A study on the corrosion behaviour of stainless steel 08Cr18Ni10Ti in supercritical water
Source abstract
Abstract
Austenitic stainless steel 08Cr18Ni10Ti is widely used in WWER reactor. Therefore, it was considered one of the prospective materials for supercritical water-cooled reactors. In this study, coupon specimens were exposed close to the critical point of water and high temperature of supercritical water. Corrosion behaviour was described based on the results of X-ray diffraction and scanning electron microscopy involving chemical and crystallographic analyses. In contrast to the thin oxide layer of approximately 1 µm formed in water close to the supercritical point, the localised form of corrosion was observed at the high temperature supercritical water.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Subcritical and Supercritical Water Processes · High-Temperature Coating Behaviors · Advanced Materials Characterization Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. Guzonas · 2018
2. D. Guzonas, W. Cook, Corrosion in a supercritical water-cooled reactors - developing a mechanistic framework, In: Proceedings of the 3rd China-Canada Jt. Work. Supercrit. React., Xi´an, China, 2012: s. 13.
3. P. Macdonald, J. Buongiorno, J.W. Sterbentz, C. Davis, P.R. Witt, Feasibility Study of Supercritical Light Water Cooled Reactors for Electric Power Production. Final Report. 12th Quarterly Report, (2001).10.2172/910979 ↗
4. Schulenberg · 2012
5. C.S. Water, D. Toshiba, Status report 71 - Japanese Supercritical Water-Cooled Reactor (JSCWR), (2011) 1–12.
6. Core design of super LWR with double tube water rods10.1016/j.nucengdes.2013.07.008 ↗
7. V. Yurmanov, V. Belous, V. Vasian, E. Yurmanov, Chemistry and Corrosion Issues in Supercritical Water Reactors, Oppor. chanllenges water Cool. React. 21sth century. (2009). 〈http://www.pub.iaea.org/MTCD/publications/PDF/P1500_CD_Web/htm/pdf/topic5/5S12_V.Yurmanov.pdf〉.
8. Research activities on a supercritical pressure water reactor in Korea10.5516/NET.2007.39.4.273 ↗
9. LOCA analysis of SCWR-M with passive safety system10.1016/j.nucengdes.2013.03.007 ↗
10. Pourbaix diagrams for the iron-water system extended to high-subcritical and low-supercritical conditions10.1016/j.corsci.2011.10.034 ↗
11. Oxidation of stainless steel 316 and Nitronic 50 in supercritical and ultrasupercritical water10.1016/j.apsusc.2015.03.127 ↗
12. Surface nanocrystallization and gradient microstructural evolutions in the surface layers of 321 stainless steel alloy treated via severe shot peening10.1016/j.vacuum.2017.07.016 ↗
13. Effect of surface modification on the corrosion resistance of austenitic stainless steel 316L in supercritical water conditions10.1016/j.supflu.2013.05.002 ↗
14. D. Guzonas, J. Wills, H. Dole, J. Michel, S. Jang, M. Haycock, M. Chutumstid, Steel corrosion in supercritical water: an assessment of the key parameters, In: Proceedings of the 2nd Canada-China Jt. Work. Supercrit. Water-Cooled React., 2010: s. 13.
15. The effect of surface finish on the scaling behavior of stainless steel in steam and supercritical water10.1007/s11085-013-9380-4 ↗
16. Corrosion behavior of alloy 800H (Fe-21Cr-32Ni) in supercritical water10.1016/j.corsci.2010.10.021 ↗
17. Microstructure tailoring for property improvements by grain boundary engineering10.1016/j.jnucmat.2007.08.015 ↗
18. The effect of grain boundary engineering on the oxidation behavior of INCOLOY alloy 800H in supercritical water10.1016/j.jnucmat.2005.09.023 ↗
19. Heat transfer deterioration mechanism for water at supercritical pressure
20. Dalle · 2017
21. Microstructural investigation of the breakdown of the protective oxide scale on a 304 steel in the presence of oxygen and water vapour at 600 °C10.1016/j.corsci.2005.08.012 ↗
22. Oxidation behavior analysis of a ferritic ODS steel in supercritical water10.1016/j.fusengdes.2020.111991 ↗
23. A comparative study on the oxidation of austenitic alloys 304 and 304-oxide dispersion strengthened steel in supercritical water at 650 °C10.1016/j.supflu.2016.10.002 ↗
24. Corrosion behavior of alumina-forming and oxide dispersion strengthened austenitic 316 stainless steel in supercritical water10.1016/j.corsci.2018.04.026 ↗
25. M. Růžičková, P. Hájek, Š. Šmida, R. Všolák, J. Petr, J. Kysela, Supercritical water loop design for corrosion and water chemistry tests under irradiation., In: Proceedings of the Nucl. Eng. Technol. Spec. issue 3rd Int. Symp. SCWR. 40, 2007. pp. 127–132.10.5516/NET.2008.40.2.127 ↗
26. First experience with operating the supercritical water loop
27. The pseudocritical regions for supercritical water10.1016/j.nucengdes.2012.07.007 ↗
28. Corrosion in high-temperature and supercritical water and aqueous solutions: a review10.1016/S0896-8446(03)00031-7 ↗
29. Corrosion mechanisms of candidate structural materials for supercritical water-cooled reactor10.1007/s11708-009-0024-y ↗
30. Study of the corrosion behavior of a 18Cr-oxide dispersion strengthened steel in supercritical water10.1016/j.corsci.2012.08.021 ↗
31. Corrosion and stress corrosion cracking in supercritical water10.1016/j.jnucmat.2007.05.017 ↗
32. The detection of local plastic strain in microscopic scale10.1016/j.matlet.2007.06.065 ↗
33. Corrosion behavior of steels and nickel alloys in superheated steam10.5006/0010-9312-22.5.147 ↗
34. Effects of surface treatments on environmentally-assisted cracking susceptibility of Alloy 182 in BWR environment10.1016/j.corsci.2021.109555 ↗
35. Characterization of oxide scales grown on alloy 310S stainless steel after long term exposure to supercritical water at 500 °C10.1016/j.matchar.2016.09.013 ↗
36. Influence of the dissolved oxygen content on corrosion of the ferritic-martensitic steel P92 in supercritical water10.1016/j.corsci.2011.11.013 ↗
37. The mechanism of high temperature aqueous corrosion of stainless steels10.1016/0010-938X(91)90125-9 ↗
38. Thermally grown oxide films and corrosion performance of ferritic stainless steels under simulated exhaust gas condensate conditions10.1016/j.corsci.2014.06.041 ↗
39. Microstructural investigation of the nodular corrosion of 304NG stainless steel in supercritical water10.1016/j.corsci.2020.108652 ↗
40. Overview on corrosion in supercritical fluids10.1016/j.supflu.2016.07.022 ↗
41. Diffusion of cations in chromia layers grown on iron-base alloys10.1007/BF00665632 ↗
42. Point defects and transport properties of binary and ternary oxides10.1016/0167-2738(84)90126-7 ↗
43. A review of the oxidation behaviour of structural alloys in steam10.1179/095066010X12646898728165 ↗
44. Fritz · 2009
45. Van Uffelen · 2012
46. Corrosion behavior of alloy 316L stainless steel after exposure to supercritical water at 500 °C for 20,000h10.1016/j.supflu.2017.03.022 ↗
47. Effect of shot-peening on the oxidation of alloy 800H exposed to supercritical water and cyclic oxidation10.1016/j.corsci.2008.04.008 ↗