journal article·2012-12

Influence of applied strain on the microstructural corrosion of AlMg2 as-cast aluminium alloy in sodium chloride solution

Halina Krawiec, Zbigniew Szklarz, Vincent Vignal

Corrosion Science· Volume 65
Publisher page

Abstract

The corrosion behavior of ISO AlMg2 (AA5052) was studied at the microscale using the Electrochemical Microcell Technique. The influence of plastic deformation on the corrosion resistance of this alloy was also examined. After polishing, pitting at small copper-enriched precipitates and structural etching were observed. After deformation, numerous slip bands were found in grains. After 5.5% plastic strain, the global electrochemical behavior of samples was significantly affected. Pitting potential was decreased in sites containing slip bands or in sites with large strain gradients (measured using microgauges deposited by lithography).
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Corrosion Behavior and Inhibition · Anodic Oxide Films and Nanostructures

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (52)

Show source-provided references
1. Vargel · 2004
2. Miller · Mater. Sci. Eng. A · 2000 · 280 · 3710.1016/S0921-5093(99)00653-X ↗
3. Starke · Prog. Aerosp. Sci. · 1996 · 32 · 13110.1016/0376-0421(95)00004-6 ↗
4. Nisancioglu · J. Electrochem. Soc. · 1990 · 137 · 6910.1149/1.2086441 ↗
5. McCafferty · J. Electrochem. Soc. · 2003 · 150 · B23810.1149/1.1566412 ↗
6. Searles · Metall. Mater. Trans. A · 2001 · 32 · 285910.1007/s11661-001-1036-3 ↗
7. Birbilis · Corros. Sci. · 2006 · 48 · 420210.1016/j.corsci.2006.02.007 ↗
8. Birbilis · J. Electrochem. Soc. · 2005 · 152 · B14010.1149/1.1869984 ↗
9. Grilli · Corros. Sci. · 2010 · 52 · 285510.1016/j.corsci.2010.04.035 ↗
10. Guillaumin · Corros. Sci. · 1998 · 41 · 42110.1016/S0010-938X(98)00116-4 ↗
11. Campestrini · Corros. Sci. · 2000 · 42 · 185310.1016/S0010-938X(00)00002-0 ↗
12. Little · Corros. Sci. · 2007 · 49 · 34710.1016/j.corsci.2006.04.024 ↗
13. Ambat · Corros. Sci. · 2006 · 48 · 345510.1016/j.corsci.2006.01.005 ↗
14. Bethencourt · Corros. Sci. · 2009 · 51 · 51810.1016/j.corsci.2008.12.027 ↗
15. Blanc · Corros. Sci. · 1997 · 39 · 49510.1016/S0010-938X(97)86099-4 ↗
16. Blanc · Corros. Sci. · 2006 · 48 · 383810.1016/j.corsci.2006.01.012 ↗
17. Birbilis · Corros. Sci. · 2006 · 48 · 420210.1016/j.corsci.2006.02.007 ↗
18. Buchheit · Electrochim. Acta · 2010 · 55 · 785310.1016/j.electacta.2010.04.046 ↗
19. DeRose · Corros. Sci. · 2012 · 55 · 31310.1016/j.corsci.2011.10.035 ↗
20. Rynders · J. Electrochem. Soc. · 1994 · 141 · 143910.1149/1.2054943 ↗
21. Chen · Corrosion · 1996 · 52 · 810.5006/1.3292099 ↗
22. Park · J. Electrochem. Soc. · 1999 · 146 · 51710.1149/1.1391637 ↗
23. Seri · Corros. Sci. · 1994 · 36 · 178910.1016/0010-938X(94)90132-5 ↗
24. Seri · Corros. Sci. · 1990 · 30 · 112110.1016/0010-938X(90)90060-I ↗
25. Nisancioglu · J. Electrochem. Soc. · 1981 · 128 · 152310.1149/1.2127675 ↗
26. Birbilis · J. Electrochem. Soc. · 2008 · 155 · C11710.1149/1.2829897 ↗
27. Thompson · Mater. Sci. Forum · 1996 · 217–222 · 9510.4028/www.scientific.net/MSF.217-222.95 ↗
28. Buchheit · J. Electrochem. Soc. · 1995 · 142 · 399410.1149/1.2048447 ↗
29. Luo · Corros. Sci. · 2012 · 61 · 3510.1016/j.corsci.2012.04.005 ↗
30. Mazurkiewicz · Corros. Sci. · 1983 · 23 · 69710.1016/0010-938X(83)90034-3 ↗
31. Scully · Met. Trans. · 1992 · 23A · 264110.1007/BF02658068 ↗
32. Seyeux · J. Electrochem. Soc. · 2011 · 158 · C16510.1149/1.3568944 ↗
33. Buchler · Corros. Sci. · 2000 · 42 · 166110.1016/S0010-938X(00)00020-2 ↗
34. Ilevbare · J. Electrochem. Soc. · 2004 · 151 · B45310.1149/1.1764780 ↗
35. Schneider · J. Electrochem. Soc. · 2004 · 151 · B46510.1149/1.1764781 ↗
36. Xiao · Electrochim. Acta · 2011 · 56 · 563010.1016/j.electacta.2011.04.019 ↗
37. Szklarska-Śmiałowska · Corros. Sci. · 1999 · 41 · 174310.1016/S0010-938X(99)00012-8 ↗
38. Ambat · J. Appl. Electrochem. · 1994 · 24 · 91110.1007/BF00348781 ↗
39. Liu · Corros. Sci · 2004 · 46 · 40510.1016/S0010-938X(03)00149-5 ↗
40. Liu · Corros. Sci. · 2006 · 48 · 330910.1016/j.corsci.2005.12.003 ↗
41. Krawiec · J. Solid State Electrochem. · 2009 · 13 · 118110.1007/s10008-008-0638-8 ↗
42. Trdan · Corros. Sci. · 2012 · 59 · 32410.1016/j.corsci.2012.03.019 ↗
43. Amar · Corros. Sci. · 2011 · 53 · 321510.1016/j.corsci.2011.05.066 ↗
44. Hatamleh · Corros. Sci. · 2009 · 51 · 13510.1016/j.corsci.2008.09.031 ↗
45. Liu · Corros. Sci. · 2009 · 51 · 146010.1016/j.corsci.2009.03.035 ↗
46. Suter · J. Electrochem. Soc. · 2001 · 148 · B3610.1149/1.1344530 ↗
47. Bohni · Surf. Coat. Technol. · 2000 · 130 · 8010.1016/S0257-8972(00)00681-2 ↗
48. Baumgartner · Corros. Sci. · 1989 · 29 · 36310.1016/0010-938X(89)90041-3 ↗
49. A. Siewiorek, J. Banas, Corrosion of aluminum monocrystals in organic solutions, in: Proceedings of EUROCORR, 2003, Budapest, Hungary.
50. Banaś · J. Solid State Electrochem. · 2009 · 13 · 166910.1007/s10008-008-0649-5 ↗
51. Kempf · Philos. Mag. · 2007 · 87 · 137910.1080/14786430600928527 ↗
52. Vignal · J. Electrochem. Soc. · 2006 · 153 · B35210.1149/1.2218762 ↗