A new insight into the rate determining step of cathodic delamination
Source abstract
Abstract
One of the most important mechanisms of organic coating degradation is cathodic delamination. Although a significant progress towards the fundamentals of delamination was achieved in the recent decades, the underlying key parameters are not fully understood. It is believed that either cation migration along the delaminated interface or oxygen reduction at the interface are rate determining. However, as will be shown here this is not the case. A new hypothesis, which is cation insertion into the intact interface as the rate determining step in delamination, is proposed using a combined Scanning Kelvin Probe/potentiostat set-up and an in-depth delamination rate analysis.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Analytical Chemistry and Sensors · Semiconductor materials and devices · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. Bardal · 2004
2. Knudsen · 2017
3. The mechanism for the cathodic delamination of organic coatings from a metal surface10.1016/0033-0655(83)80002-8 ↗
4. Investigation of the delamination of polymer films from galvanized steel with the Scanning Kelvinprobe
5. The investigation of the corrosion properties of metals, covered with adsorbed electrolyte layers—a new experimental technique10.1016/0010-938X(87)90043-6 ↗
6. Corrosion protection by organic films10.1016/0013-4686(94)E0038-2 ↗
7. The scanning Kelvin probe; a new technique for the in situ analysis of the delamination of organic coatings10.1016/0300-9440(94)00542-7 ↗
8. On the atmospheric corrosion of metals which are covered with thin electrolyte layers—I. Verification of the experimental technique10.1016/0010-938X(90)90032-Z ↗
9. On the atmospheric corrosion of metals which are covered with thin electrolyte layers—II. Experimental results10.1016/0010-938X(90)90033-2 ↗
10. A new technique able to measure directly the delamination of organic polymer films10.1016/0010-938X(91)90126-A ↗
11. Use of a scanning‐kelvinprobe in the investigation of electrochemical reactions at the metal/polymer interface10.1002/bbpc.19910951109 ↗
12. Application of a Kelvin microprobe to the corrosion of metals in humid atmospheres10.1149/1.2085578 ↗
13. The delamination of polymeric coatings from steel. Part 1: Calibration of the Kelvinprobe and basic delamination mechanism10.1016/S0010-938X(98)00166-8 ↗
14. The delamination of polymeric coatings from steel. Part 2: First stage of delamination, effect of type and concentration of cations on delamination, chemical analysis of the interface10.1016/S0010-938X(98)00167-X ↗
15. The delamination of polymeric coatings from steel Part 3: Effect of the oxygen partial pressure on the delamination reaction and current distribution at the metal/polymer interface10.1016/S0010-938X(98)00168-1 ↗
16. Cathodic self-healing at cut-edges: the effect of Zn2+ and Mg2+ ions10.1016/j.corsci.2012.08.008 ↗
17. The physical meaning of electrode potentials at metal surfaces and polymer/metal interfaces: consequences for delamination10.1149/1.2926589 ↗
18. Passivity of metals and the kelvin probe technique, in: reference module in chemistry, molecular sciences and chemical engineering, encyclopedia of interfacial chemistry
19. The delamination of polymeric coatings from electrogalvanized steel–a mechanistic approach.: Part 3: delamination kinetics and influence of CO210.1016/S0010-938X(00)00049-4 ↗
20. Cathodic disbonding of chlorinated rubber coatings from steel10.1016/0010-938X(93)90361-J ↗
21. Chromate inhibition of corrosion-driven organic coating delamination studied using a scanning Kelvin probe technique10.1149/1.1396336 ↗
22. Cerium (III) inhibition of corrosion-driven organic coating delamination studied using a scanning Kelvin probe technique10.1149/1.1457983 ↗
23. Mechanism of cathodic delamination control of zinc–aluminum phosphate pigment in waterborne coatings10.1016/j.corsci.2004.01.009 ↗
24. Polyaniline inhibition of corrosion-driven organic coating cathodic delamination on iron10.1149/1.1850857 ↗
25. Cathodic delamination: quantification of ionic transport rates along coating–steel interfaces10.1016/j.porgcoat.2009.08.018 ↗
26. Localised SKP studies of cathodic disbondment on chromium/chromium oxide coated steel10.1149/05047.0067ecst ↗
27. The kinetics and mechanism of atmospheric corrosion occurring on tin and iron-tin intermetallic coated steels10.1149/2.0681514jes ↗
28. Cathodic delamination of unpigmented and pigmented epoxy coatings from mild steel10.1016/j.porgcoat.2015.10.002 ↗
29. Evaluation of multi-layered graphene nano-platelet composite coatings for corrosion control part II–Cathodic delamination kinetics10.1016/j.corsci.2018.03.014 ↗
30. Assessment of steel corrosion and deadhesion of epoxy barrier paint by scanning Kelvin probe10.1016/j.porgcoat.2017.09.016 ↗
31. Kinetics of corrosion-driven cathodic disbondment on organic coated trivalent chromium metal-oxide-carbide coatings on steel10.1016/j.corsci.2019.04.037 ↗
32. A mechanistic investigation of corrosion-driven organic coating failure on magnesium and its alloys10.1038/s41529-019-0103-4 ↗
33. Chromium coatings from trivalent chromium plating baths: characterization and cathodic delamination behaviour10.1016/j.corsci.2021.109525 ↗
34. The protection zone: a long-range corrosion protection mechanism around conducting polymer particles in composite coatings: Part I. polyaniline and polypyrrole10.1149/2.0971912jes ↗
35. The protection zone: a long-range corrosion protection mechanism around conducting polymer particles in composite coatings: part II. PEDOT: PSS10.1149/2.0981912jes ↗
36. Fabrication of robust reference tips and reference electrodes for Kelvin probe applications in changing atmospheres10.1021/acs.langmuir.7b02533 ↗
37. Release and transport of corrosion inhibitors in self-healing coatings for intelligent corrosion protection
38. An agar-based silver| silver chloride reference electrode for use in micro-electrochemistry10.1016/S1388-2481(99)00035-1 ↗
39. Cathodic driven coating delamination suppressed by inhibition of cation migration along Zn| polymer interface in atmospheric CO 210.1038/s41529-018-0064-z ↗
40. In situ infrared spectroscopic and scanning Kelvin probe measurements of water and ion transport at polymer/metal interfaces10.1016/j.electacta.2005.09.024 ↗