journal article·2020-07Open access

Kinetic and thermodynamic analysis of high-temperature CO2 corrosion of carbon steel in simulated geothermal NaCl fluids

N. Mundhenk, S. Carrero, K.G. Knauss, R. Wonneberger, A. Undisz, Y. Wu

Corrosion Science· Volume 171

Abstract

Abstract We discuss kinetic and thermodynamic aspects of carbon steel corrosion in CO2-containing NaCl fluids up to 240 °C. Crystalline nm-thick Fe-oxide films only form at 160 °C and 240 °C providing instantaneous and moderate corrosion protection. The absence of Fe-oxide at 80 °C results in high initial corrosion rates until a moderately protective, but thick and porous, FeCO3 film forms. From the metal/film interface it grows inwards by replacing ferrite with FeCO3. TEM reveals a precursory, likely hydrated and chloride-containing, phase that predates FeCO3 formation. Thermodynamic predictions agree well with experimental results in that Fe-oxide formation is favored over FeCO3 towards higher temperatures.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Ellis · 1977
2. Effect of CO2 and H2S on the composition and stability of passive film on iron alloys in geothermal water10.1016/j.electacta.2007.01.086 ↗
3. Barite scale control at the Soultz-sous-Forets (France) EGS site
4. Metal corrosion in geothermal brine environments of the upper Rhine graben–laboratory and on-site studies10.1016/j.geothermics.2012.10.006 ↗
5. Corrosion and scaling as interrelated phenomena in an operating geothermal power plant10.1016/j.corsci.2013.01.003 ↗
6. Electrochemical study of the corrosion of different alloys exposed to deaerated 80 °C geothermal brines containing CO210.1016/j.corsci.2014.03.027 ↗
7. On-site erosion-corrosion testing in superheated geothermal steam10.1016/j.geothermics.2014.01.007 ↗
8. Material selection for dew-point corrosion in geothermal fluids containing acid chloride10.1016/j.geothermics.2017.05.010 ↗
9. Posey · 1977
10. Casing pipe materials for deep geothermal wells
11. Key issues related to modelling of internal corrosion of oil and gas pipe-lines–a review10.1016/j.corsci.2007.06.006 ↗
12. Corrosion of carbon steel and the passivating properties of corrosion films formed under high-PT geothermal conditions10.1016/j.scitotenv.2019.04.386 ↗
13. Evolution of dissolution processes at the interface of carbon steel corroding in a CO2 environment studied by EIS10.1016/j.corsci.2009.10.007 ↗
14. Spontaneous passivation observations during scale formation on mild steel in CO2 brines10.1016/j.electacta.2011.03.053 ↗
15. Corrosion behavior of SM 80SS tube steel in stimulant solution containing H2S and CO210.1016/j.electacta.2007.12.039 ↗
16. Reactions of pipeline steels in carbon dioxide solutions10.1016/S0010-938X(98)00104-8 ↗
17. Effect of HCO3- on electrochemical kinetics of carbon steel corrosion in CO2-saturated brines10.1016/j.electacta.2018.09.114 ↗
18. Modeling of scale formation and corrosion from geothermal water10.1016/S0013-4686(97)00242-9 ↗
19. First stages of siderite crystallization during CO2 corrosion of steel evaluated using in situ synchroton small- and wide-angle X-ray scattering10.1039/C4FD00218K ↗
20. Formation, transformation and dissolution of phases formed on surfaces
21. Effect of pH on corrosion of mild steel at elevated temperatures
22. Parkhurst · 1999
23. Bethke · 1996
24. Validation of corrosion rates measured by the Tafel extrapolation method10.1016/j.corsci.2005.05.046 ↗
25. Kinetics of the corrosion of iron in aqueous electrolytes at temperatures up to 300 °C10.1002/bbpc.199000057 ↗
26. Role of conductive corrosion products in the protectiveness of corrosion layers10.5006/1.3284844 ↗
27. Impedance studies of the growth of porous magnetite films on carbon steel in high temperature aqueous systems10.1016/0010-938X(83)90063-X ↗
28. The mechanism of high temperature aqueous corrosion of steel10.1016/0010-938X(89)90120-0 ↗
29. The anodic oxidation of iron in neutral solution I. The nature and composition of the passive film10.1149/1.2425555 ↗
30. Construction and verification of pourbaix diagrams for CO2 corrosion of mild steel valid up to 250 °C
31. Effect of steel microstructure on corrosion rate and protective iron carbonate film formation10.5006/1.3290361 ↗
32. On the fundamentals of electrochemical corrosion of X65 steel in CO2-containing formation water in the presence of acetic acid in petroleum production10.1016/j.corsci.2008.10.013 ↗
33. An in situ synchroton radiation grazing incidence X-ray diffraction study of carbon dioxide corrosion10.1149/1.2007227 ↗
34. Causes of abundant calcite scaling in geothermal wells in the Bavarian Molasse Basin, Southern Germany10.1016/j.geothermics.2017.05.001 ↗
35. The EQ3/6 software package for geochemical modeling: current status
36. Landolt · 2007
37. New insights on the role of CO2 in the mechanism of carbon steel corrosion10.1016/j.corsci.2017.02.016 ↗
38. Near surface pH measurements in aqueous CO2 corrosion10.1016/j.electacta.2018.09.117 ↗
39. The formation of FeCO3 and Fe3O4 on carbon steel and their protective capabilities against CO2 corrosion at elevated temperature and pressure10.1016/j.corsci.2019.06.016 ↗