Comparison of the isothermal and cyclic oxidation behavior of Cr and Mo containing γ-TiAlNb alloys
Source abstract
Abstract
Abstract The isothermal and cyclic oxidation behavior of γ-Ti-46.5Al-5Nb-0.3B alloys containing 2 at.% Cr, 2 at.% Mo, 1 at.% each of Cr and Mo, is compared at 900 °C until 500 h. The alloys exhibit parabolic oxidation, similar isothermal oxidation rates, but contrasting cyclic oxidation characteristics. The Mo-containing alloys form more Al2O3, exhibit extensive oxide spallation and weight loss; and vice-versa is observed for the Cr-rich alloy. The residual stresses, strains and spallation mechanisms in the multi-layered oxide scale are analyzed. Higher Al2O3 formation, high compressive stress (∼1 GPa) and strain (> 0.2 %) induce early delamination of oxide scale and weight degradation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · MXene and MAX Phase Materials · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (71)
Show source-provided references
1. Structural aluminides for elevated temperature applications, edited, the minerals
2. Titanium aluminides for aerospace applications, superalloys 1992
3. Appel · 2011
4. TiAl compounds for structural applications, structural intermetallics
5. Alloying mechanisms of beta stabilizers in TiAl alloys10.1007/s11661-001-0136-4 ↗
6. Microstructural evolution and mechanical properties of a forged gamma titanium aluminide alloy10.1016/0956-7151(92)90411-7 ↗
7. Ordered intermetallic alloys, part III: gamma titanium aluminides10.1007/BF03220745 ↗
8. Strength and ductility in TiAl alloys10.1016/S0966-9795(98)00037-5 ↗
9. Huang · 1991 · 105
10. Toughening mechanisms in titanium aluminides10.1007/BF02656627 ↗
11. Rate and environmental effects on fracture of a two-phase TiAl-alloy10.1007/BF02669609 ↗
12. Notch fracture in γ-titanium aluminides Metall10.1007/BF02595639 ↗
13. High-temperature structural intermetallics10.1016/S1359-6454(99)00301-8 ↗
14. Progress in the understanding of gamma titanium aluminides10.1007/BF03221103 ↗
15. High temperature oxidation behavior of TiAl-Cr-Nb-Mo alloys10.1016/j.intermet.2013.07.023 ↗
16. Alloy design for improvement of ductility and workability of alloys based on intermetallic compound TiAl
17. Solidification structures of Ti-Al-Cr alloys10.1016/S0966-9795(98)00067-3 ↗
18. Microstructure and transformation characteristics of a TiAlNb alloy with Cr and Mo addition10.1590/S1516-14392011005000095 ↗
19. Oxidation behavior of gamma titanium aluminides with or without protective coatings10.1179/1743280414Y.0000000034 ↗
20. Isothermal oxidation behavior of powder metallurgy beta gamma TiAl-2Nb-2Mo alloy10.1016/j.intermet.2011.05.027 ↗
21. Oxidation behavior of gamma alloys designed for high temperature applications10.1016/j.intermet.2004.12.007 ↗
22. Oxidation behavior of γ-TiAl based alloys at 900°C in air10.1080/09603409.2016.1164523 ↗
23. The high-temperature oxidation behavior of Ti-47Al-2Cr-2Si and Ti-48Al-2Cr-2Nb compared with Ti-48Al-2Cr10.1016/S0966-9795(97)00025-3 ↗
24. Thermodynamic aspects of TiAl and TiSi2oxidation: the Al-Ti-O and Si-Ti-O phase diagrams10.1007/BF00666500 ↗
25. Oxidation of intermetallics-Japanese activity10.1002/maco.19970480102 ↗
26. Environmental embrittlement of a third generation γ TiAl alloy10.1016/j.intermet.2011.10.006 ↗
27. The oxidation and protection of gamma titanium aluminides10.1007/BF03223244 ↗
28. Effect of Nb on the high temperature oxidation of Ti-(0-50 at.%)Al10.1016/S1359-6462(02)00042-8 ↗
29. Effects of Nb addition on oxidation behavior of TiAl10.1016/0966-9795(95)94254-C ↗
