Investigation on the corrosion behavior of Alloy 800H at various levels of deformation
Source abstract
Abstract
The corrosion behavior of Alloy 800H in deaerated supercritical water was investigated. Multi-pass cold rolling was used to achieve thickness reductions of up to 80%, and the weight gain vs. time (up to 1000 h) in supercritical water at 600 ℃ and 25 MPa were obtained for specimens in the polished vs. ground surface condition. Polished specimens without rolling showed the highest corrosion rates, and surface grinding or cold rolling significantly increased the corrosion resistance. A thick oxide film develops, with an outer moderately uniform layer of magnetite (Fe 3O 4 ) with crystallites along the surface, and areas of uneven oxidation into the metal that incorporate Cr (e.g., FeCr 2O 4). Very few Cr 2O 3 particles exist, and preferentially near the grain boundaries. Continuous Cr-rich oxide films were found in the thin oxide films on the surface of ground specimens and heavily rolled specimens, and an associated Cr depleted zone in the metal under the oxide of ground specimens, but not in heavily rolled specimens. This indicates that the high density of dislocations accelerates the diffusion of elements and enhance the formation of Cr-rich oxide film, which promotes passivity.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Advanced Materials Characterization Techniques · Subcritical and Supercritical Water Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. Design concepts of supercritical water-cooled reactor (SCWR) and nuclear marine vessel: A review
2. D. Guzonas, R. Novotny, S. Penttila, A. Toivonen, W. Zheng. Materials and Water Chemistry for Supercritical Water-cooled Reactors. Woodhead Publishing2018.10.1016/B978-0-08-102049-4.00004-0 ↗
3. Corrosion resistance of candidate cladding materials for supercritical water reactor10.1016/j.anucene.2018.12.007 ↗
4. W. Ren, R. Swindeman. A Review of Alloy 800H for Applications in the Gen IV Nuclear Energy Systems. ASME 2010 Pressure Vessels and Piping Conference: Volume 6, Bellevue, Washington, USA, 2010. pp. 821–836.10.1115/PVP2010-25278 ↗
5. Analyses of oxide films grown on AISI 304L stainless steel and Incoloy 800HT exposed to supercritical water environment10.1016/j.jnucmat.2011.05.007 ↗
6. Oxidation behavior of Incoloy 800 under simulated supercritical water conditions10.1016/j.jnucmat.2008.12.004 ↗
7. Corrosion assessment of candidate materials for fuel cladding in Canadian SCWR10.1007/s11837-015-1745-5 ↗
8. Corrosion behavior of alloy 800H (Fe–21Cr–32Ni) in supercritical water10.1016/j.corsci.2010.10.021 ↗
9. Effects of cold work on the oxidation behavior and carburization resistance of Alloy 80010.1002/maco.19870381003 ↗
10. Microstructural changes in AISI 304L stainless steel due to surface machining: Effect on its susceptibility to chloride stress corrosion cracking10.1016/j.jnucmat.2010.05.028 ↗
11. Surface characterization of austenitic stainless steel 304L after different grinding operations10.1186/s40712-017-0074-6 ↗
12. TEM Study of Supercritical Water Corrosion in 310S and 800H Alloys10.1017/S1431927614011064 ↗
13. Point defect model for the corrosion of steels in supercritical water: Part I, film growth kinetics10.1016/j.corsci.2019.108280 ↗
14. Oxidation resistance of Fe-Cr-Ni laser cladding layer under supercritical water10.1088/2051-672X/ab9b6a ↗
15. Corrosion characteristics and mechanisms of typical Ni-based corrosion-resistant alloys in sub- and supercritical water10.1016/j.supflu.2020.105138 ↗
16. Effect of shot-peening on the oxidation of alloy 800H exposed to supercritical water and cyclic oxidation10.1016/j.corsci.2008.04.008 ↗
