journal article·2014-07

Ablation mechanism of SiC coated C/C composites at 0° angle in two flame conditions under an oxyacetylene flame

Chang Ni, Kezhi Li, Lei Liu, Hejun Li, Qiangang Fu, Linjun Guo, Ningkun Liu

Corrosion Science· Volume 84
Publisher page

Abstract

Abstract A SiC coating was prepared on the surface of C/C composites by pack cementation and composites were ablated under an oxyacetylene flame in two flame conditions (HF1 and HF2). The gas fluxes of O 2 and C 2 H 2 in HF2 were higher than those in HF1. And the ablation angle was 0° during ablation. The ablation mechanism of composites was analysed. Results showed that SiC coated C/C composites had good ablation resistance in HF1, while SiC coating lost protection in HF2. The influence of oxyacetylene flame on the physico-chemical properties of SiC and SiO 2 was the main reason for different ablation behaviours.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Energetic Materials and Combustion · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. The future of carbon/carbon composite10.1016/0008-6223(87)90116-3 ↗
2. The effect of carbon fabric treatment on delamination of 2D-C/C composites10.1016/j.compscitech.2006.03.025 ↗
3. Carbon–carbon: an overview
4. C/C–SiC composites for space applications and advanced friction systems10.1016/j.msea.2005.08.204 ↗
5. Oxidation protective multilayer coatings for carbon–carbon composites10.1016/S0008-6223(01)00151-8 ↗
6. Modelling of carbon–carbon composite ablation in rocket nozzles10.1016/j.compscitech.2010.04.002 ↗
7. Oxidation protective glass coating for SiC coated carbon/carbon composites for application at 1773K10.1016/j.matlet.2005.09.006 ↗
8. A MoSi2/SiC oxidation protective coating for carbon/carbon composites10.1016/j.corsci.2010.11.024 ↗
9. Oxidation protection of SiC-coated C/C composites by SiC nanowire-toughened CrSi2–SiC–Si coating10.1016/j.corsci.2011.11.001 ↗
10. Mechanical and ablation properties of 2D-carbon/carbon composites pre-infiltrated with a SiC filler10.1016/j.carbon.2006.06.003 ↗
11. Ablation characteristics of carbon fibre reinforced carbon (CFRC) composites in the presence of silicon carbide (SiC) coating10.1016/j.surfcoat.2003.10.071 ↗
12. Microstructure and ablation behavior of SiC coated C/C–SiC–ZrC composites prepared by a hybrid infiltration process10.1016/j.carbon.2013.08.014 ↗
13. Microstructure and ablation mechanism of C/C–SiC composites10.1016/j.jeurceramsoc.2013.08.026 ↗
14. Effects of porous C/C density on the densification behavior and ablation property of C/C–ZrC–SiC composites10.1016/j.carbon.2013.01.059 ↗
15. Structural evolution and ablation mechanism of a hafnium carbide coating on a C/C composite in an oxyacetylene torch environment10.1016/j.corsci.2012.04.033 ↗
16. Mechanism of ablation of 3D C/ZrC–SiC composite under an oxyacetylene flame10.1016/j.corsci.2012.11.009 ↗
17. Effect of reaction melt infiltration temperature on the ablation properties of 2D C/C–SiC–ZrC composites10.1016/j.corsci.2012.01.001 ↗
18. Laser ablation behaviors of SiC–ZrC coated carbon/carbon composites10.1016/j.surfcoat.2011.03.039 ↗
19. Laser ablation behavior and mechanism of C/SiC composite10.1016/j.ceramint.2013.02.012 ↗
20. Degradation of CVD-SiC coated C/SiC composites exposed to the monopropellant combustion products based on Hydroxylammonium nitrate (HAN)10.1016/j.corsci.2013.04.036 ↗
21. C/SiC/MoSi2–Si multilayer coatings for carbon/carbon composites for protection against oxidation10.1016/j.corsci.2011.07.036 ↗
22. Sealing role of B2O3 in MoSi2–CrSi2–Si/B-modified SiC coating for C/C composites10.1016/j.corsci.2012.04.018 ↗
23. Effect of oxidation on elastic modulus of C/C–SiC composites10.1016/j.msea.2007.09.078 ↗
24. Effect of surface ablation products on the ablation resistance of C/C–SiC composites under oxyacetylene torch10.1016/j.corsci.2012.10.003 ↗
25. Effects of SiC addition on the ablation properties of C/C composites in different heat fluxes under oxyacetylene torch10.1016/j.vacuum.2012.09.025 ↗
26. Microstructure and oxidation of multi-layer MoSi2–CrSi2–Si coatings for SiC coated carbon/carbon composites10.1016/j.corsci.2010.05.020 ↗
27. Oxidation mechanism and resistance of ZrB2–SiC composites10.1016/j.corsci.2009.07.005 ↗
28. Growth of nanowires10.1016/j.mser.2008.01.001 ↗
29. Growth mechanism of silica nanowires without a metal catalyst via oxyacetylene torch ablation10.1016/j.matlet.2012.01.056 ↗
30. Effects of nozzle length on flame and emission behaviors of multi-fuel-jet inverse diffusion flame burner10.1016/j.apenergy.2011.02.040 ↗
31. Influence of SiC additive on the ablation behavior of C/C composites modified by ZrB2–ZrC particles under oxyacetylene torch10.1016/j.ceramint.2013.06.036 ↗
32. Perrin · 2005
33. Effect of reference state on exergy efficiencies of one-and two-stage crude oil distillation plants10.1016/j.ijthermalsci.2004.04.015 ↗
34. Comparison of morphology and microstructure of ablation centre of C/SiC composites by oxy-acetylene torch at 2900 and 3550°C10.1016/j.corsci.2008.07.019 ↗
35. Liu · 2002