journal article·2020-02

Corrosion behavior of ion-irradiated SiC in FLiNaK molten salt

Jianjian Li, Long Yan, Hefei Huang, Qing Huang, CuiLan Ren, Guanhong Lei, Jun Lin, Chonglong Fu, Juju Bai

Corrosion Science· Volume 163
Publisher page

Abstract

Abstract High-purity 4H-SiC samples exposed to 1-MeV Si ions irradiation at RT were corroded in FLiNaK molten salt at 650° C for 168 h. Results revealed the corrosion degree of irradiated SiC was dependent on the irradiation fluence. The amorphous region induced by irradiation was preferentially corroded, where Si elements could dissolve into the salt more easily than those in the unirradiated region. The dissolution of Si elements caused the formation of sustained nanocracks and nanopores, and thus the corrosion layer having a thickness of 200 ± 50 nm fell off. Moreover, oxygen impurities might play a role in the irradiation-assisted corrosion.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Silicon Carbide Semiconductor Technologies · Fusion materials and technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. The critical issues of SiC materials for future nuclear systems10.1016/j.scriptamat.2017.03.001 ↗
2. Recent progress in the development of SiC composites for nuclear fusion applications
3. Motivation for utilizing new high-performance advanced materials in nuclear energy systems10.1016/j.cossms.2016.10.004 ↗
4. Effects of bubbles on high-temperature corrosion of helium ion-irradiated Ni-based alloy in fluoride molten salt10.1016/j.corsci.2017.06.027 ↗
5. Effects of He ion irradiation on the corrosion performance of alloy GH3535 welded joint in molten FLiNaK10.1016/j.corsci.2018.10.038 ↗
6. Corrosion-driven outward migration and growth of helium bubbles in a nickel-based alloy in high-temperature molten salt environment10.1016/j.corsci.2019.03.026 ↗
7. Effect of oxygen on the corrosion of SiC in LiF-NaF-KF molten salt10.1016/j.corsci.2015.11.014 ↗
8. Microstructure evolution and high-temperature mechanical properties of SiCf/SiC composites in liquid fluoride salt environment10.1016/j.corsci.2017.05.016 ↗
9. FLiNaK compatibility studies with Inconel 600 and silicon carbide10.1016/j.nucengdes.2016.06.037 ↗
10. Effect of irradiation damage on corrosion of 4H-SiC in FLiNaK molten salt10.1016/j.corsci.2017.05.028 ↗
11. Corrosion behavior of TiC-SiC composite ceramics in molten FLiNaK salt10.1016/j.jeurceramsoc.2017.02.020 ↗
12. Design, fabrication, and testing of ceramic plate-type heat exchangers with integrated flow channel design10.1111/j.1744-7402.2010.02573.x ↗
13. Corrosion of Si, C, and SiC in molten salt10.1016/j.corsci.2018.10.027 ↗
14. Effects of Cr3+ on the corrosion of SiC in LiF-NaF-KF molten salt10.1016/j.corsci.2016.10.026 ↗
15. Effect of irradiation damage on hydrothermal corrosion of SiC
16. SRIM - the stopping and range of ions in matter (2010)10.1016/j.nimb.2010.02.091 ↗
17. On the use of SRIM for computing radiation damage exposure10.1016/j.nimb.2013.05.008 ↗
18. Displacement energy surface in 3C and 6H SiC
19. Compatibility of container materials with Cr in molten FLiNaK salt10.1016/j.jfluchem.2014.09.010 ↗
20. Preparation of high-purity molten FLiNaK salt by the hydrofluorination process10.1016/j.jfluchem.2017.03.006 ↗
21. Raman spectroscopy of epitaxial graphene on a SiC substrate10.1103/PhysRevB.77.115416 ↗
22. Effects of thermal treatment on the mechanical integrity of silicon carbide in HTR fuel up to 2200 degrees C
23. Lattice damage and nanohardness in 6H-SiC implanted with multiple-energy Xe ions10.1016/j.nimb.2011.11.034 ↗
24. Role of irradiation-induced defects on SiC dissolution in hot water10.1016/j.corsci.2016.08.007 ↗
25. First-principles modeling of anisotropic anodic dissolution of metals and alloys in corrosive environments10.1016/j.actamat.2017.03.027 ↗
26. Corrosion of SiC induced by Hastelloy N alloy and its corrosion products in LiF-NaF-KF molten salt10.1016/j.corsci.2016.03.029 ↗
27. Interaction between SiO2 and a KF-KCl-K2SiF6 melt10.1021/jp4086816 ↗