journal article·2021-09

Hot corrosion-creep interaction in IN718 under simulated marine environment: Introducing strain-associated-time (SAT) plots for comprehensive understanding

Venkateswara Rao Mannava, N.T.B.N. Koundinya, SambasivaRao A., Neeta Paulose, Kamaraj M., Ravi Sankar Kottada

Corrosion Science· Volume 190
Publisher page

Abstract

Abstract Creep-rupture behaviour of IN718 with deposit of 87.5 wt.%Na2SO4+5 wt.%NaCl+7.5 wt.%NaVO3 (3SM) in the stress range of 550–850 MPa at 650 °C is investigated. 3SM shortens the creep-rupture time by ≈70–90 %. Comprehensive microstructural analysis suggests that oxygen-induced-dynamic- embrittlement, sulphidation followed by oxidation, and vanadic-hot corrosion operate during creep. Creep-hot corrosion interaction influence on rupture strain is explained by introducing strain-associated-time (SAT) and Δte plots, for the first time. These plots accompanied by detailed microstructural examination demonstrate that deleterious influence of 3SM increases with decreasing stress. Further, SAT plots and EPMA analysis confirm that oxygen-induced-dynamic-embrittlement commences from ∼9% strain under 3SM at 550 MPa.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · High Temperature Alloys and Creep · Fatigue and fracture mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (65)

