Abstract

Abstract Pit propagation on high purity aluminium electrode in 2 M HCl solutions with and without H 2 SO 4 under an alternating current (AC) has been examined. Pit development and potential transients were dependent on the H 2 SO 4 concentration. In the sulfate-free etchant, most pits developed from the pretreated surface, with little tendency to form clusters of pits. With increasing H 2 SO 4 concentration the size of the pit clusters increased. There is an optimal H 2 SO 4 concentration, which is 0.01 M H 2 SO 4 in this study, to form a deep etched layer of uniform thickness with high surface area. At H 2 SO 4 concentrations higher than 0.01 M, the pit propagation proceeded on limited foil surface sites and deep etched regions were formed locally, since sulfate ions assisted passivation and reduced the number of pit nucleation sites on foil surface. Analysis of potential transients during the anodic half-cycle supports the hypothesis that sulfate ions retarded the pit nucleation.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Anodic Oxide Films and Nanostructures · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. The effect of alternating voltage on aluminium electrodes in hydrochloric acid10.1016/S0010-938X(78)80092-4 ↗
2. A geometric model of alternating current etching of aluminium10.1063/1.332299 ↗
3. Pitting mechanism of aluminium in hydrochloric acid under alternating current10.1149/1.2119934 ↗
4. Electrochemical AC etching of aluminium foils in hydrochloric acid electrolytes10.4028/www.scientific.net/MSF.217-222.1565 ↗
5. Pitting behaviour of aluminium foil during alternating current etching in hydrochloric acid containing sulfate ions10.1149/1.2131830 ↗
6. The alternating current etching of aluminium lithographic sheet10.1080/00202967.1979.11870504 ↗
7. AC electrograining of aluminium10.1080/00202967.1988.11870820 ↗
8. The electrograining of aluminium in hydrochloric acid – Morphological appearance10.1016/0010-938X(91)90129-D ↗
9. The electrograining of aluminium in hydrochloric acid – Formation of etch products10.1016/0010-938X(91)90130-H ↗
10. R.S. Alwitt, H. Uchi, Processing of Al foil for electrolytic capacitors, in: H. Terryn, (Ed.), Proceedings 2nd International Symposium on Aluminium Surface Science and Technology (ASST 2000), p. 213, UMIST, Manchester, England, 2000, 213–220.
11. The influence of manganese on the AC electrolytic graining of aluminium10.1016/0010-938X(96)00135-7 ↗
12. On the mechanism of the AC electrolytic graining of rolled aluminium substrates10.1080/00202967.1996.11871118 ↗
13. A wall-jet electrode reactor and its application to the study of electrode reaction mechanisms. Part 3: Study of the mechanism of the ac electrolytic graining of aluminium in hydrochloric acid10.1023/A:1003288305367 ↗
14. Interpretation of the anodic and cathodic potential variations during the AC-graining of aluminium in hydrochloric acid10.1016/j.corsci.2007.03.009 ↗
15. Surface changes during AC etching of aluminium10.1149/1.2127408 ↗
16. Electrochemical study of the pitting corrosion of aluminium and its alloys – Determination of critical pitting and protection potentials10.1016/0013-4686(88)85023-0 ↗
17. Electrochemical study of the pitting corrosion of aluminium and its alloys. II. Study of the interaction of chloride ions with a passive film on aluminium and initiation of pitting corrosion10.1016/0013-4686(89)87119-1 ↗
18. Effects of applied potential and solution temperature on the pitting corrosion of pure aluminium in sulphate ion-containing chloride solution10.1007/BF03026309 ↗
19. Effects of sulphate ion additives on the pitting corrosion of pure aluminium in 0.01M NaCl solution10.1016/S0013-4686(99)00418-1 ↗
20. Adsorption of sulfate and chloride ions on aluminium10.1016/S0013-4686(97)10188-8 ↗
21. Improvements in the etching of hard aluminium electrolytic capacitor foil10.1149/1.2407775 ↗
22. Effect of sulphate anions on tunnel etching of aluminium10.1007/BF00260695 ↗
23. Tunnel morphology in anodic etching of aluminium10.1149/1.1837730 ↗
24. Interpretation of potential transients during aluminium etch tunnel growth in the presence of sulfuric acid10.5796/electrochemistry.69.843 ↗
25. Etching characteristics of high-purity aluminium in hydrochloric acid solutions10.1016/j.msea.2006.01.159 ↗
26. Pit nucleation behaviour of aluminium foil for electrolytic capacitors during early stage of DC etching10.1016/S0010-938X(99)00117-1 ↗
27. Aluminium pitting in chloride solutions: morphology and pit growth kinetics10.1016/0010-938X(90)90112-I ↗
28. S. Ono, H. Habazaki, Morphological change in pits on aluminium during AC etching in hydrochloric acid, to be submitted.
29. AC etching characteristics of aluminium in hydrochloric/sulfuric acid solution10.4139/sfj.49.643 ↗
30. Influence of anodic half cycle on surface area of high purity aluminium foil in hydrochloric acid solution under triangular AC etching10.4139/sfj.54.547 ↗