sn–Zn–Al alloy extruded at low temperature10.1016/j.scriptamat.2008.07.042 ↗
17. Microstructure and mechanical properties of binary Mg–Sn alloys subjected to indirect extrusion10.1016/j.msea.2010.03.031 ↗
18. Strong and ductile heat-treatable Mg–Sn–Zn–Al wrought alloys10.1016/j.actamat.2015.06.060 ↗
19. Low-temperature superplasticity of extruded Mg–Sn–Al–Zn alloy10.1016/j.scriptamat.2011.04.005 ↗
20. Heat-treatable Mg–Sn–Zn wrought alloy10.1016/j.scriptamat.2009.03.014 ↗
21. Microstructure and mechanical properties of an indirect-extruded Mg–8Sn–1Al–1Zn alloy10.1016/j.matlet.2009.09.062 ↗
22. Strength and ductility of novel Mg–8Sn–1Al–1Zn alloys extruded at different speeds10.1016/j.matlet.2011.03.010 ↗
23. Effect of extrusion conditions on microstructure and mechanical properties of microalloyed Mg–Sn–Al–Zn alloys10.1016/j.msea.2013.09.050 ↗
24. Effect of cold pre-forging on the microstructure and mechanical properties of extruded Mg–8Sn–1Al–1Zn alloy10.1016/j.msea.2014.06.053 ↗
25. Compositional optimization of Mg–Sn–Al alloys for higher age hardening response10.1016/j.msea.2012.12.041 ↗
26. Effect of rare earth additions on microstructure and texture development of magnesium alloy sheets10.1016/j.scriptamat.2009.12.033 ↗
27. Enhancement of tensile ductility and stretch formability of magnesium by addition of 0.2 wt%(0.035 at%)Ce10.1016/j.msea.2008.04.059 ↗
28. Excellent room-temperature ductility and formability of rolled Mg–Gd–Zn alloy sheets10.1016/j.jallcom.2010.11.141 ↗
29. Designing a magnesium alloy with high strength and high formability10.1038/s41467-018-04981-4 ↗
30. Effect of group II elements on the cold stretch formability of Mg–Zn alloys10.1016/j.actamat.2014.10.005 ↗
31. Understanding Mg corrosion in the body for biodegradable medical implants10.1016/j.scriptamat.2018.05.021 ↗
32. Magnesium-based composites and alloys for medical applications: a review of mechanical and corrosion properties10.1016/j.jallcom.2019.04.080 ↗
33. Corrosion of ultra-high-purity Mg in 3.5% NaCl solution saturated with Mg(OH)210.1016/j.corsci.2013.05.018 ↗
34. Effect of iron content on the corrosion of pure magnesium: critical factor for iron tolerance limit10.1016/j.corsci.2018.04.024 ↗
35. G1-03 · 2017
36. Design of Mg–Cu alloys for fast hydrogen production, and its application to PEM fuel cell10.1016/j.jallcom.2017.12.257 ↗
37. Effect of Zn addition on the microstructure and mechanical properties of cast, rolled and extruded Mg–6Sn–xZn alloys10.1016/j.msea.2016.10.075 ↗
38. Effects of minor Ca addition on microstructure and mechanical properties of the Mg–4.5Zn–4.5Sn–2Al-based alloy system10.1016/j.jallcom.2012.08.102 ↗
39. The influence of Sc addition on microstructure and tensile mechanical properties of Mg–4.5Sn–5Zn alloys10.1016/j.jma.2019.05.004 ↗
40. Influence of alloyed Al on the microstructure and corrosion properties of extruded Mg–8Sn–1Zn alloys10.1016/j.corsci.2015.03.007 ↗
41. Improved corrosion resistance of Mg–8Sn–1Zn–1Al alloy subjected to low-temperature indirect extrusion10.1016/j.corsci.2018.06.011 ↗
42. Crystal structure magnetic properties and hyperfine interactions in RFe4Al8 (R = rare earth) systems10.1016/0022-3697(78)90109-9 ↗
