journal article·2023-05

Effect of Al addition on the corrosion behavior of Al CoCrFeNi high entropy alloys in supercritical water

Xi Huang, Qi Zhao, Zixiong Zhan, Junxiong Liu, Xinhua Liao, Jincheng Deng, Lihua Wei, Xiaoyan Li

Corrosion Science· Volume 216
Publisher page

Abstract

The effect of Al addition on the corrosion behavior of high entropy alloys Al xCoCrFeNi ( x = 0, 0.1, and 1.0) in supercritical water was investigated. The weight gain and oxide film thickness reduced with the increase of Al content. A duplex-structure oxide film, consisting of FeCr 2O 4 outer and Cr 2O 3 inner layer, was developed on CoCrFeNi alloy. A triple-layered oxide film consisting of FeCr 2O 4 outer, Cr 2O 3 middle, and Al 2O 3 inner layer was developed on Al 0.1 CoCrFeNi and AlCoCrFeNi alloys. The improvement of corrosion resistance by adding Al was attributed to the high Al concentration that accelerated the formation of Al 2O 3.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · High Entropy Alloys Studies · Subcritical and Supercritical Water Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (74)

Show source-provided references
1. Challenges toward carbon neutrality in China: strategies and countermeasures10.1016/j.resconrec.2021.105959 ↗
2. Corrosion and stress corrosion cracking in supercritical water10.1016/j.jnucmat.2007.05.017 ↗
3. Oxidation of ferritic–martensitic alloys T91, HCM12A and HT-9 in supercritical water10.1016/j.jnucmat.2007.05.023 ↗
4. Supercritical-water heat transfer in a vertical bare tube10.1016/j.nucengdes.2009.09.003 ↗
5. Point defect model for the corrosion of steels in supercritical water: Part I, film growth kinetics10.1016/j.corsci.2019.108280 ↗
7. Effect of surface modification on the corrosion resistance of austenitic stainless steel 316L in supercritical water conditions10.1016/j.supflu.2013.05.002 ↗
8. Influence of temperature on the oxidation behaviour of a ferritic-martensitic steel in supercritical water10.1016/j.corsci.2016.10.020 ↗
9. Effect of thermo-mechanical processing on oxidation of austenitic stainless steel 316L in supercritical water10.1016/j.corsci.2015.02.008 ↗
10. Effect of exposure temperature on the corrosion behaviors of TP347H austenitic stainless steel in supercritical water10.1016/j.corsci.2019.108188 ↗
11. A comparative study of oxide scales grown on stainless steel and nickel-based superalloys in ultra-high temperature supercritical water at 800 °C10.1016/j.corsci.2016.02.004 ↗
12. The corrosion behavior of nickel-based alloy Inconel 740H in supercritical water10.1016/j.corsci.2021.109848 ↗
13. Corrosion behavior of a 14Cr-ODS steel in supercritical water10.1016/j.jnucmat.2013.02.002 ↗
14. Corrosion behavior of an Al added high-Cr ODS steel in supercritical water at 600 °C10.1016/j.apsusc.2019.03.019 ↗
15. Corrosion behavior of nickel base alloys, stainless steel and titanium alloy in supercritical water containing chloride, phosphate and oxygen10.1016/j.cherd.2015.05.003 ↗
16. Corrosion properties of candidate materials in supercritical water oxidation process
17. Materials assessment for the Canadian SCWR core concept10.1007/s11837-015-1758-0 ↗
18. Low activation, refractory, high entropy alloys for nuclear applications10.1016/j.jnucmat.2019.151744 ↗
19. Low activation high entropy alloys for next generation nuclear applications10.1016/j.mtla.2018.09.014 ↗