17. Effect of surface modification on the corrosion resistance of austenitic stainless steel 316L in supercritical water conditions10.1016/j.supflu.2013.05.002 ↗
18. Corrosion behavior of alumina-forming and oxide dispersion strengthened austenitic 316 stainless steel in supercritical water10.1016/j.corsci.2018.04.026 ↗
19. Corrosion and stress corrosion cracking susceptibility of type 347H stainless steel in supercritical water10.5006/2459 ↗
20. New insights into the oxidation mechanisms of a Ferritic-Martensitic steel in high-temperature steam10.1016/j.actamat.2020.05.052 ↗
21. Geometrically necessary dislocations and strain-gradient plasticity: a few critical issues10.1016/S1359-6462(02)00335-4 ↗
22. Mehrer · 2007
23. Measurement of local plastic strain distribution of stainless steel by electron backscatter diffraction10.1016/j.matchar.2008.07.010 ↗
24. High-resolution characterization of the internal and external oxidation of austenitic alloys in supercritical water10.1016/j.scriptamat.2021.113814 ↗
25. Corrosion of austenitic alloys in supercritical water10.5006/1.3278237 ↗
26. Microstructure understanding of high Cr-Ni austenitic steel corrosion in high-temperature steam10.1016/j.actamat.2022.117634 ↗
27. Diffusion of iron in Cr2O3: polycrystals and thin films10.1016/j.msea.2004.09.033 ↗
28. A novel method to promote selective oxidation of Ni-Cr alloys: Surface spreading α-Al2O3 nanoparticles10.1016/j.corsci.2021.109717 ↗
29. Ellingham Diagram
30. Oxidation processes and involved chemical reactions of corrosion-resistant alloys in supercritical water10.1021/acs.iecr.0c01394 ↗
31. Reducibility of oxides and sulphides in metallurgical processes
32. Ridge National Lab. ORNL. A review of the oxidation behaviour of structural alloys in steam10.1179/095066010X12646898728165 ↗
33. Diffusion of chromium, manganese, and iron in MnCr2O4 spinel10.1007/s11669-005-0051-2 ↗
34. Study of ion diffusion in oxidation films grown on a model Fe–15%Cr alloy10.1016/j.ssi.2015.03.027 ↗
35. AES characterization of oxide films formed on nickel-base alloys at Supercritical Water Reactor (SCWR) conditions10.1002/sia.5906 ↗
36. Effect of Cr content on supercritical water corrosion of high Cr alloys10.4028/www.scientific.net/MSF.475-479.1483 ↗
37. Formation of Cr2O3 diffusion barrier between Cr-contained stainless steel and cold-sprayed Ni coatings at high temperature10.1007/s11666-015-0371-7 ↗
38. Oxidation behaviour of Super 304H stainless steel in supercritical water10.1080/1478422X.2018.1459064 ↗
39. Internal-external transition for the oxidation of Fe-Cr-Ni austenitic stainless steels in steam10.1007/BF00665267 ↗
40. A theoretical analysis of the oxidation of Fe-Si alloys10.1016/0010-938X(82)90071-3 ↗
41. Rapid nickel diffusion in cold-worked type 316 austenitic steel at 360-500℃10.3139/146.111542 ↗
42. Grain boundary oxidation in iron-based alloys10.1016/j.corsci.2015.04.009 ↗
43. Mehrer · 1990
44. Diffusion of oxygen in nickel: a variable charge molecular dynamics study10.1016/j.ssc.2009.12.012 ↗
45. Effect of Fe on corrosion of Ni-20Cr and Ni-30Cr alloys in wet CO2 gas at 650 and 700 °C10.1016/j.corsci.2019.04.007 ↗
46. Thermodynamics, diffusion and the Kirkendall effect in solids. springer international publishing AG
47. Chromium volatilization rates from Cr2O3 scales into flowing gases containing water vapor10.1007/s11085-006-9030-1 ↗
48. Steam oxidation and chromia evaporation in ultrasupercritical steam boilers and turbines10.1149/1.3155442 ↗
49. Grain coarsening behaviour of solution annealed Alloy 625 between 600–800°C10.1016/j.msea.2016.11.060 ↗
50. Evolution of deformation and annealing textures in Incoloy 800H/HT via different rolling paths and strains10.1016/j.msea.2014.07.035 ↗