journal article·2012-04

Susceptibility to stress corrosion cracking of NiTi laser weldment in Hanks’ solution

C.W. Chan, H.C. Man, T.M. Yue

Corrosion Science· Volume 57
Publisher page

Abstract

Abstract In this study, the susceptibility to stress corrosion cracking (SCC) of laser-welded NiTi wires in Hanks’ solution at 37.5 °C was studied by the slow strain-rate test (SSRT) at open-circuit potential and at different applied anodic potentials. The weldment shows high susceptibility to SCC when the applied potential is near to the pitting potential of the heat-affected zone (HAZ). The pits formed in the HAZ become sites of crack initiation when stress is applied, and cracks propagate in an intergranular mode under the combined effect of corrosion and stress. In contrast, the base-metal is immune to SCC under similar conditions. The increase in susceptibility to SCC in the weldment could be attributed to the poor corrosion resistance in the coarse-grained HAZ.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Shape Memory Alloy Transformations · Hydrogen embrittlement and corrosion behaviors in metals · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (52)

Show source-provided references
1. Medical shape memory alloy applications – the market and its products10.1016/j.msea.2003.10.326 ↗
2. On the nature of the biocompatibility and medical applications of NiTi shape memory and superelastic alloys10.3233/BME-1996-6405 ↗
3. Surface, corrosion, and biocompatibility aspects of nitinol as an implant material
4. An overview of nitinol medical applications10.1016/S0921-5093(99)00294-4 ↗
5. Effect of Nd-YAG laser welding on the functional properties of the Ni-49.6at.%Ti10.1016/S0921-5093(99)00422-0 ↗
6. Tensile strength and pseudo-elasticity of YAG laser spot melted TiNi shape memory alloy wires10.2320/matertrans.45.1070 ↗
7. Laser welding of a NiTi alloy: mechanical and shape memory behaviour10.1016/j.msea.2005.08.209 ↗
8. Laser welding of NiTi wires10.1016/j.msea.2006.11.179 ↗
9. Laser welding of thin foil nickel–titanium shape memory alloy10.1016/j.optlaseng.2010.08.007 ↗
10. Effects of process parameters upon the shape memory and pseudo-elastic behaviours of laser-welded NiTi thin foil10.1007/s11661-011-0623-1 ↗
11. The corrosion behaviour of nickel titanium shape memory alloys10.1016/0010-938X(90)90004-O ↗
12. Corrosion properties of laser surface melted NiTi shape memory alloy10.1016/S1359-6462(01)01182-4 ↗
13. Corrosion behavior of nitinol wires in body fluid environments10.1002/jbm.a.10099 ↗
14. Influence of fluoride and chloride on corrosion behaviour of NiTi orthodontic wires10.1016/j.actbio.2007.02.002 ↗
15. Corrosion behaviour of NiTi alloy10.1016/j.electacta.2008.08.001 ↗
16. Stress corrosion behaviour of Ni–Ti shape memory alloys in high temperature water10.2320/jinstmet1952.60.6_577 ↗
17. Localized corrosion behaviour in simulated human body fluids of commercial NiTi orthodontic wires10.1016/S0142-9612(98)90233-2 ↗
18. Stress corrosion cracking of NiTi in artifical saliva10.1016/j.dental.2006.01.001 ↗
19. Effects of acid type on corrosion and fracture behavior of Ni–Ti superelastic alloy under sustained tensile load in physiological saline solution containing hydrogen peroxide10.1016/j.corsci.2008.07.018 ↗
20. Degradation and fracture of Ni–Ti superelastic wire in an oral cavity10.1016/S0142-9612(00)00414-2 ↗
21. Fracture analysis of hydrogen-charged nickel–titanium superelastic alloy10.2320/matertrans.42.141 ↗
22. Susceptibility to delayed fracture of Ni–Ti superelastic alloy10.1016/S0921-5093(02)00201-0 ↗
23. Effects of potential, temperature and pH on hydrogen absorption and thermal desorption behaviors of Ni–Ti superelastic alloy in 0.9% NaCl solution10.1016/j.corsci.2008.04.022 ↗
24. Evaluation of hydrogen absorption behaviour during acid etching for surface modification of commercial pure Ti, Ti-6Al-4V and Ni–Ti superelastic alloys10.1016/j.corsci.2009.12.029 ↗
