journal article·2018-07

Performance of an FeCrAl alloy in a high-temperature CO2 environment

I.E. McCarroll, A. La Fontaine, T.D. Nguyen, A.F. Smith, J. Zhang, D.J. Young, J.M. Cairney

Corrosion Science· Volume 139
Publisher page

Abstract

Abstract Supercritical CO2 has been suggested as a candidate heat transfer fluid in concentrated solar power plants, but its implementation requires cost-effective materials that can resist corrosion in high-temperature C-rich environments. Alumina-forming alloys are known to resist high-temperature corrosion in oxygen, but little is known about their performance in CO2. Here, Kanthal APM was reacted in flowing CO2 at 1100 °C under isothermal and cyclic conditions. Scanning electron microscopy and atom probe tomography showed the structure to be dense, adherent and free of grain boundary carbon. The alloy performed well under these conditions providing a protective, carbon free, alumina scale.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Materials Characterization Techniques · High-Temperature Coating Behaviors · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Enabling greater penetration of solar power via the use of CSP with thermal energy storage
2. Thermodynamic study of advanced supercritical carbon dioxide power cycles for concentrating solar power systems10.1115/1.4024030 ↗
3. Review of heat transfer fluids in tube-receivers used in concentrating solar thermal systems: properties and heat transfer coefficients10.1016/j.rser.2015.10.059 ↗
4. Supercritical CO2 Brayton cycles for solar-thermal energy10.1016/j.apenergy.2013.06.020 ↗
5. A qualitative thermo-fluid-dynamic analysis of a CO2 solar pipe receiver10.1016/j.solener.2011.12.023 ↗
6. Scientific assessment in support of the materials roadmap enabling low carbon energy technologies: concentrating solar power technologies
7. Martensitic transformation in an intergranular corrosion area of austenitic stainless steel during thermal cycling10.1016/j.corsci.2014.04.048 ↗
8. Chromium depletion and martensite formation at grain boundaries in sensitised austenitic stainless steel10.1016/0001-6160(86)90091-X ↗
9. Decomposition of austenite in austenitic stainless steels10.2355/isijinternational.42.325 ↗
10. Penetration of protective chromia scales by carbon10.1016/j.scriptamat.2014.01.009 ↗
11. Corrosion by carbonaceous gases, carburization and metal dusting, and methods of prevention10.1179/mht.2000.063 ↗
12. Early stages of the oxidation of A FeCrAlRE alloy (Kanthal AF) at 900 °C: a detailed microstructural investigation10.1016/j.corsci.2008.05.019 ↗
13. First three-dimensional atomic resolution investigation of thermally grown oxide on a FeCrAl alloy
14. Atom probe tomography of thermally grown oxide scale on FeCrAl10.1016/j.ultramic.2013.02.004 ↗
15. The effect of water vapor on the initial stages of oxidation of the FeCrAl alloy kanthal AF at 900°C10.1007/s11085-007-9055-0 ↗
16. Oxidation of alumina formers at 1173 K: effect of yttrium ion implantation and yttrium alloying addition10.1016/S0010-938X(02)00254-8 ↗
17. Hot corrosion behaviour and its mechanism of a new alumina-forming austenitic stainless steel in molten sodium sulphate10.1016/j.corsci.2013.08.003 ↗
18. Initial oxidation of Fe–Al and Fe–Cr–Al alloys: Cr as an alumina booster10.1007/s11085-011-9258-2 ↗
19. Ionic segregation on grain boundaries in thermally grown alumina scales10.3184/096034012X13343209167745 ↗
20. 2011
21. Alumina scale formation: a new perspective
22. On the growth of Al2O3 scales10.1016/j.actamat.2013.07.024 ↗
23. Microstructural evidence for counter-diffusion of aluminum and oxygen during the growth of alumina scales10.1179/mht.2003.030 ↗
24. The prediction of breakaway oxidation for alumina forming ODS alloys using oxidation diagrams10.1002/maco.19940450404 ↗
25. Characterization of the breakaway Al content in alumina-forming alloys10.1179/mht.2004.021 ↗
26. The reactive element effect in commercial ODS FeCrAl alloys10.1080/09603409.1995.11689496 ↗
27. Quantification of carbon contamination under electron beam irradiation in a scanning transmission electron microscope and its suppression by plasma cleaning
28. Probing the improbable: imaging c atoms in alumina10.1016/S1369-7021(10)70184-X ↗
29. Field-ion specimen preparation using focused ion-beam milling10.1016/S0304-3991(99)00055-8 ↗
30. A simple approach to atom probe sample preparation by using shadow masks10.1016/j.ultramic.2015.09.005 ↗
31. Focused ion-beam milling for field-ion specimen preparation: preliminary investigations10.1016/S0304-3991(98)00058-8 ↗
32. Gault · 2012
33. Oxidation behaviour of Fe-Cr-Al alloys during resistance and furnace heating10.1002/maco.200503897 ↗
34. The oxidation mechanism of θ-Al2O3 scales10.1016/0167-2738(95)00013-V ↗
35. New atom probe approaches to studying segregation in nanocrystalline materials10.1016/j.ultramic.2012.12.013 ↗
36. Challenges associated with the characterisation of nanocrystalline materials using atom probe tomography10.4028/www.scientific.net/MSF.654-656.2366 ↗
37. The field ionization characteristics of individual atomic planes10.1016/0039-6028(71)90031-8 ↗
38. A reproducible method for damage-free site-specific preparation of atom probe tips from interfaces10.1002/jemt.21081 ↗
39. Factors affecting aluminum depletion during cyclic oxidation of Fe-base alumina-forming alloys10.3184/096034009X464401 ↗
40. Effect of cycle frequency on high-temperature oxidation behavior of alumina-forming alloys10.1023/A:1016064524521 ↗
41. Effect of H2O and CO2 on the oxidation behavior and durability at high temperature of ODS-FeCrAl10.1007/s11085-013-9382-2 ↗
42. Young · 2016
43. Microstructure, adhesion and growth kinetics of protective scales on metals and alloys10.1007/BF00656571 ↗
44. The relationship between oxide grain morphology and growth mechanisms for Fe-Cr-Al and Fe-Cr-Al-Y alloys10.1149/1.2129170 ↗
45. FEG-SEM examination of alumina scales formed on FeCrAl alloys10.3184/096034005782744001 ↗
46. Oxidation kinetics of Y-doped FeCrAl-alloys in low and high pO2 gases10.1002/maco.200905432 ↗
47. Quantification of aluminum outward diffusion during oxidation of FeCrAl alloys10.1007/s11085-005-4391-4 ↗
48. Effect of environment on the scale formed on oxide dispersion strengthened FeCrAl at 1050°C and 1100°C10.3184/096034012X13317275660176 ↗
49. The formation of aluminum oxide scales on high-temperature alloys10.1007/BF00666913 ↗
50. Residual stresses in alumina scales. Experiments, modeling, and stress-relaxation phenomena10.1023/A:1004530729859 ↗
51. High-temperature oxidation behavior of iron-chromium-aluminum alloys10.1023/A:1004682316408 ↗