journal article·2015-05Open access

The comparative breakdown of passivity of tin by fluorides and chlorides interpreted through the ‘law of matching affinities’ concept

J.L. Trompette

Corrosion Science· Volume 94
Publisher page

Abstract

The comparative breakdown of passivity of tin by fluorides and chlorides highlight the significant slower kinetics of attack by the kosmotrope fluoride when compared to the chaotrope chloride at pH 5.7 and 10. The origin of this difference is ascribed to the predominant halide-dependent mechanism of attack, pitting with chlorides and film thinning with fluorides, which is conditioned according to the anion-specific hydration properties.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Radioactive element chemistry and processing · Metal Extraction and Bioleaching · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (72)

Show source-provided references
1. The corrosion of tin in nearly neutral solutions10.1039/tf9373301152 ↗
2. The anodic oxidation of metals at very low current density. Part VI. Tin10.1039/jr9540003103 ↗
3. Anodic polarization of tin, nickel and a tin-nickel alloy in alkaline media containing halide ions10.5006/0010-9312-36.11.591 ↗
4. Electrochemical polarization and passivation of tin in neutral solutions of chloride, bromide and iodide ions10.1002/mawe.19820131104 ↗
5. Breakdown of tin passivity in aqueous sodium stannate solution10.1179/000705985798272669 ↗
6. A review on the electrochemistry of tin10.1016/0254-0584(89)90100-4 ↗
7. The corrosion and passivation of tin in borate solutions and the effect of halide ions10.1016/0013-4686(96)00068-0 ↗
8. Electrochemical behaviour of tin in sodium borate solutions and the effect of halide ions and some inorganic inhibitors10.1016/j.corsci.2005.08.002 ↗
9. The anodic behaviour of tin in alkaline solutions-I. 0.1 M sodium borate solution10.1016/0013-4686(63)85012-4 ↗
10. On the anodic passivity of tin in alkaline solutions10.1016/0013-4686(64)85039-8 ↗
11. Some passivation studies on tin electrodes in alkaline solutions10.1016/S0010-938X(67)80114-8 ↗
12. The anodic dissolution of tin in acid chloride solutions10.1016/0022-5088(74)90220-3 ↗
13. Anodic passivation of tin in sodium hydroxide solutions10.1016/S0022-0728(76)80063-0 ↗
14. Anodic passivation of tin in buffered phosphate electrolyte10.1016/S0022-0728(76)80223-9 ↗
15. Electrochemical reactions of tin in aqueous electrolytic solutions10.1016/0376-4583(77)90011-5 ↗
16. On the pitting corrosion of tin in aqueous solutions10.1016/0010-938X(78)90034-3 ↗
17. Anodic behaviour of tin in neutral phosphate solution10.1016/0010-938X(79)90016-7 ↗
18. Anodic passivation of tin in slightly alkaline solutions10.1016/0013-4686(80)80016-8 ↗
19. Potential-pH diagrams for the Sn–H2O–Cl system10.1016/0013-4686(84)87028-0 ↗
20. Electrochemical behaviour of tin in bicarbonate solution at pH 810.1007/BF01103835 ↗
21. On the pitting corrosion of tin by sulphate anion10.1016/0010-938X(92)90009-R ↗
22. Passivation of tin in citrate buffer solutions10.1016/0022-0728(92)80574-N ↗
23. Corrosion and passivation of tin anode in Na2CO3 solutions and the effect of halide ions10.1135/cccc19932013 ↗
24. Electrochemical and X-ray photoelectron spectroscopy studies of passive film on tin in citrate buffer solution10.1016/0022-0728(95)04502-3 ↗
25. Inhibition of chloride pitting corrosion of tin in alkaline and near neutral medium by some inorganic anions10.1016/S0013-4686(96)00212-5 ↗
26. Inhibiting effect of citric acid on the pitting corrosion of tin10.1023/A:1003468731553 ↗
27. Protective film growth on tin in perchlorate and citric acid electrolytes10.1016/S0254-0584(00)00458-2 ↗
28. Role of ClO4− in breakdown of tin passivity in NaOH solutions10.1016/S0010-938X(01)00040-3 ↗
29. Potentiodynamic behaviour of tin in different buffer solutions10.1016/S0010-938X(01)00032-4 ↗
30. Electrochemical studies of the pitting corrosion of tin in citric acid solution containing Cl−10.1016/j.electacta.2008.01.051 ↗
31. Potentiodynamic studies on anodic dissolution and passivation of tin, indium and tin-indium alloys in some fruit acids solutions10.1016/j.corsci.2009.06.050 ↗
32. Polarographic study of the complex ions of tin in fluoride solutions10.1021/ja01649a083 ↗
