Water vapour effects on corrosion of Ni-Cr alloys in CO2 gas at 650 °C
Source abstract
Abstract
Abstract Binary Ni-Cr alloys containing 5–30 wt% Cr were oxidized in Ar-20CO 2 -20H 2 O gas at 650 °C. Weight gain kinetics for alloys reacted with electropolished surfaces generally increased with increasing Cr content up to 25 wt%. All alloys underwent both internal oxidation and outer NiO formation. The NiO developed as separated, isolated growths on all alloys. Internal oxide zones on high chromium alloys underwent buckling. Weight gain and internal oxidation rates were slower than in dry Ar-20CO 2 . These differences are discussed in terms of altered diffusion processes in NiO in the presence of H 2 O, and displacement of metal from the internal oxidation zone.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Advanced materials and composites · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Effect of surface condition on steam oxidation of martensitic steels and nickel-based alloys10.5006/1859 ↗
2. Future directions in the field of high-temperature corrosion research10.1007/s11085-017-9719-3 ↗
3. The oxidation behaviour of the 9% Cr steel P92 in CO2- and H2O-rich gases relevant to oxyfuel environments10.3139/146.110271 ↗
4. Scale formation mechanisms of martensitic steels in high CO2/H2O-containing gases simulating oxyfuel environments10.3184/096034009X438185 ↗
5. Carburisation of ferritic Fe-Cr alloys by low carbon activity gases10.1016/j.corsci.2011.05.013 ↗
6. Mechanism of breakaway oxidation of Fe-Cr and Fe-Cr-Ni alloys in dry and wet carbon dioxide
7. Characteristic scales on pure nickel-chromium alloys at 800°–1200 °C10.1149/1.2423955 ↗
8. Oxidation of Ni-Cr alloys between 800° and 1200 °C
9. Temperature effect on oxidation behavior of Ni-Cr alloys in CO2 gas atmosphere10.1149/2.1021706jes ↗
10. Effect of water vapour on growth and adherence of chromia scales formed on Cr in high and low pO2-environments at 1000 and 1050 °C10.3184/096034005782744443 ↗
11. Protective and non-protective scale formation of NiCr alloys in water vapour containing high- and low-pO2 gases10.1016/j.corsci.2008.03.001 ↗
12. Effect of in-situ gas changes on thermally grown chromia scales formed on Ni-25Cr alloy at 1000 °C in atmospheres with and without water vapour10.1179/0960340914Z.000000000108 ↗
13. Effect of H2/H2O ratio on thermally grown chromia scales formed on Ni25Cr alloy in Ar-H2-H2O atmospheres at 1000 °C10.3184/096034012X13322698137785 ↗
14. The role of oxide microstructure and growth stresses in the high-temperature scaling of nickel10.1007/BF02642020 ↗
15. On the high-temperature oxidation of nickel10.1016/S0010-938X(02)00085-9 ↗
16. Internal oxidation of Ni-Al and Ni-Al-Si alloys at the dissociation pressure of NiO10.1016/0956-7151(94)90292-5 ↗
17. ImageJ for microscopy10.2144/000112517 ↗
18. The diffusion and solubility of oxygen in solid nickel10.1007/BF02646220 ↗
19. Young · 2016
20. Reaktionstypen bei der oxydation von legierungen
21. Enhanced diffusion of oxygen during internal oxidation of nickel-base alloys10.1080/01418618208236942 ↗
22. Internal oxidation in dry and wet conditions for oxygen permeability of Fe-Ni alloys at 1150 and 1100 °C10.1007/s11085-017-9724-6 ↗
23. Tracer diffusion in the chromium-nickel system10.1002/pssa.2210080230 ↗
24. The high-temperature internal oxidation and intergranular oxidation of nickel-chromium alloys10.1016/0010-938X(83)90056-2 ↗
25. Scale formation of alloy 602 CA during isothermal oxidation at 800–1100 °C in different types of water vapor containing atmospheres10.1007/s11085-015-9595-7 ↗
26. Über die innere oxydation von metallegierungen10.1016/0001-6160(64)90036-7 ↗
27. Thermo-Calc & DICTRA, computational tools for materials science10.1016/S0364-5916(02)00037-8 ↗
28. Precipitation and solid solubility in the system NiO-Cr2O310.1111/j.1151-2916.1983.tb10092.x ↗