journal article·2021-12

Thermal properties, oxidation corrosion behavior, and the in situ ceramization mechanism of SiB6@BPR/HF composites under high-temperature corrosion

Zhenyue Zou, Yan Qin, Chenyi Xue, Di Zhu, Huadong Fu, Zongyi Deng, Zhixiong Huang

Corrosion Science· Volume 193
Publisher page

Abstract

Abstract Pyrolytic carbon generated by phenolic resin at high temperatures is easily oxidized. In this paper, SiB6 @BPR/HF composites were prepared, and their thermal properties, oxidation behavior, and the in situ ceramic mechanism under high-temperature corrosion were studied. The results show that the linear ablation rates of SiB6 @BPR/HF composites can reach 7.5 µm/s, and the mass residual rate can reach 95.5% when the SiB6 content is 50%. Additionally, XRD and XPS analyses showed that there was a complex in situ ceramization reaction to form Si-B-C-O ceramics which prevented the corrosion of composites under an aerobic high-temperature environment of about 1800–1900 °C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Evaluation of the effective properties of high silica/phenolic composite under volumetric ablation condition
2. ZrO2f-coated Cf hybrid fibrous reinforcements and properties of their reinforced ceramicizable phenolic resin matrix composites10.1016/j.jeurceramsoc.2020.08.034 ↗
3. Thermal protection systems for space vehicles: a review on technology development, current challenges and future prospects10.1016/j.actaastro.2020.06.047 ↗
4. Study on improving the high-temperature oxidation resistance of pyrolytic carbons of phenolic resin binder by in-situ formation of carbon nanotubes10.1016/j.reactfunctpolym.2020.104772 ↗
5. Effects of zirconium carbide content on thermal stability and ablation properties of carbon/phenolic composites10.1016/j.ceramint.2019.10.152 ↗
6. The effect of fibre content on properties of ceramifiable composites10.1080/14658011.2020.1731258 ↗
7. Zirconium carbide-modified polymer-matrix composites with improved reflectivity under high-energy laser ablation10.1016/j.ceramint.2019.05.335 ↗
8. Elevated temperature resistance of SiC-carbon/phenolic nanocomposites reinforced with zirconium diboride nanofibers10.1177/0021998317723447 ↗
9. Thermal behavior of phenolic-based ceramizable composites modified by nano-aluminum oxide10.1177/0954008315596800 ↗
10. Morphology measurement on phenolic-resin/vitreous-silica-fabric ablation composites modified with tetraethoxysilicate and silsesquioxanes
11. Effects of SiC content on mechanical, thermal and ablative properties of carbon/phenolic composites10.1016/j.ceramint.2020.03.170 ↗
12. Ablation behavior and mechanism of TaSi2-modified carbon fabric-reinforced phenolic composite10.1007/s10853-020-04636-0 ↗
13. X-ray diffraction and thermodynamics kinetics of SiB6 under gamma irradiation dose10.1007/s12633-018-0039-2 ↗
14. Enhanced mechanical properties of carbon fibre/lithium aluminosilicate composites modified by SiB6 addition10.1080/17436753.2018.1504503 ↗
15. Effect of oxygen partial pressure and temperature on the oxidation behavior of SiB610.1007/s11663-019-01749-z ↗
16. Reaction bonded Si/SiB6: effect of carbon additions on composition and properties
17. Arc jet wind tunnel characterization of ultra-high-temperature ceramic matrix composites10.1016/j.corsci.2018.12.039 ↗
18. Ablation-resistant carbide Zr0.8Ti0.2C0.74B0.26 for oxidizing environments up to 3,000 °C10.1038/ncomms15836 ↗
19. Effect of glass frit with low softening temperature on the properties, microstructure and formation mechanism of polysiloxane elastomer-based ceramizable composites10.1016/j.polymdegradstab.2016.12.012 ↗
20. Oxidation and ablation behaviors of carbon fiber/phenolic resin composites modified with borosilicate glass and polycarbosilane interface10.1016/j.jallcom.2020.154277 ↗
21. Effects of polycarbosilane interface on oxidation, mechanical, and ablation properties of carbon fiber-reinforced composites10.1016/j.ceramint.2018.09.087 ↗
22. Influence of the boundary on the interdiffusion in heterostructures10.1016/0921-5107(94)90163-5 ↗
23. Ignition mechanism of the titanium–boron pyrotechnic mixture10.1002/sia.740110614 ↗
24. Core-electron binding energies for compounds of boron, carbon, and chromium10.1021/ic50085a035 ↗
25. Biased referencing experiments for the XPS analysis of non-conducting materials10.1016/0169-4332(86)90001-2 ↗
26. X‐ray photoelectron spectroscopy investigation of pumice‐supported nickel catalysts10.1002/sia.740230408 ↗
27. An XPS study of amorphous MoO3/SiO films deposited by co-evaporation10.1007/BF01045385 ↗
28. Chemical and tribological studies of MoS2 films on SiC substrates10.1016/0257-8972(90)90009-2 ↗