journal article·2021-12

Effect of pre-oxidation on the failure mechanisms of EB-PVD thermal barrier coatings with (Ni,Pt)Al bond coats

S. Li, M.M. Xu, C.Y. Zhang, Z.B. Bao, Y.F. Yang, S.L. Zhu, F.H. Wang

Corrosion Science· Volume 193
Publisher page

Abstract

Abstract In order to clarify the effect of pre-oxidation for (Ni,Pt)Al bond coat on failure modes of TBCs, cyclic oxidation behavior of thermal barrier coatings system with both pre-oxidized and normal (Ni,Pt)Al bond coats was investigated at 1100 °C. The results indicated that thermal cycling resistance of TBCs was dramatically enhanced by pre-oxidation, where thinner and lower residual stress oxide scale, lighter rumpling of the BC/TGO interface were achieved pre-oxidized. The failure modes of these two TBCs were completely diverse. Besides, the lower oxygen partial pressure effectively enhanced transformation from θ to α-Al2O3 during pre-oxidation.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Advanced materials and composites · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Thermal-barrier coatings for more efficient gas-turbine engines10.1557/mrs.2012.232 ↗
2. Thermal barrier coatings for gas-turbine engine applications10.1126/science.1068609 ↗
3. Advanced structural ceramics in aerospace propulsion10.1038/nmat4687 ↗
4. Mechanisms controlling the durability of thermal barrier coatings10.1016/S0079-6425(00)00020-7 ↗
5. Mechanism of spallation in platinum aluminide/electron beam physical vapor-deposited thermal barrier coatings10.1007/s11661-999-0332-1 ↗
6. Oxidation-induced failure of EB-PVD thermal barrier coatings10.1016/S0257-8972(01)01482-7 ↗
7. The formation of aluminum oxide scales on high-temperature alloys10.1007/BF00666913 ↗
8. Development of a pre-oxidation treatment to improve the adhesion between thermal barrier coatings and NiCoCrAlY bond coatings10.1007/s11085-006-9036-8 ↗
9. The effect of pre-oxidation atmosphere on the durability of EB-PVD thermal barrier coatings with CoNiCrAlY bond coats10.1016/j.surfcoat.2007.10.001 ↗
10. The effect of oxidation pre-treatment on the cyclic life of EB-PVD thermal barrier coatings with platinum–aluminide bond coats10.1016/j.surfcoat.2005.07.088 ↗
11. Effect of thermally grown oxide (TGO) microstructure on the durability of TBCs with PtNiAl diffusion bond coats10.1016/j.msea.2005.11.014 ↗
12. Microstructural analysis after furnace cyclic testing of pre-oxidized ReneN5/(Ni,Pt)Al/7YSZ thermal barrier coatings10.1016/j.surfcoat.2020.126376 ↗
13. Co-doping effect of Hf and Y on improving cyclic oxidation behavior of (Ni,Pt)Al coating at 1150 °C10.1016/j.corsci.2020.109093 ↗
14. Determination of the piezospectroscopic coefficients for chromium-doped sapphire10.1111/j.1151-2916.1995.tb08493.x ↗
15. Kinetic study of the competitive growth between θ- Al2O3 and α-Al2O3 during the early stages of oxidation of β-(Ni,Pt)Al bond coat systems: Effects of low oxygen partial pressure and temperature10.1007/s11661-014-2669-3 ↗
16. On basal slip and basal twinning in sapphire (α-Al2O3)—I. Basal slip revisited10.1016/1359-6454(95)00264-2 ↗
17. Metastable alumina polymorphs: crystal structures and transition sequences10.1111/j.1151-2916.1998.tb02581.x ↗
18. The formation of α-Al2O3 from θ-Al2O3: The relevance of a “critical size” and: Diffusional nucleation or “synchro-shear”?10.1023/A:1017545213590 ↗
19. The mechanism of simultaneous sintering and phase transformation in alumina10.1007/BF00708257 ↗
20. Metastable alumina polymorphs: crystal structures and transition sequences10.1111/j.1151-2916.1998.tb02581.x ↗
21. Alumina scale formation: a new perspective
22. Assessment of TBC systems failure mechanisms using a fracture mechanics approach10.1016/j.actamat.2005.06.003 ↗
23. Strength degradation and failure mechanisms of electron-beam physical-vapor-deposited thermal barrier coatings10.1111/j.1151-2916.2001.tb00875.x ↗
24. Characterization of a cyclic displacement instability for a thermally grown oxide in a thermal barrier system10.1016/S1359-6454(01)00071-4 ↗
25. Mechanisms for the failure of electron beam physical vapor deposited thermal barrier coatings induced by high temperature oxidation
26. Preparation and enhanced oxidation performance of a Hf-doped single-phase Pt-modified aluminide coating10.1016/j.corsci.2016.09.014 ↗
27. The oxidation behaviour of NiAl-I. Phase transformations in the alumina scale during oxidation of NiAl and NiAl-Cr alloys10.1016/0010-938X(92)90002-K ↗
28. Microstructural study of the theta-alpha transformation in alumina scales formed on nickel-aluminides10.1179/mht.2000.011 ↗
29. Effect of θ-alumina formation on the growth kinetics of alumina-forming superalloys10.1007/BF01048641 ↗
30. Surface rumpling of a (Ni,Pt)Al bond coat induced by cyclic oxidation10.1016/S1359-6454(00)00156-7 ↗
31. The role of chemical composition on the oxidation performance of aluminide coatings10.1016/j.surfcoat.2004.08.007 ↗
32. Understanding of failure mechanisms of the oxide scales formed on nanocrystalline coatings with different Al content during cyclic oxidation10.1016/j.actamat.2020.116576 ↗
33. Comparison of thermal expansion and oxidation behavior of various high-temperature coating materials and superalloys10.1179/mht.2004.012 ↗
34. The influence of bondcoat and topcoat mechanical properties on stress development in thermal barrier coating systems10.1016/j.actamat.2009.01.017 ↗
35. Modeling of residual stress in oxide scales10.1023/A:1018822222663 ↗
36. Wrinkling of α-alumina films grown by oxidation-II. Oxide separation and failure10.1016/S1359-6454(98)00134-7 ↗
37. Application of a simple statistical spalling model for the analysis of high-temperature, cyclic-oxidation kinetics data10.1023/A:1023004430423 ↗