Reason for negative effect of Nb addition on oxidation resistance of alumina-forming austenitic stainless steel at 1323 K
Source abstract
Abstract
Abstract To know reason for negative effect of Nb addition on oxidation resistance in alumina-forming austenitic stainless steels at high temperature, effects of Nb addition on microstructural evolution and oxidation resistance were investigated in Fe-25Ni-10Cr-4.5Al based steels after oxidation at 1323 K. The results showed that the degraded oxidation resistance due to the Nb addition resulted from suppressed outward diffusion of Al atoms by formation of Fe2Nb phase. Pre-aging at 1223 K could improve the oxidation resistance of the Nb-containing Fe-25Ni-10Cr-4.5Al steel due to the pre-precipitated B2-NiAl phase.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · High Temperature Alloys and Creep · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Precipitation in creep resistant austenitic stainless steels10.1179/026708301101508972 ↗
2. Creep-resistant, Al2O3-forming austenitic stainless steels10.1126/science.1137711 ↗
3. Recent developments in stainless steels10.1016/j.mser.2009.03.001 ↗
4. Creep-strengthening of steel at high temperatures using nano-sized carbonitride dispersions10.1038/nature01740 ↗
5. The use of model alloys to develop corrosion-resistant stainless steels
6. Volatility of common protective oxides in high-temperature water vapor: current understanding and unanswered questions10.4028/www.scientific.net/MSF.461-464.765 ↗
7. Evaluation of Mn substitution for Ni in alumina-forming austenitic stainless steels10.1016/j.msea.2009.06.043 ↗
8. The development of alumina-forming austenitic stainless steels for high-temperature structural use10.1007/s11837-008-0083-2 ↗
9. Compositional and structural characterization of alumina coatings deposited electrochemically on stainless steel10.1016/j.apsusc.2004.05.119 ↗
10. Small-angle neutron scattering study of the wet and dry high-temperature oxidation of alumina-and chromia-forming stainless steels10.1016/j.corsci.2012.01.024 ↗
11. Corrosion behavior of an alumina forming austenitic steel exposed to supercritical carbon dioxide10.1016/j.corsci.2013.12.023 ↗
12. Corrosion of alumina-forming austenitic steel Fe-20Ni-14Cr-3Al-0.6Nb-0.1Ti in supercritical water10.1016/j.jnucmat.2010.01.025 ↗
13. Influence of sulfur and water vapor on high-temperature oxidation resistance of an alumina-forming austenitic alloy
14. Effects of minor alloy additions and oxidation temperature on protective alumina scale formation in creep-resistant austenitic stainless steels10.1016/j.scriptamat.2007.08.032 ↗
15. On the loss of protective scale formation in creep-resistant, alumina-forming austenitic stainless steels at 900℃ in air10.4028/www.scientific.net/MSF.595-598.725 ↗
16. Alumina-forming austenitic stainless steels strengthened by Laves Phase and MC carbide precipitates10.1007/s11661-007-9319-y ↗
17. Overview of Strategies for high-temperature creep and oxidation resistance of alumina-forming austenitic stainless steels10.1007/s11661-010-0295-2 ↗
18. Improvement of high-temperature oxidation resistance and strength in alumina-forming austenitic stainless steels10.1016/j.matlet.2011.07.021 ↗
19. Composition, microstructure, and water vapor effects on internal/external oxidation of alumina-forming austenitic stainless steels10.1007/s11085-009-9161-2 ↗
20. Improvement of oxidation resistance of remelted zone in an Al2O3-forming austenitic stainless steel by annealing10.1007/s11085-014-9520-5 ↗
21. Increasing the upper temperature oxidation limit of alumina forming austenitic stainless steels in air with water vapor10.1007/s11085-011-9237-7 ↗
22. Oxidation of high-aluminum austenitic stainless steels10.1007/BF00666596 ↗
23. Oxidation and hot-corrosion resistant high aluminum austenitic stainless steel10.1007/BF02833427 ↗
24. Oxidation behavior and microstructure evolution of alumina-forming austenitic & high entropy alloys in steam environment at 1200 °C10.1016/j.corsci.2020.108654 ↗
25. Effect of alloying additions on phase equilibria and creep resistance of alumina-forming austenitic stainless steels10.1007/s11661-009-9886-1 ↗
26. Ultrahigh stability and strong precipitation strengthening of nanosized NbC in alumina-forming austenitic stainless steels subjecting to long-term high-temperature exposure10.1016/j.msea.2018.09.081 ↗
27. Design of alumina-forming austenitic stainless steel using genetic algorithms
28. Precipitation behavior of Laves phase in the vicinity of oxide film of ferritic stainless steel: selective oxidation-induced precipitation10.1007/s11085-019-09955-5 ↗
29. Effect of grain boundaries on the formation of oxide scale in Fe-Cr alloy for SOFCs10.1016/j.ssi.2008.01.090 ↗
30. Oxidation behavior of Fe-20Cr-25Ni-Nb austenitic stainless steel in high-temperature environment with small amount of water vapor10.1016/j.corsci.2018.09.016 ↗
31. Oxidation behaviors of Fe-25Cr-20Ni-χNb austenitic weld metals at 1100 °C in ambient air: role of elemental niobium10.1016/j.corsci.2019.108137 ↗
32. Niobium in modern steels10.1179/095066003225008833 ↗
33. Corrosion behavior of alumina-forming and oxide dispersion strengthened austenitic 316 stainless steel in supercritical water10.1016/j.corsci.2018.04.026 ↗