Abstract

Abstract Ni-base superalloy C263 has been oxidized from 700 °C to 1100 °C in artificial dry air. A continuous Cr rich (Cr, Ti)2O3 layer is formed during oxidation, while the oxidation kinetics deviated from the parabolic kinetics. The oxidation microstructures were different in as-machined and polished samples. Recrystallization below the oxide layer occurred in as-machined samples together with severe internal degradation (internal oxidation and nitridation). Grain boundaries provide paths for fast diffusion of O and N into the substrate and outward diffusion of Ti and Cr. Surface deformation and recrystallization exhibit detrimental effects on the oxidation behavior of C263.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Metal and Thin Film Mechanics · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. Reed · 2006
2. Sims · 1987
3. Chromia layer growth on a Ni-based superalloy: sub-parabolic kinetics and the role of titanium10.1016/j.corsci.2013.05.016 ↗
4. The cyclic oxidation behaviour of Ni-based superalloy GTD-111 with sulphur impurities at 1100°C10.1016/j.corsci.2014.10.030 ↗
5. Evolution of Ni-based superalloys for single crystal gas turbine blade applications10.1016/S1270-9638(99)00108-X ↗
6. Oxidation of nickel-based single-crystal superalloys for industrial gas turbine applications10.1016/j.actamat.2010.09.027 ↗
7. The formation of aluminum oxide scales on high-temperature alloys10.1007/BF00666913 ↗
8. Birks · 2006
9. Growth and adherence of chromia based surface scales on Ni-base alloys in high- and low-pO2 gases10.1016/j.msea.2007.05.035 ↗
10. Thermal oxidation kinetics and oxide scale adhesion of Fe–15Cr alloys as a function of their silicon content10.1016/j.actamat.2006.04.023 ↗
11. Maintaining adhesion of protective Al2O3 scales10.1007/s11837-000-0110-4 ↗
12. Hot Corrosion mechanism of composite alumina/yttria-stabilized zirconia coating in molten sulfate–vanadate salt10.1111/j.1551-2916.2005.00120.x ↗
13. Gessinger · 2013
14. Kofstad · 1988
15. Selective oxidation and internal nitridation during high-temperature exposure of single-crystalline nickel-base superalloys10.1007/s11661-000-0051-0 ↗
16. Selective carbide oxidation and internal nitridation of the Ni-base superalloys IN 738 LC and IN 939 in air10.1007/BF00656646 ↗
17. Oxidation behavior of GTD111 Ni-based superalloy at 900°C in air10.1016/j.corsci.2015.07.031 ↗
18. An atom probe tomography study of the oxide–metal interface of an oxide intrusion ahead of a crack in a polycrystalline Ni-based superalloy10.1016/j.scriptamat.2014.10.025 ↗
19. Intergranular crack tip oxidation in a Ni-base superalloy10.1016/j.actamat.2013.02.050 ↗
20. Oxidation ahead of a crack tip in an advanced Ni-based superalloy10.1016/j.actamat.2012.12.017 ↗
21. Simultaneous internal oxidation and nitridation of Ni–Cr–Al alloys10.1023/A:1010304026026 ↗
22. Internal nitridation of nickel-base alloys. Part II. Behavior of quaternary Ni-Cr-Al-Ti alloys and computer-based description10.1023/A:1018895628849 ↗
23. Internal nitridation of nickel-chromium alloys10.1007/BF00738289 ↗
24. Formation and compensation of internal stresses during internal nitridation of nickel-base alloys10.1016/S0921-5093(00)01670-1 ↗
25. Internal nitridation of nickel-base alloys. Part I. Behavior of binary and ternary alloys of the Ni-Cr-Al-Ti System10.1023/A:1018843612011 ↗
26. Kinetics, microstructures and mechanism of internal oxidation – its effect and prevention in high temperature alloy oxidation10.5006/0010-9312-21.12.382 ↗
27. Mechanism of internal oxidation of alloy 617 in He-CO-CO2 environments at 1123 K (850°C)10.1007/s11661-014-2629-y ↗
28. The effect of surface treatment on the oxidation of ferritic stainless steels used for solid oxide fuel cell interconnects10.1016/j.jpowsour.2008.06.010 ↗
29. Factors affecting the development of oxide scales on austenitic stainless steels during hot rolling in Steckel Mills10.1007/s11661-008-9577-3 ↗
30. Influence of dissolved oxygen on oxide films of Alloy 690TT with different surface status in simulated primary water10.1016/j.corsci.2011.07.012 ↗
31. Prestraining effect on creep behaviour of nickel base C263 superalloy10.1179/026708302225004838 ↗
32. Oxidation of Ni-Cr-Al alloys between 1000°C and 1200°C10.1149/1.2407837 ↗
33. An experimental analysis and measurement of process performances in machining of nimonic C-263 super alloy10.1016/j.measurement.2012.06.006 ↗
34. Physically-based model for creep in nickel-base superalloy C263 both above and below the gamma solvus10.1016/S1359-6454(02)00119-2 ↗
35. Microstructure stability: optimisation of 263 Ni-based superalloy
36. NIH image to imageJ: 25 years of image analysis10.1038/nmeth.2089 ↗
37. High-resolution elastic strain measurement from electron backscatter diffraction patterns: new levels of sensitivity10.1016/j.ultramic.2005.10.001 ↗
38. Measurement of residual elastic strain and lattice rotations with high resolution electron backscatter diffraction10.1016/j.ultramic.2011.05.007 ↗
39. High resolution electron backscatter diffraction measurements of elastic strain variations in the presence of larger lattice rotation10.1016/j.ultramic.2012.01.004 ↗
40. Strains, planes, and EBSD in materials science10.1016/S1369-7021(12)70163-3 ↗
41. Diffusion induced grain boundary migration10.1179/095066087790150304 ↗
42. STEM analysis of the transient oxidation of a Ni-20Cr alloy at high temperature10.1023/A:1018827108376 ↗
43. Reducibility of oxides and sulfides in metallurgical processes
44. Effects of alloyed aluminum and titanium on the oxidation behavior of INCONEL 740 superalloy10.1016/j.jallcom.2015.10.198 ↗
45. Passivity and inhibition during the oxidation of metals at elevated temperatures10.1016/S0010-938X(65)80003-8 ↗
46. Anomalous behavior during internal oxidation and nitridation10.1007/BF03222725 ↗
47. Internal nitridation of nickel-chromium alloys10.1007/BF00738289 ↗