Show source-provided references
1. Nickel base superalloys: current status and potential
2. Physical metallurgy of alloy 718
3. The precipitation of Ni3Nb Phases in a Ni-Fe-Cr-Nb alloy10.1007/BF03037800 ↗
4. Coarsening behaviour of γ″ and γ′ particles in Inconel alloy 71810.1179/030634582790427118 ↗
5. Delta phase in Inconel 718: mechanical properties and forging process requirements10.7449/1994/Superalloys_1994_281_291 ↗
6. Delta phase precipitation in Inconel 71810.1016/j.matchar.2004.07.004 ↗
7. Carbide precipitation in nickel base superalloys 718 and 625 and their effect on mechanical properties10.7449/1997/Superalloys_1997_367_378 ↗
8. The precipitation of primary carbides in alloy 71810.7449/1994/Superalloys_1994_65_78 ↗
9. Morphology of γ′ and γ″ precipitates and thermal stability of Inconel 718 type alloys10.1007/BF02649604 ↗
10. Steady-state creep deformation of superalloy Inconel71810.1016/0025-5416(87)90246-1 ↗
11. A study of back stress during creep deformation of a superalloy Inconel 71810.1016/0025-5416(87)90467-8 ↗
12. Effect of particle size on the creep rate of superalloy Inconel 71810.1016/0025-5416(87)90264-3 ↗
13. Effect of grain size on the steady-state creep rate of Inconel 71810.1016/S0036-9748(88)80344-2 ↗
14. Steady-state creep rate equation of Inconel 718 superalloy
15. Grain boundary dependent creep behavior of Inconel 71810.1179/cmq.1993.32.4.363 ↗
16. Stress rupture property-microstructure correlation in hot-rolled superalloy 71810.1016/1044-5803(95)80108-1 ↗
17. Preferential coarsening of γ″ precipitates in Inconel 718 during creep
18. Dependence of creep fracture behavior of IN718 on grain boundary precipitates10.1016/S1359-6454(96)00399-0 ↗
19. Creep properties of phosphorus +boron-modified alloy 71810.1016/S1359-6462(97)00476-4 ↗
20. Beneficial effect of phosphorus on the creep the behaviour of Inconel 71810.1016/S1359-6462(99)00158-X ↗
21. Creep rupture of alloy 718 after thermal aging10.1007/s11837-000-0114-0 ↗
22. Compensation effect in creep of conventional polycrystalline alloy 71810.1016/S1359-6462(00)00314-6 ↗
23. Aging effects on the microstructure and creep behaviour of Inconel 718 superalloy10.1016/j.msea.2008.04.097 ↗
24. Effect of serrated grain boundaries on the creep property of Inconel718 superalloy10.1016/j.msea.2011.10.014 ↗
25. Effect of hot corrosion on the mechanical performances of superalloys and coating systems10.1016/0010-938X(93)90331-A ↗
26. Hot corrosion in gas turbine components10.1016/S1350-6307(00)00035-2 ↗
27. Hot corrosion of metals and alloys10.1007/s11085-011-9254-6 ↗
28. Kofstad · 1988
29. Lai · 2007
30. Impurity deposits in gas turbines from fuels containing sodium and vanadium10.1149/1.2123941 ↗
31. Corrosion resistance of superalloys in temperature range of 800–1300 °F10.1007/BF02833378 ↗
32. The effect of SO2 and NaCl on high-temperature hot corrosion10.1149/1.2131463 ↗
33. High-temperature behaviour of superalloys exposed to sodium chloride: I. Mechanical properties10.1007/BF02649631 ↗
34. The high temperature behaviour of superalloys exposed to sodium chloride: II. Corrosion10.1007/BF02649632 ↗
35. Influence of alloying elements on hot corrosion of superalloys and coatings: the necessity of smart coatings for gas turbine engines10.1179/026708303225009382 ↗
36. Hot corrosion behaviour of superalloy IN718 at 550 and 650 °C10.1007/s11665-013-0532-0 ↗
37. Hot corrosion studies on Ni-base superalloy at 650 °C under marine-like environment conditions using three salt mixture (Na2SO4+NaCl+NaVO3)10.1016/j.corsci.2016.01.008 ↗
38. Influence of two different salt mixture combinations of Na2SO4-NaCl-NaVO3 on hot corrosion behaviour of Ni-base superalloy at 800 °C10.1007/s11665-019-3866-4 ↗
39. Hot corrosion behaviour and near-surface microstructure of a low-temperature high-activity Cr-aluminide coating on Inconel 738LC exposed to Na2SO4, Na2SO4 + V2O5 and Na2SO4 + V2O5 + NaCl at 900 °C10.1016/j.corsci.2017.09.004 ↗
40. Balsone · 1985
41. The effect of hot corrosion on creep and fracture behaviour of cast nickel-based superalloy IN738LC
42. Influence of hot corrosion on the creep strength of the nickel-base superalloy10.1016/0025-5416(84)90262-3 ↗
43. Effect of creep or low cycle fatigue on the oxidation or hot corrosion behaviour of nickel-base superalloys10.1016/0025-5416(87)90085-1 ↗
44. Effect of environmental factors on the creep rupture properties of a Nickel base superalloys subjected to hot corrosion10.2320/matertrans1960.29.26 ↗
45. Vanadic hot corrosion - creep interaction of superni - C276 in the temperature range 650-750 °C10.1515/HTMP.1994.13.4.277 ↗
46. Creep rupture of Nimonic-90 under salt-induced high temperature corrosion
47. Influence of saline environment on creep rupture life of Nimonic-263 for marine turbine application10.1016/j.msea.2012.12.081 ↗
48. Analysis of combined static load and low temperature hot corrosion induced cracking in CMSX-4 at 550 °C
49. Stress corrosion of Ni-based superalloys10.1080/09603409.2017.1392414 ↗
50. High-temperature hot-corrosion effects on the creep–fatigue behavior of a directionally solidified nickel-based superalloy: mechanism and lifetime prediction10.1177/1056789519891765 ↗
51. Interaction of hot corrosion and creep in Alloy 61710.1016/j.engfailanal.2016.03.012 ↗
52. An investigation of oxidation/hot corrosion-creep interaction at 800 °C in a Ni-base superalloy coated with salt mixture deposits of Na2SO4-NaCl-NaVO310.1016/j.corsci.2018.11.029 ↗
53. An innovative spraying setup to obtain uniform salt(s) mixture deposition to investigate hot corrosion10.1063/1.4941779 ↗
54. Effects of the environment on the crack propagation behavior of IN718 in the temperature range of the dynamic embrittlement10.1520/JAI103569 ↗
55. Oxygen-induced intergranular cracking of a Ni-base alloy elevated temperatures-an example of dynamic embrittlement10.1016/S1359-6454(01)00005-2 ↗
56. Dynamic embrittlement in alloy 71810.7449/2001/Superalloys_2001_701_707 ↗
57. Oxygen-induced intergranular fracture of the nickel-base alloy IN718 during mechanical loading at high temperature10.1590/S1516-14392004000100006 ↗
58. Surface enrichment of niobium on Inconel 718 (100) single crystals10.1016/0169-4332(94)00152-9 ↗
59. High temperature oxidation of Nb, NbC and Ni3Nb and oxygen enhanced crack growth10.1016/S1359-6462(99)00336-X ↗
60. Oxidation characteristics and thermal expansion of IN718 from 300-1273K10.7449/1997/Superalloys_1997_689_693 ↗
61. The influence of oxidation on the steady state creep of iron at 823–1023K10.1080/01418618108239559 ↗
62. Role of metal-oxide interfacial reactions on the interactions between oxidation and deformation10.1016/S1359-6462(98)00202-4 ↗
63. Stresses and decohesion of oxides10.1179/mst.1988.4.5.407 ↗
64. Hot corrosion of materials: a fluxing mechanism?10.1016/S0010-938X(01)00057-9 ↗
65. the hot corrosion of Ni-based ternary alloys and superalloys for application in gas turbines employing residual fuels10.1016/0010-938X(87)90093-X ↗