journal article·2016-05

The influence of the high Fe and Cr contents of Alloy 800 on its inter- and intragranular oxidation tendency in 480 °C hydrogenated steam

S.Y. Persaud, S. Ramamurthy, A. Korinek, G.A. Botton, R.C. Newman

Corrosion Science· Volume 106
Publisher page

Abstract

Abstract Alloy 800 was exposed to 480 °C hydrogenated steam with conditions maintained at an oxygen partial pressure well below the dissociation pressure of NiO. Oxidation phenomena in Alloy 800 were investigated using high resolution electron microscopy techniques. Limited oxygen penetration was detected at grain boundaries while extensive internal oxidation occurred intragranularly. Internal oxidation was possible in an alloy containing a reactive solvent element, Fe, with the solute element, Ni, displaced to the surface. Several stress relief mechanisms are observed to operate simultaneously. The relevance of the observed oxidation phenomena on the primary water SCC resistance of Alloy 800 is discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Fusion materials and technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. Dependence of stress corrosion cracking of Alloy 690 on temperature, cold work, and carbide precipitation—role of diffusion of vacancies at crack tips10.5006/1.3563640 ↗
2. Linking grain boundary microstructure to stress corrosion cracking of cold-rolled Alloy 690 in pressurized water reactor primary water10.5006/0808 ↗
3. One dimensional cold rolling effects on stress corrosion crack growth in Alloy 690 tubing and plate materials
4. Effect of Deformation and Orientation on SCC of Alloy 690
5. SCC of Alloy 690 and its weld metals
6. Environmentally assisted crack growth in one-dimensionally cold worked Alloy 690TT in primary water10.1016/j.corsci.2011.12.031 ↗
7. Analytical electron microscopy of a crack tip extracted from a stressed Alloy 800 sample exposed to an acid sulfate environment10.1016/j.micron.2014.02.011 ↗
8. An electrochemical study assisting the interpretation of acid sulfate stress corrosion cracking of NiCrFe alloys10.1016/j.corsci.2014.10.033 ↗
9. Update of Alloy 800 behaviour in secondary side of PWR steam generators
10. Electrochemical aspects of the stress corrosion cracking of Fe–Cr–Ni alloys in caustic solutions10.1016/0010-938X(80)90135-3 ↗
11. Intergranular stress corrosion cracking growth behavior of Ni–Cr–Fe alloys in pressurized water reactor primary water10.5006/1205 ↗
12. Comparison of corrosion resistance of UNS N06690TT and UNS N08800SN in simulated primary water with various concentrations of dissolved oxygen10.5006/1167 ↗
13. Some possible mechanisms of intergranular stress corrosion cracking of Alloy 600 in PWR primary water
14. The effects of stress on the internal oxidation of Ni–Cr and Ni–Al alloys10.4028/www.scientific.net/MSF.251-254.341 ↗
15. Internal oxidation of Ni–Al and Ni–Al–Si Alloys at the dissociation pressure of NiO10.1016/0956-7151(94)90292-5 ↗
16. The morphological and structural development ot internal oxides in nickel–aluminum alloys at high temperatures10.1007/BF00662034 ↗
17. Internal oxidation10.1179/mst.1988.4.12.1072 ↗
18. The third-element effect in the oxidation of Ni–xCr–7Al (x=0 5. 10. 15at.%) alloys in 1atm oxygen at 900–1000°C10.1016/j.corsci.2006.03.008 ↗
19. Enhanced diffusion of oxygen during internal oxidation of nickel-base alloys10.1080/01418618208236942 ↗
20. Grain boundary embrittlement of Alloy 600 by internal oxidation in simulated primary water environments
21. Internal oxidation of Alloy 600 exposed to hydrogenated steam and the beneficial effects of thermal treatment10.1016/j.corsci.2014.04.041 ↗
22. Internal oxidation of Alloy 690 in hydrogenated steam10.1016/j.corsci.2014.11.006 ↗
23. The effect of weld chemistry on the oxidation of Alloy 82 dissimilar metal welds10.1016/j.corsci.2014.10.044 ↗
24. Internal oxidation of Ag-in alloys: stress relief and the influence of imposed strain10.1007/BF00664274 ↗
25. High-temperature behavior of a Pd–Ag alloy for porcelain10.1177/00220345830620121201 ↗
26. The transition from internal to external oxidation and the formation of interruption bands in silver–indium alloys10.1016/0001-6160(61)90103-1 ↗
27. Kinetic study of the low temperature internal oxidation of nickel based model alloys exposed to PWR primary water10.4028/www.scientific.net/MSF.595-598.449 ↗
28. Oxidation of Ni base alloys in PWR water: oxide layers and associated damage to the base metal
29. Examinations of oxidation and sulfidation of grain boundaries in Alloy 600 exposed to simulated pressurized water reactor primary water10.1017/S1431927613000421 ↗
30. Grain boundary oxidation and embrittlement prior to crack initiation in Alloy 600 in PWR primary water
31. TEM investigations of intergranular stress corrosion cracking in austenitic alloys in PWR environmental conditions10.1179/mht.2003.066 ↗
32. Corrosion behavior for Alloy 690 and Alloy 800 tubes in simulated primary water10.1016/j.corsci.2012.10.018 ↗
33. Influence of oxide films on primary water stress corrosion cracking initiation of Alloy 60010.1016/j.jnucmat.2005.10.002 ↗
34. Three-dimensional characterization of stress corrosion cracks10.1016/j.jnucmat.2010.11.068 ↗
35. Effect of dissolved hydrogen on corrosion of Inconel Alloy 600 in high temperature hydrogenated water10.1016/j.electacta.2011.07.032 ↗
36. High-resolution characterization of intergranular attack and stress corrosion cracking of Alloy 600 in high-temperature primary water10.5006/1.3280561 ↗
37. S.Y. Persaud, R.C., Newman, J., Smith, A., Korinek, G.A. Botton, High Resolution Analysis of Oxidation in Ni-Fe-Cr Alloys after Exposure to 315 °C Deaerated Water with added Hydrogen, Corrosion Science, Manuscript submitted for publication (2015).10.1016/j.corsci.2016.02.009 ↗
38. Characterisation of stress corrosion cracking and internal oxidation of Alloy 600 in high temperature hydrogenated steam
39. Oxidation studies of Alloy 600 in low pressure hydrogenated steam
40. Alloy oxidation studies related to PWSCC
41. Effect of surface preparation on intergranular stress corrosion cracking of Alloy 600 in hydrogenated steam10.5006/1.3279916 ↗
42. Oxidation embrittlement of Alloy 600 in hydrogenated steam at 400°C
43. Internal oxidation and embrittlement of Alloy 600
44. Oxidation embrittlement of Alloy 600 in hydrogenated steam at 400°C
45. An atom probe tomography study of internal oxidation processes in Alloy 600
46. IGSCC behaviour of Alloy 600 steam generator tubing in water or steam tests above 360°C10.5006/1.3583859 ↗
47. Alloy 690 surface nanostructures during exposure to PWR primary water and potential influence on stress corrosion crack initiation
48. Penetrative internal oxidation from Alloy 690 surfaces and stress corrosion crack walls during exposure to PWR primary water
49. The oxidation of NiAl-III. Internal and intergranular oxidation10.1016/0010-938X(94)90107-4 ↗