journal article·2014-07

Effects of Al, Ti, and Zr doping on oxide film formation in Co–29Cr–6Mo alloy used as mould material for Al die-casting

Yunping Li, Phacharaphon Tunthawiroon, Ning Tang, Huakang Bian, Fenglin Wang, Shihai Sun, Yan Chen, Kazuyo Omura, Yuichiro Koizumi, Akihiko Chiba

Corrosion Science· Volume 84
Publisher page

Abstract

Abstract The reactive-element (RE) effect in chromia-forming-alloys on the adherence properties of the oxide scale is well known. A comparative study of chromia scale in four Co–Cr–Mo alloys, an undoped and three doped with 0.5 wt% Al/Ti/Zr, is conducted under FESEM/EPMA, LSM, and XPS. After air oxidation at 700 °C for 24 h, all doped alloys show a thinner, smoother oxide scale with enhanced adherence. The cross-sectional compositional maps show significant increase in the concentration of Ti in the oxide scale, and Al near the oxide/alloy interface. The reactive elements inhibited the diffusion of Cr and O ions, formed oxide preferentially, and eliminated the void formation at the oxide/alloy interface.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Metallurgical Processes and Thermodynamics · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. Review durability of materials in molten aluminum alloys10.1023/A:1004843621542 ↗
2. J. Mihelich, R.F. Decker, US Patent No. 5711366, 1998.
3. A novel C-free Co-based alloy for high temperature tooling applications10.1016/j.msea.2010.10.037 ↗
4. Interfacial reactions of solid Co and solid Fe with liquid Al10.1016/j.corsci.2012.04.015 ↗
5. Effect of nitriding treatment on corrosion behaviour of Co–Cr–Mo alloy in liquid Al10.1016/j.corsci.2013.10.004 ↗
6. Interfacial reaction between Co–Cr–Mo alloy and liquid Al10.1016/j.corsci.2013.06.009 ↗
7. Interfacial reactions between molten al and a Co–Cr–Mo alloy with and without oxidation treatment10.1016/j.corsci.2011.08.015 ↗
8. High-temperature oxidation of Co–10w/o Cr alloys: I. Microstructure of oxide scales10.1149/1.2411802 ↗
9. High-temperature oxidation of Co–10w/o Cr alloys: II. Oxidation kinetics10.1149/1.2411803 ↗
10. Oxidation of Co–25w/o Cr at high temperature10.1149/1.2411603 ↗
11. Discussion of oxidation of Co–25w/o Cr at high temperature10.1149/1.2407372 ↗
12. Oxidation of a Co-based super alloy
13. Diffusion and oxidation of solid metals10.1021/ie50521a023 ↗
14. Kofstad · 1966
15. The influence of manganese and silicon on the oxidation behavior of Co–Cr alloys10.1007/BF00603486 ↗
16. The kinetics of the oxidation of cobalt10.1149/1.2778139 ↗
17. The oxidation of cobalt–tungsten alloys10.1016/0010-938X(76)90032-9 ↗
18. Study on the surface oxidation of Co–Cr films10.1109/20.104835 ↗
19. G.C. Mechler, Manufacturing and Cost Analysis for Aluminum and Copper Die Cast Induction Motors for GM’s Powertrain and R&D Divisions, Thesis for Bachelor’s degree, University of Arizona, September 2010.
20. Differences in growth mechanisms of oxide scales formed on ODS and conventional wrought alloys10.1007/BF00665269 ↗
21. The effect of yttrium and thorium on the oxidation behavior of Ni–Cr–Al alloys10.1007/BF00604042 ↗
22. Characterisation of oxide films formed on Co–29Cr–6Mo alloy used in die-casting moulds for aluminium10.1016/j.corsci.2013.03.026 ↗
23. Growth mechanism of Cr2O3 scales: oxygen and chromium diffusion, oxidation kinetics and effect of yttrium10.1016/0921-5093(96)10173-8 ↗
24. The effect of implanted lanthanum on chemical diffusion in Cr2O3-scales on Co–40Cr alloy10.1016/0167-2738(92)90005-A ↗
25. High temperature oxidation of alloys
26. A theory of the formation of protective oxide films on metals10.1039/tf9393501175 ↗
27. Transport processes during the growth of oxide films at elevated temperature10.1103/RevModPhys.57.437 ↗
28. The protective action of oxide scales in gaseous environments at high temperature10.1088/0034-4885/50/7/002 ↗
29. Effect of Sm, Gd, Yb, Sc and Nd as reactive elements on oxidation behaviour of β-NiAl at 1200 °C10.1016/j.corsci.2013.10.021 ↗
30. Experimental observation in support of the dynamic-segregation theory to explain the reactive-element effect10.1007/BF01046818 ↗
31. The role of alloying elements in the initiation of nanoscale porosity in oxide films formed on zirconium alloys10.1016/j.corsci.2013.08.006 ↗
32. Corrosion behavior of chromium oxide based ceramics in supercritical water (SCW) environments10.1016/j.corsci.2012.08.048 ↗
33. Analytical models for the internal oxidation of a binary alloy that forms oxide precipitates of high stability10.1016/j.corsci.2013.03.028 ↗
34. Effect of thermal stability of the amorphous substrate on the amorphous oxide growth on Zr–Al–(Cu, Ni) metallic glass surfaces10.1016/j.corsci.2013.04.009 ↗
35. Effects of pH value on characteristics of oxide films on 316L stainless steel in Zn-injected borated and lithiated high temperature water10.1016/j.corsci.2013.09.017 ↗
36. Microstructure and protection characteristics of the naturally formed oxide films on Mg–xZn alloys10.1016/j.corsci.2013.03.021 ↗
37. Time dependence of growth and crystallization of anodic titanium oxide films in potentiostatic mode10.1016/j.corsci.2013.06.004 ↗
38. Determination of diffusion induced concentration profiles in Cr2O3 films on ceramic Al2O3 by Auger sputter depth profiling10.1007/BF00321316 ↗
39. Room temperature strains in Cr2O3 scales formed at elevated temperatures on Ni–25wt%Cr and Y- and Al-doped Ni–25Cr10.1016/0956-7151(91)90284-8 ↗
40. Effects of aluminum diffusion on the adhesive behaviour of the Ni(111)/Cr2O3(0001) interface: First principle study10.1016/j.commatsci.2013.05.037 ↗
41. The cyclic oxidation behavior of α-Cr+β-NiAl alloys with and without trace Zr addition10.1016/S0010-938X(96)00149-7 ↗
42. Aluminum oxide adherence on Fe–Cr–Al alloys modified with group IIIB, IVB, VB, and VIB elements10.1007/BF00665442 ↗
43. Effectiveness of 0.1at.% Ziroconium on the cyclic oxidation resistance of β-NiAl10.1007/BF00659006 ↗
44. Effect of La and Zr addition on high temperature oxidation resistance of 20%Cr–5%Al steel foils