Effect of deposition temperature on the corrosion behavior of CVD SiC coatings on SiCf/SiC composites under simulated PWR conditions
Source abstract
Abstract
Abstract To improve the hydrothermal corrosion resistance of SiCf/SiC composites, SiC coatings were chemical vapor deposited at 1000, 1150 and 1200 °C. Their corrosion behaviors were investigated using immersion tests and various analytical methods. The intergranular corrosion phenomenon was observed at all three coatings. It caused the delamination on the surface of 1000 and 1150 °C coatings, whereas only the local fall-off of large grains occurred on the 1200 °C coating. The large grain size and high crystallinity of coating deposited at 1200 °C contributed to the excellent corrosion resistance compared with coatings deposited at other two temperatures.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Metal and Thin Film Mechanics · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Handbook of SiC properties for fuel performance modeling10.1016/j.jnucmat.2007.05.016 ↗
2. Stability of SiC and its composites at high neutron fluence10.1016/j.jnucmat.2010.12.088 ↗
3. Thermophysical and mechanical properties of near-stoichiometric fiber CVI SiC/SiC composites after neutron irradiation at elevated temperatures10.1016/j.jnucmat.2010.06.002 ↗
4. Accident tolerant fuels for LWRs: a perspective10.1016/j.jnucmat.2013.12.005 ↗
5. Accident tolerant fuel cladding development: promise, status, and challenges10.1016/j.jnucmat.2017.12.043 ↗
6. Current research and development activities on fission products and hydrogen risk after the accident at Fukushima Daiichi Nuclear Power Station
7. Safety assessment of SiC cladding oxidation under loss-of-Coolant accident conditions in light water reactors10.13182/NT12-122 ↗
8. Oxidation behavior of silicon carbide at 1200 °C in both air and water-vapor-rich environments10.1016/j.corsci.2014.07.052 ↗
9. Pitting corrosion in CVD SiC at 300 °C in deoxygenated high-purity water10.1016/j.jnucmat.2008.03.025 ↗
10. Corrosion behavior of reaction-bonded silicon carbide ceramics in high-temperature water10.1023/A:1015797324658 ↗
11. Factors affecting the hydrothermal corrosion behavior of chemically vapor deposited silicon carbides10.1016/j.jnucmat.2019.03.026 ↗
12. Hydrothermal degradation of chemical vapour deposited SiC fibres10.1023/A:1004480814477 ↗
13. Hydrothermal corrosion of SiC in LWR coolant environments in the absence of irradiation10.1016/j.jnucmat.2015.06.019 ↗
14. Corrosion behaviors of sintered and chemically vapor deposited silicon carbide ceramics in water at 360 °C10.1023/A:1023390111074 ↗
15. Microstructure and hydrothermal corrosion behavior of NITE-SiC with various sintering additives in LWR coolant environments10.1016/j.jeurceramsoc.2016.11.033 ↗
16. H. Feinroth, B.R. Hao. Multi-layered ceramic tube for fuel containment barrier and other applications in nuclear and fossil power plants. US20060039524A1.
17. Hydrothermal corrosion behavior of SiCf/SiC composites candidate for PWR accident tolerant fuel cladding10.1016/j.ceramint.2018.09.079 ↗
18. Influence of microstructure on hydrothermal corrosion of chemically vapor processed SiC composite tubes10.1016/j.jnucmat.2017.05.010 ↗
19. Effect of dissolved hydrogen on the corrosion behavior of chemically vapor deposited SiC in a simulated pressurized water reactor environment10.1016/j.corsci.2015.05.031 ↗
20. Long-term corrosion behavior of CVD SiC in 360 °C water and 400 °C steam10.1016/j.jnucmat.2013.07.058 ↗
21. Role of irradiation-induced defects on SiC dissolution in hot water10.1016/j.corsci.2016.08.007 ↗
22. Hydrothermal corrosion behavior of CVD SiC in high temperature water10.1016/j.jnucmat.2020.152241 ↗
23. Effect of free carbon on micro-mechanical properties of a chemically vapor deposited SiC coating10.1016/j.ceramint.2018.06.165 ↗
24. Effect of microstructure on the corrosion of CVD-SiC exposed to supercritical water10.1016/j.jnucmat.2009.08.008 ↗
25. Quantitative analysis of stacking faults in the structure of SiC by X-ray powder profile refinement method10.2109/jcersj.96.1003 ↗
26. High-resolution electron microscopy observations of stacking faults in β-SiC10.1111/j.1151-2916.1989.tb06014.x ↗
27. Raman investigation of SiC polytypes10.1002/1521-396X(199707)162:1<39::AID-PSSA39>3.0.CO;2-L ↗
28. Mechanical properties of CVD-SiC coatings with Si impurity10.1016/j.ceramint.2018.08.266 ↗
29. A microstructural study of silicon carbide fibres through the use of Raman microscopy10.1023/A:1004830505979 ↗
30. Raman spectral characterization of silicon carbide nuclear fuel coatings10.1111/j.1151-2916.1983.tb10075.x ↗
31. A.V. Naumkin, A. Kraut-Vass, S.W. Gaarenstroom, C.J. Powell. NIST standard reference database 20, version 4.1. https://doi.org/10.18434/T4T88K.
32. Composition, microstructure, and thermal stability of silicon carbide chemical vapor deposited at low temperatures10.1016/S0924-0136(00)00428-3 ↗
33. Kinetic laws of the chemical process in the CVD of SiC ceramics from CH3SiCl3-H2 precursor10.1051/jp4:1993373 ↗
34. Experimental kinetic study of the chemical vapour deposition of SiC-based ceramics from CH3SiCl3/H2 gas precursor10.1016/0022-0248(95)00180-8 ↗
35. The structure of chemical vapor deposited silicon carbide10.1016/0040-6090(77)90103-1 ↗
36. Revealing irradiation damage along with the entire damage range in ion-irradiated SiC/SiC composites using Raman spectroscopy10.1016/j.jnucmat.2019.151778 ↗
37. A study of the microstructure and mechanical properties of SiC coatings on spherical particles10.1016/j.jeurceramsoc.2011.12.014 ↗