Abstract Several K-Ca-Si glass compositions typical of Central-European glassworks are susceptible to damage beyond recall, even in mild museum conservative conditions. In order to provide a comprehensive picture of the deterioration process, replica samples were produced and exposed to four different museum-like environments. The corrosion experiment was followed by the use of ToF-SIMS, μ-Raman and μ-FTIR, performing a systematic compositional and structural study for the early stages (one year) of surface alteration. This work demonstrates the dominant role of Pb2+ and Ca2+ content for the inferable existence of connected conduction pathways, with strong implications on the surface's hydration, alkali-diffusion and hydrolysis.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Cultural Heritage Materials Analysis · Building materials and conservation · Conservation Techniques and Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (86)

Show source-provided references
1. A comparative analytical investigation on the origins of the Venetian glassmaking
2. Weathering of glass in moist and polluted air10.1016/S0168-583X(97)00758-1 ↗
3. Glass of the past: the degradation and deterioration of medieval glass artifacts10.1007/BF01245513 ↗
4. Effects of humidity on the weathering of glass10.1016/0022-3093(75)90084-8 ↗
5. Characterisation of an intermediate decay phenomenon of historical glasses10.1007/s10853-005-3948-6 ↗
6. Clark · 1979
7. Paul · 1990
8. Quantitative characterization of surface layers on corroded medieval window glass with SIMS
9. The effect of corrosion on stained glass windows10.3989/mc.1996.v46.i242-243.527 ↗
10. A comparative study of the natural and experimental corrosion of poorly durable potash-lime-silica glasses
11. Tapping-mode AFM in comparison to contact-mode AFM as a tool for in situ investigations of surface reactions with reference to glass corrosion10.1021/ac9607020 ↗
12. Using stained glass windows to understand the durability of toxic waste matrices10.1016/S0009-2541(00)00315-6 ↗
13. Ion beam and infrared analysis of medieval stained glass10.1007/s00339-004-2538-9 ↗
14. Statistical evaluation of potash-lime-silica glass weathering10.1007/s00216-004-2595-0 ↗
15. Evaluation procedure for leaching studies on naturally weathered potash-lime-silica glasses with medieval composition by scanning electron microscopy10.1016/j.jnoncrysol.2005.02.020 ↗
16. Corrosion behaviour of R2O–CaO–SiO2 glasses submitted to accelerated weathering10.1016/j.jeurceramsoc.2004.05.004 ↗
17. Characterization of potash-glass corrosion in aqueous solution by ion beam and IR spectroscopy10.1016/j.jnoncrysol.2006.08.032 ↗
18. The effect of Mn, Fe and Cu ions on potash-glass corrosion10.1016/j.jnoncrysol.2009.05.051 ↗
19. Early stage of weathering of medieval-like potash-lime model glass: evaluation of key factors10.1007/s11356-010-0370-7 ↗
20. Corrosion of 15th and early 16th century stained glass from the monastery of Batalha studied with external ion beam10.1016/j.matchar.2010.12.001 ↗
21. ToF-SIMS analysis for leaching studies of potash-lime-silica glass10.1016/j.apsusc.2013.05.101 ↗
22. Long-term weathering rate of stained-glass windows using H and O isotopes10.1038/s41529-018-0038-1 ↗
23. Leaching studies on naturally weathered potash-lime-silica glasses10.1016/j.jnoncrysol.2006.01.017 ↗
24. The development of an ion chromatography protocol for detecting the early stages of glass degradation
25. Weeping glass: the identification of ionic species on the surface of vessel glass using ion chromatography
26. Unstable historic glass: symptoms, causes, mechanisms and conservation
27. Characterization of glass surface morphology by optical coherence tomography10.1179/sic.2009.54.2.117 ↗
28. Modern and ancient glass: nature, composition and deterioration mechanisms
29. Section 1. Water and glass, durability, and transport phenomena – glass-water interactions10.1016/0022-3093(88)90105-6 ↗
30. Understanding glass deterioration in museum collections: a multi-disciplinary approach
31. Molecular mechanisms for corrosion of silica and silicate glasses10.1016/0022-3093(94)90708-0 ↗
32. Water diffusion in silicate glasses under natural weathering conditions: evidence from buried medieval stained glasses10.1016/j.jnoncrysol.2006.08.041 ↗
33. Theory of corrosion of glass and ceramics
34. Doremus · 1994
35. Glass corrosion mechanisms: a multiscale analysis10.1016/j.ssi.2008.07.019 ↗
36. The influence of selected organic compounds on the corrosion of historical glass based on their state of preservation10.12693/APhysPolA.130.1406 ↗
37. Leach testing of model glasses containing sodium or potassium ions as a flux
38. A study of eighteenth century glass vessels from central Europe by X-ray fluorescence analysis10.1002/1097-4539(200007/08)29:4<310::AID-XRS431>3.0.CO;2-E ↗
39. Some observations on crizzled glass (preliminary results of a survey of 18th century central European tableware)