20. Influence of irradiation temperature on void swelling in NiCoFeCrMn and NiCoFeCrPd10.1016/j.scriptamat.2018.08.021 ↗
21. Oxidation behavior of Al0.2CoCrFeNi high-entropy alloy film in supercritical water environment10.1007/s12598-021-01859-1 ↗
22. Corrosion behavior of a dual-phase FeNiCrCuAl high entropy alloy in supercritical water10.1016/j.corsci.2022.110617 ↗
23. Oxidation behavior of high-entropy alloys AlxCoCrFeNi (x=0.15, 0.4) in supercritical water and comparison with HR3C steel10.1016/S1003-6326(15)63733-5 ↗
24. Review of recent research on AlCoCrFeNi high-entropy alloy10.3390/met11081302 ↗
25. Effect of Al on oxidation behavior of AlxCrCuFeNi2 (x = 0.2, 0.4, 0.6) high entropy alloys10.1016/j.corsci.2022.110697 ↗
26. Effects of Al addition on microstructure and mechanical properties of AlCoCrFeNi High-entropy alloy10.1016/j.msea.2015.09.034 ↗
27. Effects of Al addition on the microstructure and mechanical property of AlxCoCrFeNi high-entropy alloys10.1016/j.intermet.2012.03.005 ↗
28. Effects of nanotwins on the mechanical properties of AlxCoCrFeNi high entropy alloy thin films10.1016/j.scriptamat.2017.06.009 ↗
29. Effect of aluminum contents on microstructure and properties of AlxCoCrFeNi alloys10.1016/j.jallcom.2010.03.111 ↗
30. Phase transformation induced by lattice distortion in multiprincipal component CoCrFeNiCuxAl1−x solid-solution alloys10.1063/1.2938690 ↗
31. Spinodal Transformation Structures, in
32. Corrosion behavior of ferritic/martensitic steel P92 in supercritical water10.1016/j.supflu.2009.06.019 ↗
33. In situ Raman spectroscopic investigation of chromium surfaces under hydrothermal conditions10.1016/S0169-4332(01)00338-5 ↗
34. Raman spectroscopic study of solid solution spinel oxides, University of Nevada
35. Raman spectroscopic study of magnetite (FeFe2O4): a new assignment for the vibrational spectrum10.1016/S0022-4596(03)00294-9 ↗
36. Photoluminescence and Raman spectroscopy studies of low-temperature γ-Al2O3 phases synthesized from different precursors10.1016/j.optmat.2016.01.029 ↗
37. Excitation frequency dependence and fluorescence in the raman spectra of Al2O310.1366/0003702971941331 ↗
38. Raman fingerprint of chromate, aluminate and ferrite spinels10.1002/jrs.4764 ↗
39. Raman studies of cation distribution and thermal stability of epitaxial spinel NiCo2O4
40. Effect of Al content on the thermal oxidation behaviour of AlHfMoNbTi high-entropy alloys analysed by in situ environmental TEM10.1016/j.corsci.2021.109711 ↗
41. Effects of Al and Mo on high temperature oxidation behavior of refractory high entropy alloys10.1016/S1003-6326(19)65054-5 ↗
42. High-entropy alloy: challenges and prospects10.1016/j.mattod.2015.11.026 ↗
43. Microstructures and properties of high-entropy alloys10.1016/j.pmatsci.2013.10.001 ↗
44. Corrosion behaviour of 16%Cr–4%Al and 16%Cr ODS ferritic steels under different metallurgical conditions in a supercritical water environment10.1016/j.corsci.2010.05.043 ↗
45. Oxidation behavior of 9Cr-4.5Al ODS steel in 600 °C supercritical water and the effect of pre-oxidation10.1016/j.corsci.2019.108380 ↗
46. Corrosion behavior of oxide dispersion strengthened ferritic steels in supercritical water10.1016/j.jnucmat.2017.01.014 ↗
47. Corrosion characteristics and mechanisms of typical Ni-based corrosion-resistant alloys in sub- and supercritical water10.1016/j.supflu.2020.105138 ↗
48. The role of noncrystalline films in the oxidation and corrosion of metals10.1007/BF01058831 ↗
