journal article·2014-07

Electrochemical study of the corrosion of different alloys exposed to deaerated 80°C geothermal brines containing CO2

N. Mundhenk, P. Huttenloch, R. Bäßler, T. Kohl, H. Steger, R. Zorn

Corrosion Science· Volume 84
Publisher page

Abstract

Abstract Corrosion of metallic engineering materials accounts for problems during geothermal operation in the Upper Rhine Graben (URG). Herein, we study the electrochemical behaviour of various metal alloys in an 80 °C simulated geothermal environment by using potentiodynamic polarisation and open-circuit potential measurements. Two different natural geothermal waters from URG geothermal sites were used for the experiments. The measurements reveal spontaneous passivation to be a key process for all alloys. This ennoblement protects more noble alloys from significant corrosion (e.g. titanium gr. 2, alloy 625) and brings less noble alloys to failure, mostly due to pitting corrosion (e.g. 316L).
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Gupta · 2007
2. Chemistry and materials in geothermal systems
3. Ellis · 1977
4. Cyclic polarisation studies on clad and thermal sprayed Ni-base alloys in synthetic geothermal brine
5. Chemistry and isotopes of deep geothermal saline fluids in the Upper Rhine Graben: origin of compounds and water-rock interactions10.1016/0016-7037(93)90387-C ↗
6. Main characteristics of the deep geothermal brine (5km) at Soultz-sous-Forêts (France) determined using geochemical and tracer test data10.1016/j.crte.2009.10.009 ↗
7. Corrosion and scaling as interrelated phenomena in an operating geothermal power plant10.1016/j.corsci.2013.01.003 ↗
8. Effect of CO2 on the stability of steels with 1% and 13% Cr in saline water10.1016/j.corsci.2009.01.025 ↗
9. Spontaneous passivation observations during scale formation on mild steel in CO2 brines10.1016/j.electacta.2011.03.053 ↗
10. Pourbaix · 1973 · 336
11. Synergism of alloying elements and pitting corrosion of stainless steels10.1016/0010-938X(93)90137-6 ↗
12. The role of alloyed molybdenum in the inhibition of pitting corrosion in stainless steels10.1016/S0010-938X(00)00086-X ↗
13. Passive films on stainless steels – chemistry, structure and growth10.1016/S0013-4686(02)00841-1 ↗
14. Reactions of pipeline steels in carbon dioxide solutions10.1016/S0010-938X(98)00104-8 ↗
15. G.S. Frankel, Pitting Corrosion, in: S.D. Cramer, B.S. Covino Jr. (Eds.), Metals Handbook, vol. 13A, ASM International, 2003.
16. Environmental factors affecting the critical potential for pitting in 18-8 stainless steel10.1149/1.2423801 ↗
17. A method to predict pitting corrosion of stainless steels in evaporative conditions10.1016/j.jcsr.2008.07.001 ↗
18. An assessment of the corrosion behaviour of high-grade alloys in seawater at elevated temperature and under a high velocity impinging flow10.1016/0010-938X(96)00180-1 ↗
19. Corrosion studies of austenitic and duplex stainless steels in aqueous lithium bromide solution at different temperatures10.1016/j.corsci.2004.05.025 ↗
20. Effect of temperature on the corrosion resistance and pitting behaviour of alloy 31 in LiBr solutions10.1016/j.corsci.2008.03.016 ↗
21. R. Bäßler, A. Burkert, R. Kirchheiner, A. Saadat, M. Finke, in: Proceedings of NACE Corrosion 2009, Paper No. 09377, NACE International, Atlanta, 2009.
22. Pitting corrosion of stainless steels10.1002/maco.19960470104 ↗
23. Sedriks · 1979
24. ASTM G5-82, Standard practice for standard reference method for making potentiostatic and potentiodynamic anodic polarisation measurements, in: G.S. Haynes, R. Baboian (Eds.), Laboratory Corrosion Tests and Standards. ASTM Committee G-1 on corrosion of metals, ASTM special technical publication 866, 1985.
25. A. Roine, Outokumpu HSC Chemistry_6.0 User’s Guide Volume 1/2 – Chemical Reaction and Equilibrium Software with Extensive Thermochemical Database and Flowsheet Simulation Outokumpu Research Finland, 2006.
26. Pourbaix diagrams for chromium, aluminum and titanium extended to high-subcritical and low-supercritical conditions10.1016/j.corsci.2012.02.002 ↗
27. The use of potential-pH diagrams for the interpretation of corrosion phenomena in high salinity geothermal brines10.5006/0010-9312-35.1.1 ↗
28. An assessment of the corrosion behaviour of high-grade alloys in seawater at elevated temperature and under high velocity impinging flow10.1016/j.biomaterials.2004.02.023 ↗
29. Surface modification of titanium alloys for combined improvements in corrosion and wear resistance10.1016/S0257-8972(98)00580-5 ↗
30. Critical pitting and repassivation temperatures for duplex stainless steel in chloride solutions10.1016/j.electacta.2008.02.047 ↗
31. H.S. Klapper, R. Baessler, K. Weidauer, D. Stuerzbecher, Evaluation of suitability of high-alloyed materials for geothermal applications in the North German basin, in: Proceedings of the NACE 2011, vol. 68, NACE International, Houston, TX, 2011.10.5006/1.3676631 ↗