30. Role of W, Mo, Nb and Si on oxidation of TiAl in air at high temperatures
31. The influence of ternary element addition on the oxidation behavior of TiAl intermetallic compound in high temperature air10.1016/0010-938X(93)90313-6 ↗
32. The effect of various ternary additives on the oxidation behavior of TiAl in high temperature air10.1007/BF01046826 ↗
33. Oxidation behavior of a Ti–46Al–1Mo 0.2Si alloy: the effect of Mo addition and alloy microstructure10.1016/S0921-5093(00)00755-3 ↗
34. Effect of Mo addition on oxidation behavior of TiAl intermetallic compound
35. Effect of Cr on microstructure and oxidation behavior of TiAl-based alloy with high Nb10.1007/s41230-018-7020-y ↗
36. The effect of Cr addition on the binary TiAl-base alloys10.1007/BF02851355 ↗
37. High-temperature oxidation behavior of multi-phase Mo-containing γ-TiAl-based alloys10.1016/j.intermet.2014.04.010 ↗
38. The microstructure, mechanical properties, and oxidation behavior of beta gamma TiAl alloy with excellent hot workability10.1016/j.msea.2017.06.025 ↗
39. Alloy design concepts for refined gamma titanium aluminide based alloys10.1016/j.intermet.2006.05.003 ↗
40. Effects of major alloying additions on the microstructure and mechanical properties of γ-TiAl10.1016/S0966-9795(98)00016-8 ↗
41. Effect of Fe and Mo additions on microstructure and mechanical properties of TiAl intermetallics10.1016/S1003-6326(11)61208-9 ↗
42. Influence of Mo content on microstructure and mechanical properties of β-containing TiAl alloy10.1016/S1003-6326(17)60094-3 ↗
43. Microstructural design and mechanical properties of a cast and heat-treated intermetallic multi-phase γ-TiAl based alloy10.1016/j.intermet.2013.09.010 ↗
44. Fundamentals of TiAl oxidation - a critical review
45. Mechanism of isothermal oxidation of the intermetallic TiAl and of TiAl alloys10.1007/BF00665663 ↗
46. TEM investigations of the early stages of TiA1 oxidation10.1007/BF01050799 ↗
47. Diffusion in the Ti-Al System10.1016/S1359-6454(99)00400-0 ↗
48. Kofstad · 1988
49. The oxidation behavior of Ti-46.5Al-5Nb at 900°C10.1016/j.intermet.2006.09.010 ↗
50. Microstructural evolution and high-temperature oxidation mechanisms of a titanium aluminide based alloy10.1016/j.actamat.2018.02.013 ↗
51. Kofstad · 1966 · 100
52. Oxygen diffusion in rutile from 750 to 1000⁰C and 0.1 to 1000 MPa10.2138/am-1998-7-803 ↗
53. Oxygen and aluminum diffusion in α-Al2O3: how much do we really understand?10.1016/j.jeurceramsoc.2007.12.020 ↗
54. Revised effective Ionic radii and systematic studies of interatomic distances in halides and chalcogenides10.1107/S0567739476001551 ↗
55. Residual stress and cracking in thin PVD coatings10.1016/S0042-207X(01)00327-X ↗
56. Mechanical integrity in PVD coatings due to the presence of residual stresses10.1016/S0040-6090(01)01043-4 ↗
57. The thermomechanical integrity of thin films and multilayers10.1016/0956-7151(94)00444-M ↗
58. An analytical model for predicting thermal residual stresses in multilayer coating systems10.1016/j.tsf.2005.04.027 ↗
59. 2019 · 510
60. https://www.azom.com/properties.aspx?ArticleID=1179.
61. 2019 · 538
62. 2019 · 509
63. https://www.azom.com/properties.aspx?ArticleID=52.
64. https://accuratus.com/alumox.html.
65. 2019
66. Leyens · 2003
67. Pierson · 1996
68. Hardness and elastic modulus of TiN based on continuous indentation technique and new correlation10.1116/1.577270 ↗
69. Hutchinson · 1996
70. Crack deflection at an interface between dissimilar elastic materials: role of residual stresses10.1016/0020-7683(94)90025-6 ↗
71. Crack deflection at an interface between dissimilar elastic materials10.1016/0020-7683(89)90021-8 ↗