40. Ultraviolet blue fluorescence of the 18th century Central European glass: an auxiliary indicator for curators and conservators
41. Late 17th century glass vessels from Eiland – technological approach
42. L’invenzione del cristallo muranese: una verifica analitica delle fonti storiche
43. Lead in central European 18th century colourless vessel glass
44. Eiland: Georg Gundelach and the Glasswork on the Decin Estate of Count Mazimilian Thun-Hohenstein
45. Analyses of 18th-century central European colourless glass vessels
46. Fungal biodeterioration of stained-glass windows10.1016/j.ibiod.2014.03.007 ↗
47. Moisture attack on museum glass measured by SIMS
48. Early stages of surface alteration of soda-rich-silicate glasses in the museum environment10.1016/j.corsci.2018.08.012 ↗
49. Contribution of atom-probe tomography to a better understanding of glass alteration mechanisms: application to a nuclear glass specimen altered 25 years in a granitic environment10.1016/j.chemgeo.2013.04.001 ↗
50. Atom-probe tomography, TEM and ToF-SIMS study of borosilicate glass alteration rim: a multiscale approach to investigating rate-limiting mechanisms10.1016/j.gca.2016.12.029 ↗
51. The use of Raman spectrometry to predict the stability of historic glasses10.1002/jrs.1540 ↗
52. Correlations between Raman parameters and elemental composition in lead and lead alkali silicate glasses10.1002/jrs.1894 ↗
53. Raman identification of glassy silicates used in ceramics, glass and jewellery: a tentative differentiation guide10.1002/jrs.1515 ↗
54. Non-destructive determination of the structure and composition of glazes by Raman spectroscopy10.1111/j.1551-2916.2005.00096.x ↗
55. Polymerization degree and Raman identification of ancient glasses used for jewelery, ceramic enamels and mosaics10.1016/S0022-3093(03)00303-X ↗
56. The controversial role of inter-diffusion in glass alteration10.1016/j.chemgeo.2016.07.014 ↗
57. Dynamics of self-reorganization explains passivation of silicate glasses10.1038/s41467-018-04511-2 ↗
58. Properties of glass surfaces10.1146/annurev.ms.02.080172.002525 ↗
59. Physical chemistry of glass surfaces10.1016/0022-3093(78)90077-7 ↗
60. Use of FTIR reflectance spectroscopy to monitor corrosion mechanisms on glass surfaces10.1016/j.jnoncrysol.2007.05.012 ↗
61. What can vibrational spectroscopy tell about the structure of dissolved sodium silicates?10.1016/j.micromeso.2010.06.013 ↗
62. Derrick · 1999
63. Infrared reflectivity spectroscopy of silicate glasses10.1016/S0022-3093(87)80280-6 ↗
64. IR absorption spectra of vitreous silica and silicate glasses: the nature of bands in the 1300 to 5000 cm−1 region10.1016/j.chemgeo.2006.01.022 ↗
65. Alteration of soda silicate glasses by organic pollutants in museums: mechanisms and kinetics10.1016/j.jnoncrysol.2009.05.011 ↗
66. Structure-property relationships in multicomponent oxide glasses10.1016/S1631-0748(02)01459-5 ↗
67. Applying FTIR spectroscopy in the study of archeometric sensor glasses10.1016/S0022-2860(99)00160-X ↗
68. Structural studies of silicate glasses and melts—applications and limitations of Raman spectroscopy
69. Structure and chemical durability of lead crystal glass10.1021/acs.est.6b02971 ↗
70. Potash-lime-silica glass: protection from weathering10.1186/s40494-015-0051-4 ↗
71. Evolution of the adsorbed water layer structure on silicon oxide at room temperature10.1021/jp053042o ↗
72. New insight into atmospheric alteration of alkali-lime silicate glasses10.1016/j.corsci.2017.03.025 ↗
73. Sub-critical crack growth in silicate glasses: role of network topology10.1063/1.4932377 ↗
74. Channel formation and intermediate range order in sodium silicate melts and glasses10.1103/PhysRevLett.93.027801 ↗
75. Recent progress to understand stress corrosion cracking in sodium borosilicate glasses: linking the chemical composition to structural, physical and fracture properties10.1088/1361-6463/aa7a8b ↗
76. Sodium and hydrogen analysis of room temperature glass corrosion using low energy Cs SIMS10.1016/j.apsusc.2006.02.101 ↗
77. Characterization of some glasses in the system SiO2, Na2O·RO by infrared spectroscopy10.1016/S0254-0584(02)00215-8 ↗
78. Origin and consequences of silicate glass passivation by surface layers10.1038/ncomms7360 ↗
79. Volf · 1984
80. Lead monoxide. Electronic structure and bonding10.1021/j150670a038 ↗
81. Coordination of Pb2+ in oxide glasses determined by ESR and properties of binary lead glasses
82. X-ray diffraction and EXAFS studies of silicate glasses containing Mg, Ca and Ba atoms10.1016/S0022-3093(96)00632-1 ↗
83. Computational simulations of solid state NMR spectra: a new era in structure determination of oxide glasses10.1039/c3ra40627j ↗
84. The structure of silicate glasses and melts10.2113/gselements.2.5.269 ↗
85. A comparative review of the aqueous corrosion of glasses, crystalline ceramics, and metals10.1038/s41529-018-0037-2 ↗
86. Cleaning glass: a many-faceted issue