25. Microelectrochemical corrosion study of super martensitic welds in chloride-containing media10.1016/j.corsci.2011.07.040 ↗
26. Pitting corrosion in pipeline steel weld zones10.1016/j.corsci.2011.08.005 ↗
27. Micro-electrochemical characterization of corrosion of welded X70 pipeline steel in near-neutral pH solution10.1016/j.corsci.2009.04.030 ↗
28. Jones · 1996
29. Effect of post weld heat treatment on stress corrosion cracking of a low alloy steel on stainless steel transition weld10.1016/S0010-938X(00)00182-7 ↗
30. Stress corrosion cracking behaviour of Nd:YAG laser butt welded AZ31 Mg sheet10.1016/j.msea.2006.08.075 ↗
31. Slow strain rate stress corrosion cracking behaviour of as-welded and plasma electrolytic oxidation treated AZ31HP magnesium alloy autogenous laser beam weldment10.1016/j.msea.2009.03.069 ↗
32. Evaluation of environment-assisted cracking susceptibility of a grade X100 pipeline steel10.1016/j.corsci.2011.08.030 ↗
33. Mechanical and functional properties of laser-welded Ti-55.8wt% Ni nitinol wires10.1007/s11661-011-0639-6 ↗
34. ASTM Standard G61-86, Standard test method for conducting cyclic potentiodynamic polarization measurements for localized corrosion susceptibility of iron-, nickel-, or cobalt-based alloys, ASTM standards, ASTM, Philadelphia, PA, USA, 2009.
35. A general model for the repassivation potential as a function of multiple aqueous solution species10.1016/j.corsci.2003.10.002 ↗
36. Pitting corrosion of welded joints of austenitic stainless steels studied by using an electrochemical minicell10.1016/j.corsci.2007.11.028 ↗
37. Characterization of microstructure and local deformation in 316NG weld heat-treated zone and stress corrosion cracking in high temperature water10.1016/j.corsci.2011.02.009 ↗
38. Effect of grain size and twins on corrosion behaviour of AZ31B magnesium alloy10.1016/j.corsci.2009.10.018 ↗
39. Possible origin of superior corrosion resistance for electrodeposited nanocrystalline Ni10.1016/j.scriptamat.2008.03.033 ↗
40. Grain size effects on the corrosion behaviour of Ni50.5Ti49.5 and Ni45.6Ti49.3Al5.1 films10.1016/j.jelechem.2008.02.020 ↗
41. S. Shabalovskaya, G. Rondelli, V. Itin, J Anderegg, Surface and corrosion aspects of NiTi alloys, in: S.M. Russell, A.R. Pelton (Eds.), Proceedings of the International Conference on Shape Memory and Superelastic Technologies, SMST Society Inc., California, 2001. pp. 299–308.
42. Materials of Construction
43. Environmentally assisted cracking behaviour of duplex stainless steel in concentrated sodium chloride solution10.1016/S0010-938X(00)00029-9 ↗
44. Analysis of the galvanostatic polarization method for determining reliable pitting potentials on stainless steels in crevice-free conditions10.1016/S0010-938X(03)00102-1 ↗
45. On the corrosion behaviour of phosphoric irons in simulated concrete pore solution10.1016/j.corsci.2007.06.017 ↗
46. Effects of welding parameters on the mechanical performance of laser welded nitinol10.2320/matertrans.MRA2008243 ↗
47. Effects of local phase conversion on the tensile loading of pulsed Nd:YAG laser processed nitinol10.1016/j.msea.2010.06.025 ↗
48. Aqueous stress corrosion on titanium alloy10.1179/000705975798320783 ↗
49. J. Brettle, Stress corrosion of titanium and its alloy in aqueous chloride environments, Meter. Mater. (1972) 442–451.
50. Fracture of Ni–Ti superelastic alloy under sustained tensile load in physiological saline solution containing hydrogen peroxide10.1002/jbm.a.31173 ↗
51. S. Shabalovskaya, J. Anderegg, G. Rondelli, J.P. Xiong, The effect of surface particulates on the corrosion resistance on nitinol wire, in: A.R. Pelton, T. Duerig (Eds.), Proceedings of the International Conference on Shape Memory and Superelastic Technologies, SMST Society Inc., California, 2003, pp. 399–408.
52. Corrosion behavior of a laser-welded NiTi shape memory alloy10.1016/j.matchar.2006.07.010 ↗