A HfB 2-SiC skeleton was designed on SiC-coated C/C composites using hollow SiO 2 microspheres as sacrificial templates, which was densified by SiC via chemical vapor infiltration to fabricate a dense SiC-HfB 2 oxidation protective coating. In this way, the uniform distribution of HfB 2 in the coating was realized. Cracks in the SiC inner coating were covered by the SiC-HfB 2 coating; Hf-oxides improved the stability and inhibited the volatilization of SiO 2 in the compound glass layer. Therefore, the coating can protect C/C composites against oxidation for 59 h at 1473 K, 503 h at 1773 K, and 166 h at 1973 K.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Recent progress in 1D nanostructures reinforced carbon/carbon composites10.1002/adfm.202204965 ↗
2. Micro/nano multiscale reinforcing strategies toward extreme high-temperature applications: take carbon/carbon composites and their coatings as the examples10.1016/j.jmst.2021.03.076 ↗
3. Interface graphitization of carbon-carbon composites by nanoindentation10.1016/j.carbon.2019.05.038 ↗
4. Oxidation resistance and mechanical properties of HfC nanowire-toughened ultra-high temperature ceramic coating for SiC-coated C/C composites10.1016/j.apsusc.2015.11.097 ↗
5. Effect of microstructure on the ablation behavior and mechanical properties of CVD-HfC coating
6. Advances in antioxidation coating materials for carbon/carbon composites10.1016/j.jallcom.2021.161143 ↗
7. Investigation on the ablation performance and mechanism of HfC coating modified with TaC10.1016/j.corsci.2020.108649 ↗
8. A dense ZrB2-SiC-Si/SiC-Si coating to protect carbon/carbon composites against oxidation at 1773 K and 1973 K10.1016/j.corsci.2021.109331 ↗
9. Microstructure and oxidation behavior of C/C-ZrB2-SiC composites coated with SiC coating at high temperature10.1016/j.corsci.2015.08.015 ↗
10. Preparation of ZrC nano-particles reinforced amorphous carbon composite coating by atmospheric pressure chemical vapor deposition10.1016/j.apsusc.2009.03.045 ↗
11. A novel gradient SiC-ZrB2-MoSi2 coating for SiC coated C/C composites by supersonic plasma spraying10.1016/j.surfcoat.2017.01.019 ↗
12. Silicon carbide coating to protect carbon/carbon composites against oxidation10.1016/j.scriptamat.2004.12.029 ↗
13. Siliconization elimination for SiC coated C/C composites by a pyrolytic carbon coating and the consequent improvement of the mechanical property and oxidation resistances10.1016/j.jeurceramsoc.2021.04.008 ↗
14. SiC-Si coating with micro-pores to protect carbon/carbon composites against oxidation10.1016/j.jeurceramsoc.2020.08.045 ↗
15. Oxidation protective SiC-Si coating for carbon/carbon composites by gaseous silicon infiltration and pack cementation: a comparative investigation10.1016/j.jeurceramsoc.2020.07.040 ↗
16. Comparison of the oxidation behaviors of SiC coatings on C/C composites prepared by pack cementation and chemical vapor deposition10.1016/j.surfcoat.2016.05.071 ↗
17. Effect of La2O3 on the oxidation resistance of SiC ceramic at 1973 K: experimental and theoretical study10.1111/jace.16708 ↗
18. Effect of Zr doping on the high-temperature stability of SiO2 glass10.1016/j.commatsci.2018.01.051 ↗
19. Evolution behavior of rare-earth yttria modified silicide oxidation-resistant coating at 1700 ℃10.1016/j.jeurceramsoc.2020.06.012 ↗
20. Effect of the ZrB2 content on the oxygen blocking ability of ZrB2-SiC coating at 1973 K10.1016/j.jeurceramsoc.2020.10.036 ↗
21. In-situ formation of SiC, ZrB2-SiC and ZrB2-SiC-B4C-YAG coatings for high temperature oxidation protection of C/C composites10.1016/j.corsci.2018.07.002 ↗
