Abstract
Abstract Cycling oxidation behavior of the nanocrystalline coating on the N5 superalloy substrate of different surface finishing is investigated at 1050 °C. Results indicate that the surface finishing of the alloy substrate affects oxidation behavior of the sputtered nanocrystalline coating. After cyclic oxidation, oxide scale on the nanocrystalline coating rumples heavily and spalls off following a way of layer-by-layer in case that the alloy substrate is pretreated by sand blasting. However, it just roughens rather than rumples when the alloy substrate is pre-polished or ground by 2000# SiC paper and its spallation follows a way of bulk fracture.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Metal and Thin Film Mechanics · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. A duplex nanocrystalline coating for high-temperature applications on single-crystal superalloy10.1016/j.corsci.2015.09.020 ↗
2. Comparative study of oxidation and interdiffusion behavior of AIP NiCrAlY and sputtered nanocrystalline coatings on a nickel-based single-crystal superalloy10.1016/j.corsci.2015.05.062 ↗
3. Ta effect on oxidation of a nickel-based single-crystal superalloy and its sputtered nanocrystalline coating at 900–1100°C10.1016/j.apsusc.2015.03.157 ↗
4. Corrosion behaviour of an aluminized nickel coating in a carbon dioxide capture process using aqueous monoethanolamine10.1016/j.corsci.2011.07.009 ↗
5. High-temperature oxidation of hot-dip aluminizing coatings on a Ti3Al–Nb alloy and the effects of element additions10.1016/j.corsci.2012.07.009 ↗
6. Thermal barrier coatings for gas-turbine engine applications10.1126/science.1068609 ↗
7. Coatings for blade and vane applications in gas turbines10.1016/0010-938X(89)90104-2 ↗
8. Oxidation behavior of sputtered microcrys-talline coating of superalloy K17F at high temperature10.1016/0921-5093(95)10021-0 ↗
9. Cross-sectional oxide distribution of cast IN738 and its sputtered coating at 1000°C10.1016/S0257-8972(02)00909-X ↗
10. Oxidation and hot corrosion behavior of sputtered nanocrystalline coating of superalloy K5210.1016/j.tsf.2007.07.131 ↗
11. Influence of sputtered nanocrystalline coating on oxidation and hot corrosion of a nickel-based super-alloy M95110.1016/j.jmst.2014.01.001 ↗
12. Effect of microcrystallization on the cyclic oxidation behavior of ß-NiAl intermetallics at 1000°C in air10.1016/S0966-9795(01)00059-0 ↗
13. Effect of a sputtered TiAlCr coating on the oxidation resistance of TiAl intermetallic compound10.1007/BF02153463 ↗
14. The scaling behavior of sputtered Ni3Al coatings with and without Pt modification10.1016/j.corsci.2012.01.008 ↗
15. High temperature oxidation of NiCrAlY, nanocrystalline and enamel-metal nano-composite coatings under thermal shock10.1016/j.corsci.2015.08.033 ↗
16. Rumpling of CVD (Ni,Pt)Al diffusion coatings under intermediate temperature cycling10.1016/j.surfcoat.2009.04.016 ↗
17. Cyclic oxidation-induced cracking of platinum-modified nickel-aluminide coatings10.1016/j.scriptamat.2009.02.012 ↗
18. On the initiation of cyclic oxidation-induced rumpling of platinum-modified nickel aluminide coatings10.1016/j.actamat.2008.12.015 ↗
19. Effect of superimposed uniaxial stress on rumpling of platinum-modified nickel aluminide coatings10.1016/j.actamat.2009.01.040 ↗
20. Surface rumpling of a (Ni, Pt)Al bond coat induced by cyclic oxidation10.1016/S1359-6454(00)00156-7 ↗
21. Rumpling induced by thermal cycling of an overlay coating: the effect of coating thickness10.1016/j.actamat.2003.10.001 ↗
22. Influence of grit blasting pre-treatment on the adhesion strength of plasma sprayed coatings: fractal analysis of roughness10.1016/S0257-8972(97)00628-2 ↗
23. Effect of grit-blasting on substrate roughness and coating adhesion10.1361/105996306X124347 ↗
24. Effect of sand blasting and glass matrix composite coating on oxidation resistance of a nickel-based superalloy at 1000°C10.1016/j.corsci.2013.04.022 ↗
25. Comparison of chromia growth kinetics in a Ni-based superalloy, with and without shot-peening10.1016/j.corsci.2015.07.033 ↗
26. Effect of sand blasting on oxidation behavior of K38G superalloy at 1000°C10.1016/j.corsci.2014.12.015 ↗
27. Study of Cr2O3 coating materials and characterization by an interfacial test
28. Characterization of plastic deformation induced by shot-Peening in a Ni-Base superalloy10.1007/s11837-014-1184-8 ↗
29. Effect of shot peening on surface characteristics of Ni-based single-crystal superalloy10.2320/matertrans.M2013153 ↗
30. Analysis of shot-peening and residual stress relaxation in the nickel-based superalloy RR 100010.1016/j.actamat.2013.01.031 ↗
31. The effect of grit blasting on the oxidation behavior of a platinum-modified nickel-aluminide coating10.1007/s11661-001-0235-2 ↗
32. On the rumpling mechanism in nickel-aluminide coatings Part I: an experimental assessment
33. On the rumpling mechanism in nickel-aluminide coatings Part II: characterization of surface undulations and bond coat swelling
34. The effect of bond coat grit blasting on the durability and thermally grown oxide stress in an electron beam physical vapor deposited thermal barrier coating10.1016/S0257-8972(03)00466-3 ↗
35. Experimental study of the growth evolution from random towards a (111) preferential orientation of PVD TiN coatings10.1016/0040-6090(94)06355-9 ↗
36. A quantitative model for the evolution from random orientation to a unique texture in PVD thin film growth10.1016/0040-6090(94)06353-2 ↗
37. Columnar structures in polycrystalline thin films developed by competeive growth10.1016/S0040-6090(97)00661-5 ↗
38. Fundamental structure forming phenomena of polycrystalline films and the structure zone models10.1016/S0040-6090(97)00503-8 ↗
39. A study of the corrosion properties of TiN coated and nitrided Ti-6Al-4V10.1016/0010-938X(95)00065-R ↗
40. An electrochemical study of magnetron sputtered Ti- and TiN-coated steel10.1016/S0010-938X(97)00119-4 ↗