journal article·2019-12

Effect of exposure temperature on the corrosion behaviors of TP347H austenitic stainless steel in supercritical water

Hongsheng Chen, Rui Tang, Chongsheng Long, Guan Le

Corrosion Science· Volume 161
Publisher page

Abstract

Abstract Corrosion behaviors of TP347H austenitic stainless steel were investigated in supercritical water at different temperatures. Results show that weight gains follow roughly parabolic kinetics except after 1800 h exposure at 650 °C. Some outer isolated Fe2O3 particles are interspersed on the inner nano-sized spinel scale at 380 °C. At 550 °C, the oxide layer with outer magnetite and inner spinel gradually increases and the (Fe,Cr)2O3 layer decreases with exposure time increasing. At 650 °C, the thick magnetite layer is firstly formed and then spalled associating with a chromia layer generated at the spinel/matrix interface, resulting in significant weight loss.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Subcritical and Supercritical Water Processes · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Material performance in supercritical water
2. Progress in corrosion resistant materials for supercritical water reactors10.1016/j.corsci.2009.07.007 ↗
3. Corrosion and stress corrosion cracking in supercritical water10.1016/j.jnucmat.2007.05.017 ↗
4. Corrosion behavior of austenitic and ferritic steels in supercritical water10.5516/NET.2008.40.2.147 ↗
5. Construction of dynamic model of CANDU-SCWR using moving boundary method10.1016/j.nucengdes.2011.02.017 ↗
6. Effect of dissolved oxygen content on the oxide structure of Alloy 625 in supercritical water environments at 700 °C10.1016/j.corsci.2013.11.034 ↗
7. Conceptual fuel channel designs for CANDU-SCWR10.5516/NET.2008.40.2.139 ↗
8. Mechanical properties of fuel cladding candidate alloys for Canadian SCWR concept10.1007/s11837-015-1725-9 ↗
9. Corrosion in high-temperature and supercritical water and aqueous solutions: a review10.1016/S0896-8446(03)00031-7 ↗
10. Corrosion behavior of ferritic/martensitic steel P92 in supercritical water10.1016/j.supflu.2009.06.019 ↗
11. Effects of exposure temperature and time on corrosion behavior of a ferritic–martensitic steel P92 in aerated supercritical water10.1016/j.corsci.2014.10.022 ↗
12. Oxidation of ferritic and ferritic–martensitic steels in flowing and static supercritical water10.1016/j.corsci.2015.10.017 ↗
13. Corrosion behavior of 9–12% Cr ferritic–martensitic steels in supercritical water10.1016/j.corsci.2009.12.032 ↗
14. Investigation on early formation and evolution of oxide scales on ferritic–martensitic steels in supercritical water10.1016/j.corsci.2018.02.036 ↗
15. Effect of thermo-mechanical processing on oxidation of austenitic stainless steel 316L in supercritical water10.1016/j.corsci.2015.02.008 ↗
16. Corrosion of austenitic and ferritic-martensitic steels exposed to supercritical carbon dioxide10.1016/j.corsci.2011.06.002 ↗
17. Corrosion behavior of alloy 316L stainless steel after exposure to supercritical water at 500 °C for 20000 h10.1016/j.supflu.2017.03.022 ↗
18. Corrosion of austenitic alloys in supercritical water10.5006/1.3278237 ↗
19. Corrosion behavior of alloy 800H (Fe–21Cr–32Ni) in supercritical water10.1016/j.corsci.2010.10.021 ↗
20. Corrosion of engineering materials in a supercritical water cooled reactor: characterization of oxide scales on Alloy 800H and stainless steel 31610.1016/j.corsci.2015.07.035 ↗
21. A comparative study of oxide scales grown on stainless steel and nickel-based superalloys in ultra-high temperature supercritical water at 800 °C10.1016/j.corsci.2016.02.004 ↗
22. Characterization of Ni–20Cr–5Al model alloy in supercritical water10.1016/j.jnucmat.2013.11.011 ↗
23. Corrosion behavior of Hastelloy C-276 in supercritical water10.1016/j.corsci.2009.05.041 ↗
24. Corrosion behavior of alloys 625 and 718 in supercritical water10.5006/1.3278410 ↗
25. Corrosion behavior of Alloy 690 in aerated supercritical water10.1016/j.corsci.2012.10.001 ↗
26. The effect of thermal cycling on steam oxidation behaviour of TP347H FG at 650 °C10.1080/09603409.2017.1389380 ↗
27. Microstructural investigation of the oxide formed on TP 347H FG during long-term steam oxidation10.1002/maco.200905439 ↗
28. Long term steam oxidation of TP 347H FG in power plants10.3184/096034005782744407 ↗
29. Early oxidation mechanism of austenitic stainless steel TP347H in supercritical water10.1016/j.corsci.2017.09.023 ↗
30. Corrosion and stress corrosion cracking susceptibility of type 347H stainless steel in supercritical water10.5006/2459 ↗
31. Oxidation of austenitic steel TP347HFG exposed to supercritical water with different dissolved oxygen concentration
32. Corrosion and microstructural analysis data for AISI 316L and AISI 347H stainless steels after exposure to a supercritical water environment10.1016/j.dib.2016.04.013 ↗
33. Birks · 2006
34. Young · 2008
35. ASM International · 1987
36. Dayananda · 1987
37. Self-diffusion in compounds with spinel structure10.1080/14786437208229215 ↗
38. Anion diffusion in α‐Cr2O310.1111/j.1151-2916.1965.tb11802.x ↗
39. Corrosion behaviors of four stainless steels with similar chromium content in supercritical carbon dioxide environment at 650° C10.1016/j.corsci.2019.04.043 ↗
40. Microstructural characteristics of oxide scales grown on stainless steel exposed to supercritical water10.1016/j.scriptamat.2009.08.013 ↗
41. The role of oxide grain boundaries in the development of growth stresses during oxidation10.1016/0010-938X(83)90099-9 ↗
42. Oxidation behavior of Fe-20Cr-25Ni-Nb austenitic stainless steel in high-temperature environment with small amount of water vapor10.1016/j.corsci.2018.09.016 ↗
43. Schutze · 1997
44. A model for mild steel oxidation in CO210.1007/BF00610578 ↗
45. Corrosion of 9Cr steel in CO2 at intermediate temperature I: mechanism of void-induced duplex oxide formation10.1007/s11085-011-9271-5 ↗
46. Corrosion of 9Cr Steel in CO2 at intermediate temperature III: modelling and simulation of void-induced duplex oxide growth10.1007/s11085-011-9273-3 ↗
47. Microstructural characteristics of the oxide scale formed on 304 stainless steel in oxygenated high temperature water10.1016/j.corsci.2010.07.015 ↗
48. Analysis of oxide film formed on type 304 stainless steel in 288 °C water containing oxygen, hydrogen, and hydrogen peroxide10.5006/1.3283969 ↗
49. Effects of hydrogen peroxide on corrosion of stainless steel, (V) characterization of oxide film with multilateral surface analyses10.1080/18811248.2006.9711173 ↗
50. Oxidation of Ni-Cr alloy at intermediate oxygen pressures. I. Diffusion mechanisms through the oxide layer10.1016/j.corsci.2016.05.025 ↗
51. Oxidation behavior of iron-based alloy HCM12A exposed in supercritical water10.1016/j.corsci.2005.10.010 ↗