49. Corrosion of alumina-forming austenitic steel Fe–20Ni–14Cr–3Al–0.6Nb–0.1Ti10.1016/j.jnucmat.2010.01.025 ↗
50. The corrosion and stress corrosion cracking behavior of a novel alumina-forming austenitic stainless steel in supercritical water10.1016/j.jnucmat.2016.10.039 ↗
51. Corrosion behavior of alumina-forming and oxide dispersion strengthened austenitic 316 stainless steel in supercritical water10.1016/j.corsci.2018.04.026 ↗
52. Role of Al addition and Y2O3 on the intergranular corrosion behavior of AFA-ODS steel in the supercritical water10.1016/j.matdes.2022.111386 ↗
53. Corrosion behaviour of alumina-forming heat resistant alloy with Ti in high temperature steam10.1016/j.corsci.2021.110000 ↗
54. Effect of water vapor on high-temperature oxidation of NiAl alloy10.1016/j.corsci.2020.108963 ↗
55. High-temperature steam oxidation behavior of alumina-forming duplex FeNiCrAl and ferritic FeCrAl alloys at 800 °C to 1050 °C10.1016/j.corsci.2021.109658 ↗
56. Composition, microstructure, and water vapor effects on internal/external oxidation of alumina-forming austenitic stainless steels10.1007/s11085-009-9161-2 ↗
57. The mechanism of high temperature aqueous corrosion of stainless steels10.1016/0010-938X(91)90125-9 ↗
58. Corrosion and corrosion fatigue behaviors of 9cr steel in a supercritical water condition10.1016/j.msea.2006.05.035 ↗
59. Analysis of surface oxide films formed in hydrogenated primary water on alloy 690TT samples with different surface states10.1016/j.jmst.2014.09.002 ↗
60. Corrosion behavior of Hastelloy C-276 in supercritical water10.1016/j.corsci.2009.05.041 ↗
61. Oxidation behavior of ferritic–martensitic and ODS steels in supercritical water10.1016/j.jnucmat.2012.03.009 ↗
62. Corrosion behavior of Alx(CrFeNi)1−x HEA under simulated PWR primary water10.3390/ma15144975 ↗
63. Effect of alloying ratios and Cu-addition on corrosion behaviour of CoCrFeNiMo high-entropy alloys in superheated steam containing CO2, H2S and HCl10.1016/j.corsci.2020.109083 ↗
64. A. Roine. Outokumpu HSC Chemistry for windows, version 9.; Outokumpu Research Oy:Pori, Finland, 2018.
65. Effect of alloy composition and exposure conditions on the selective oxidation behavior of ferritic Fe–Cr and Fe–Cr–X alloys10.1007/s11085-010-9215-5 ↗
66. Corrosion of austenitic alloys in supercritical water10.5006/1.3278237 ↗
67. Oxidation and chromia evaporation of austenitic steel TP347HFG in supercritical water10.1080/09603409.2017.1381803 ↗
68. Corrosion Mechanisms of Alloys in Supercritical Water
69. On-line monitoring of oxide formation and dissolution on alloy 800H in supercritical water10.1016/j.corsci.2016.05.042 ↗
70. The effect of water vapor on the transition from internal to external oxidation of austenitic steels at 1,073 K10.1007/s11085-012-9350-2 ↗
71. Effect of environmental sulfur on the structure of alumina scales formed on Ni-base alloys10.1016/j.actamat.2015.06.031 ↗
72. High entropy and sluggish diffusion “core” effects in senary FCC Al–Co–Cr–Fe–Ni–Mn alloys10.1021/acscombsci.0c00096 ↗
73. The reproducibility of corrosion testing in supercritical water—results of a second international interlaboratory comparison exercise10.1016/j.jnucmat.2022.153759 ↗
74. The reproducibility of corrosion testing in supercritical water—Results of an international interlaboratory comparison exercise10.1016/j.corsci.2016.01.034 ↗