33. Polarographic studies of the fluoride complexes of tin (II) in neutral and acidic media10.1016/S0022-0728(70)80295-9 ↗
34. Thickness and structure of passive films on iron in acidic and basic solution10.1016/0013-4686(74)87026-X ↗
35. Anodic and cathodic behaviour of tin in alkaline solution10.1016/0013-4686(71)85163-0 ↗
36. The anodic dissolution of tin in sodium hydroxide solutions10.1016/0013-4686(78)85029-4 ↗
37. Passivation of tin10.1016/0013-4686(94)E0064-7 ↗
38. Study of passive film on Sn in the 7–14 pH range10.1016/S0022-0728(01)00432-6 ↗
39. Preparation of nanoporous tin oxide by electrochemical anodization in alkaline electrolytes10.1016/j.electacta.2011.07.085 ↗
40. X-ray photoelectron spectroscopic studies of tin electrodes after polarization in sodium hydroxide solution10.1149/1.2133654 ↗
41. Mössbauer studies of the passive film formed on tin in borate buffer10.1149/1.2131333 ↗
42. The triangular potential sweep voltammetric studies on pure tin in concentrated sodium hydroxide solutions10.1016/0013-4686(83)85225-6 ↗
43. Kinetics of anodic oxide film growth on tin: ionic transport across a barrier in the high-field limit10.1016/0254-0584(94)90145-7 ↗
44. Electrochemically grown tin oxide thin films: in situ characterization of electronic properties and growth mechanism10.1021/jp037530c ↗
45. Oxide/hydroxide films on tin. Part I: kinetic aspects of the electroformation and electroreduction of the films10.1016/j.jelechem.2007.10.002 ↗
46. Oxide/hydroxide films on tin. Part II: characterization of the anodic growth in alkaline solutions10.1016/j.jelechem.2007.10.001 ↗
47. Tin passivation in alkaline media: formation of SnO microcrystals as hydroxyl etching product10.1016/j.electacta.2013.07.200 ↗
48. Thermodynamics of solvation of ion – Part 5: Gibbs free energy of hydration at 298.15 K10.1039/FT9918702995 ↗
49. Ions in water: characterizing the forces that control chemical processes and biological structure10.1016/j.bpc.2007.03.009 ↗
50. Viscosity B-coefficient of ions in solution10.1021/cr00040a004 ↗
51. Marcus · 1997
52. Ions from the Hofmeister series and osmolytes: effects on proteins in solution and in the crystallization process10.1016/j.ymeth.2004.03.021 ↗
53. Perrin · 1982
54. Pitting potentials and inhibition potentials of iron and nickel for different aggressive and inhibiting anions10.1016/0010-938X(77)90002-6 ↗
55. The breakdown of passivity of iron and nickel by fluoride10.1016/S0010-938X(79)80123-7 ↗
56. The thinning of the passive layer of iron by halides10.1002/maco.19850360104 ↗
57. Breakdown of passivity of iron by fluorides10.1016/0013-4686(83)85043-9 ↗
58. Involvement of surface oxide film on iron in halide-induced pitting10.1016/0013-4686(89)87090-2 ↗
59. Use of SIMS to investigate the induction stage in the pitting of iron10.1149/1.2096916 ↗
60. Mechanisms of pitting corrosion
61. Implications of the kosmotrope/chaotrope nature of the anions on the breakdown of passivity of iron by halides10.1016/j.corsci.2014.01.005 ↗
62. The nature of the chemical bond. IV. The energy of single bonds and the relative electronegativity of atoms10.1021/ja01348a011 ↗
63. H. Gamsjäger, T. Gajda, J. Sangster, S.K. Saxena, W. Voigt, Chemical thermodynamics of tin, in: ‘Chemical Thermodynamics’ Series, Ed. O.E.C.D., vol. 12, Nuclear Energy Agency, Issy les Moulineaux, 2012.
64. A critical review of thermodynamic data for inorganic tin species10.1016/S0016-7037(01)00645-7 ↗
65. Influence of the anion specificity on the electrochemical corrosion of anodized aluminium substrates10.1016/j.electacta.2009.12.063 ↗
66. Influence of the anion specificity on the anodic polarization of titanium10.1016/j.corsci.2010.12.021 ↗
67. The localized breakdown and repair of passive surfaces during pitting10.1016/0010-938X(89)90038-3 ↗
68. Pitting of titanium10.1149/1.2403253 ↗
69. Pitting corrosion of aluminium10.1016/S0010-938X(99)00012-8 ↗
70. Pitting corrosion of titanium: the relationship between pitting potential and competitive anion adsorption at the oxide film/electrolyte interface10.1149/1.1393364 ↗
71. Thin oxide film formation on metals
72. TiO2 nanotubes: synthesis and applications10.1002/anie.201001374 ↗