Corrosion mechanisms of 316L stainless steel in supercritical water: The significant effect of work hardening induced by surface finishes
Source abstract
Abstract
Abstract The oxidation of 316 L stainless steel in hydrogenated supercritical water at 600 °C is strongly dependent on the effects of work hardening induced by surface finishes. The oxide scale formed under these conditions is always double-layered with an external layer of Fe-rich oxides. However, when a hardening threshold is reached, a switch in oxidation mechanisms leads to a considerable thinning of the oxide scale. This thinning results from the formation of a Cr-rich internal oxide layer that acts as a diffusion barrier against ionic species responsible for its growth but also against Fe cations implied in the external layer growth.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Subcritical and Supercritical Water Processes · High-Temperature Coating Behaviors · Advanced Materials Characterization Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. Materials for high performance light water reactors10.1016/j.jnucmat.2004.01.020 ↗
2. Materials challenges for generation IV nuclear energy systems10.13182/NT08-A3961 ↗
3. Corrosion and stress corrosion cracking in supercritical water10.1016/j.jnucmat.2007.05.017 ↗
4. Corrosion of candidate materials for use in a supercritical water CANDU® reactor
5. High burnup fuel cladding materials R&D for advanced nuclear systems – nano-sized oxide dispersion strengthening steels10.1080/18811248.2007.9711289 ↗
6. Oxidation behaviour of iron-based alloy HCM12A exposed in supercritical water10.1016/j.corsci.2005.10.010 ↗
7. The effect of surface finish on the scaling behavior of stainless steel in steam and supercritical water10.1007/s11085-013-9380-4 ↗
8. Corrosion mechanism of a Ni-based alloy in supercritical water: impact of surface plastic deformation10.1016/j.corsci.2015.06.032 ↗
9. Corrosion properties of oxide dispersion strengthened steels in super-critical water environment10.1016/j.jnucmat.2004.04.040 ↗
10. Estimation of kinetic parameters of the corrosion layer constituents of steels in supercritical water coolant conditions10.1016/j.corsci.2011.08.029 ↗
11. Effect of thermo-mechanical processing on oxidation of austenitic stainless steel 316L in supercritical water10.1016/j.corsci.2015.02.008 ↗
12. The mechanism of high temperature aqueous corrosion of stainless steels10.1016/0010-938X(91)90125-9 ↗
13. The mechanism of oxide film formation on austenitic stainless steels in high temperature water10.1016/S0010-938X(97)00140-6 ↗
14. Influence of irradiation on the oxide film formed on 316 L stainless steel in PWR primary water10.1007/s11085-013-9401-3 ↗
15. Field investigation of steamside oxidation for TP347H10.4028/www.scientific.net/MSF.461-464.1007 ↗
16. Initial oxidation and chromium diffusion. I. Effects of surface working on 9–20% Cr steels10.1016/j.corsci.2003.09.004 ↗
17. Corrosion of stainless steel in high temperature water10.2320/matertrans1960.5.22 ↗
18. Effect of implantation defects on the corrosion of 316L stainless steels in primary medium of pressurized water reactors10.1016/j.corsci.2016.02.007 ↗
19. Effect of shot-peening on the oxidation of alloy 800H exposed to supercritical water and cyclic oxidation10.1016/j.corsci.2008.04.008 ↗
20. Oxidation kinetics and mechanisms of Ni-base alloys in pressurised water reactor primary conditions: influence of subsurface defects10.1016/j.corsci.2011.07.024 ↗
21. Corrosion of nickel base alloys in PWR primary medium: new insights on the oxide growth mechanisms and kinetic modelling10.1016/j.corsci.2015.09.001 ↗
22. Oxidation of ferritic–martensitic alloys T91, HCM12A, and HT-9 in supercritical water10.1016/j.jnucmat.2007.05.023 ↗
23. Cycle chemistry and its effect on materials in a supercritical water-cooled reactor: a synthesis of current understanding10.1016/j.corsci.2012.08.006 ↗
24. Use of oxygen to study the transport mechanism during high temperature oxide scale growth10.1179/mht.2003.029 ↗
25. Carrette · 2002
26. An improved technique for determining hardness and elastic Modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
27. 2017
28. Vibrational modeling of the thermodynamic properties of magnetite at high pressure from Ramn spectroscopic study10.1063/1.1602072 ↗
29. Raman spectroscopy of titanomagnetites: calibration of the intensity of Raman peaks as a sensitive indicator for their Ti content10.2138/am.2011.3745 ↗
30. Oxidation behavior of ferritic–martensitic and ODS steels in supercritical water10.1016/j.jnucmat.2012.03.009 ↗
31. Characterization of oxide films grown on 316L stainless steel exposed to H2O2-containing supercritical water10.1016/j.supflu.2006.12.020 ↗
32. Corrosion behaviour of ferritic-martensitic steel T91 in supercritical water10.1016/j.corsci.2005.08.021 ↗
33. Hydrogen absorption associated with the corrosion mechanism of 316L stainless steels in primary medium of Pressurized Water Reactor (PWR)10.1016/j.corsci.2014.04.025 ↗
34. Fine structure of austenite produced by the reverse martensitic transformation10.1016/0001-6160(63)90085-3 ↗
35. Reverse martensitic transformation and resulting microstructure in a cold rolled metastable austenitic stainless steel10.1002/srin.200806149 ↗
36. A mechanism for the strain-induced nucleation of martensitic transformation10.1016/0022-5088(72)90173-7 ↗
37. Influence of the cold working induced martensite on the electrochemical behavior of AISI 304 stainless steel surfaces10.1016/j.jmrt.2018.10.004 ↗
38. Anomalous temperature dependence of oxidation kinetics during steam oxidation of ferritic steels in the temperature range 550–650 °C10.1016/j.corsci.2004.01.010 ↗
39. Growth mechanism of Cr2O3 scales: oxygen and chromium diffusion, oxidation kinetics and effect of yttrium10.1016/0921-5093(96)10173-8 ↗
40. Diffusion of iron in Cr2O3: polycristals and thin films10.1016/j.msea.2004.09.033 ↗
41. 55Fe diffusion in magnetite crystals at 500°C and its relevance to oxidation of iron10.1007/BF00541841 ↗
42. Creep and oxygen diffusion in magnetite10.1016/0956-7151(90)90268-L ↗
43. Mechanism of hydrogen absorption during the exposure of alloy 600-like single-crystals to PWR primary simulated media10.1016/j.jnucmat.2011.04.066 ↗
44. Characterization of oxygen and hydrogen migration through oxide scales formed on nickel-base alloys in PWR primary medium conditions10.1016/j.ssi.2012.10.012 ↗
45. Stress corrosion cracking of uni-directionally cold worked 316NG stainless steel in simulated PWR primary water with various dissolved hydrogen concentrations10.1016/j.corsci.2011.04.013 ↗
46. Stress corrosion cracking on irradiated 316 stainless steel10.1016/S0022-3115(00)00704-2 ↗
47. Irradiation-assisted stress corrosion cracking of austenitic alloys in supercritical water10.1016/j.jnucmat.2009.09.010 ↗
48. Stress corrosion cracking behavior of annealed and cold worked 316L stainless steel in supercritical water10.1016/j.nucengdes.2016.06.022 ↗