22. Gradient HfB2-SiC multilayer oxidation resistant coating for C/C composites10.1016/j.ceramint.2018.08.104 ↗
23. The effect of HfB2 content on the oxidation and thermal shock resistance of SiC coating10.1016/j.surfcoat.2018.02.029 ↗
24. The oxidation resistance of two-temperature synthetic HfB2-SiC coating for the SiC coated C/C composites10.1016/j.surfcoat.2018.02.029 ↗
25. Ultrahigh temperature ceramic HfB2-SiC coating by liquid phase sintering method to protect carbon materials from oxidation10.1016/j.matchemphys.2018.07.018 ↗
26. Dynamic oxidation protective behaviors and mechanisms of HfB2-20wt%SiC composite coating for carbon materials10.1016/j.jeurceramsoc.2019.01.033 ↗
27. Microstructure evolution of in-situ SiC-HfB2-Si ternary coating and its corrosion behaviors at ultra-high temperatures10.1016/j.jeurceramsoc.2021.05.058 ↗
28. Microstructure and oxidation resistance of Si-Mo-B coating for C/SiC coated carbon/carbon composites10.1016/j.corsci.2013.03.015 ↗
29. Oxidation of ß-SiC at high temperature in Ar/O2, Ar/CO2, Ar/H2O gas mixtures: active/passive transition10.1016/j.jeurceramsoc.2018.04.036 ↗
30. Constructing self-healing ZrSi2-MoSi2 coating for C/C composites with enhanced oxidation protective ability10.1016/j.surfcoat.2018.05.002 ↗
31. Oxidation behavior of fine-grained SiC-B4C/C composites up to 1400 ℃10.1016/S0008-6223(02)00345-7 ↗
32. Formation and oxidation resistance of the coating formed on carbon material composed of B4C-SiC powders10.1016/0008-6223(94)00164-U ↗
33. Enhancing anti-oxidation and thermal-radiation performance of the repaired borosilicate glass coating on C/C composites by Sm-doping
34. a Joining of sintered SiC ceramics at a lower temperature using borosilicate glass with laser cladding Si modification layer10.1016/j.jeurceramsoc.2020.11.044 ↗
35. HfB2-SiC-MoSi2 oxidation resistance coating fabricated through in-situ synthesis for SiC coated C/C composites10.1016/j.jallcom.2017.06.008 ↗
36. Oxidation behavior of SiC-HfB2-Si coating on C/C composites prepared by slurry dipping combined with gaseous Si infiltration10.1016/j.surfcoat.2020.125335 ↗
37. Investigation on the oxidation and ablation behaviors of HfB2-SiC-Si/SiC-Si coatings for carbon/carbon composites10.1016/j.corsci.2021.109638 ↗
38. Preparation of a double layer SiC coating and its oxidation resistance at 1773 K10.1016/j.corsci.2014.06.024 ↗
39. coating for ultralong-time anti-oxidation at 1973 K10.1016/j.corsci.2019.108119 ↗
40. Oxidation protective silicon carbide coating for C/SiC composite modified by a chromium silicide-chromium carbide outer layer10.1016/j.msea.2015.07.081 ↗
41. Oxidation behavior of plasma-sprayed MoSi2-Yb2O3 composite coating at 1700 °C10.1016/j.ceramint.2019.12.216 ↗
42. Oxidation behaviour of ZrB2-SiC (Al/Y) ceramics at 1700°C10.1016/j.jeurceramsoc.2016.02.037 ↗
43. Oxidation behavior of ZrB2-SiC-ZrC at 1700°C10.1016/j.jeurceramsoc.2016.10.034 ↗
44. Oxidation transitions for SiC part II. Passive-to-active transitions10.1111/jace.12104 ↗
45. SiC/SiC-ZrSi2 coating with micro-pore to protect C/C composites against oxidation for long-life service at high temperatures10.1016/j.corsci.2021.109780 ↗
46. Hafnium silicate formation during the reaction of β-cristobalite SiO2 and monoclinic HfO210.1111/jace.17274 ↗
47. High-temperature stability and oxidation behavior of SiOC/HfO2 ceramic nanocomposite in air10.1016/j.corsci.2020.108866 ↗
48. An oxidation and ablation protective WSi2-HfB2-SiC coating for SiC coated C/C composites at 1973 K and above10.1016/j.corsci.2020.108964 ↗
49. Oxidation protection and behavior of in-situ zirconium diboride-silicon carbide coating for carbon/carbon composites10.1016/j.jallcom.2015.04.215 ↗