43. Phase stability and mechanical properties of Al8Fe4RE via first-principle calculations10.3390/ma12050701 ↗
44. Susceptibility of rare-earth-magnesium alloys to micro-galvanic corrosion10.1016/j.corsci.2010.08.006 ↗
45. Improved corrosion resistance of extruded Mg–8Sn–1Zn–1Al alloy by microalloying with Mn10.1016/j.scriptamat.2015.07.013 ↗
46. Role of alloyed Y in improving the corrosion resistance of extruded Mg–Al–Ca-based alloy10.1016/j.corsci.2017.01.022 ↗
47. Corrosion of Mg–9Al alloy with minor alloying elements (Mn, Nd, Ca, Y and Sn)10.1016/j.matdes.2017.05.048 ↗
48. Enhanced corrosion resistance of Mg–Sn–Zn–Al alloy by Y microalloying10.1016/j.scriptamat.2019.01.015 ↗
49. Microstructure and corrosion resistance of a Mg2Sn-dispersed Mg alloy subjected to pulsed electron beam treatment10.1016/j.jma.2020.02.005 ↗
50. Effect of Nd on the corrosion behaviour of AM50 and AZ91D magnesium alloys in 3.5 wt.% NaCl solution10.1016/j.corsci.2011.10.033 ↗
51. A comparative electrochemical study of AZ31 and AZ91 magnesium alloy10.1155/2010/412129 ↗
52. Corrosion behavior of Mg, AZ31, and AZ91 alloys in dilute NaCl solutions10.1007/s10008-010-1020-1 ↗
53. The anodic surface film and hydrogen evolution on Mg10.1016/j.corsci.2015.05.047 ↗
54. Accurate electrochemical measurement of magnesium corrosion rates; a combined impedance, mass-loss and hydrogen collection study10.1016/j.electacta.2013.12.124 ↗
55. Corrosion and passivation of magnesium alloys10.1016/j.corsci.2016.05.041 ↗
56. Role of Sn in corrosion and passive behavior of extruded Mg–5wt% Sn alloy10.1016/j.corsci.2015.10.028 ↗
57. Localized corrosion of magnesium in chloride-containing electrolyte studied by a scanning vibrating electrode technique10.1149/1.2918900 ↗
58. Localized corrosion of magnesium alloys in NaCl solutions explored by scanning electrochemical microscopy in feedback mode10.1016/j.electacta.2014.04.044 ↗
59. Localized corrosion of binary Mg–Ca alloy in 0.9 wt% sodium chloride solution10.1007/s40195-015-0361-2 ↗
60. Pitting corrosion of AZ91D and AJ62x magnesium alloys in alkaline chloride medium using electrochemical techniques10.1016/j.electacta.2005.05.013 ↗
61. Limitations in the use of the potentiodynamic polarisation curves to investigate the effect of Zn on the corrosion behaviour of as-extruded Mg–Zn binary alloy10.1016/j.corsci.2013.06.027 ↗
62. Influences of metallurgical factors on the corrosion behaviour of extruded binary Mg–Sn alloys10.1016/j.corsci.2014.01.035 ↗
63. Role of hydrogen evolution rate in determining the corrosion rate of extruded Mg–5Sn–(1–4 wt%)Zn alloys10.1016/j.corsci.2014.09.011 ↗
64. Poisoning the corrosion of magnesium10.1016/j.elecom.2013.07.021 ↗
65. Simultaneously improving the corrosion resistance and strength of magnesium via low levels of Zn and Ge additions10.1016/j.corsci.2018.06.027 ↗
66. Reducing the corrosion rate of magnesium via microalloying additions of group 14 and 15 elements10.1016/j.electacta.2017.11.062 ↗
67. Research and development in magnesium alloys for industrial and biomedical applications: a review10.1007/s12540-019-00346-8 ↗
68. Recent progress on corrosion behavior and mechanism of Mg–RE based alloys with long period stacking ordered structure10.1007/s12540-019-00410-3 ↗