Improved corrosion resistance of Mg–8Sn–1Zn–1Al alloy subjected to low-temperature indirect extrusion

Soo-Min Baek, Jeong Su Kang, Jong Chan Kim, Beomcheol Kim, Hyung-Joon Shin, Sung Soo Park

Corrosion Science· Volume 141

Abstract

Abstract We report that the corrosion resistance of Mg–8Sn–1Zn–1Al alloy is significantly improved by the application of a low-temperature indirect extrusion process utilizing artificial cooling. It was found that the corrosion rates, measured by immersion tests in 0.6 M NaCl solution at 25 °C, are 27.5 and 246.7 mm y−1 for the alloys extruded with and without artificial cooling, respectively. The remarkably improved corrosion resistance is mainly attributed to the reduced nobility of cathodic Al5Fe2 particles, which results in retarded microgalvanic corrosion in the corrosive condition. Metallurgical factors affecting the electrochemical nobility of Al5Fe2 particles are discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Hydrogen Storage and Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Development of creep resistant die cast Mg–Sn–Al–Si alloy10.1016/j.msea.2005.09.022 ↗
2. Development of creep resistant Mg alloys10.4028/www.scientific.net/MSF.475-479.521 ↗
3. Compressive creep behavior of as-cast and aging-treated Mg–5wt% Sn alloys10.1016/j.msea.2008.05.006 ↗
4. The microstructure, tensile properties, and creep behavior of AZ91, AS52 and TAS652 alloy10.1016/j.jallcom.2009.12.145 ↗
5. The effect of precipitate state on the creep resistance of Mg–Sn alloys10.1016/j.scriptamat.2010.07.002 ↗
6. Enhanced age hardening response by the addition of Zn in Mg–Sn alloys10.1016/j.scriptamat.2006.04.005 ↗
7. Effect of double aging and microalloying on the age hardening behavior of a Mg–Sn–Zn alloy10.1016/j.msea.2010.05.010 ↗
8. Compositional optimization of Mg–Sn–Al alloys for higher age hardening response10.1016/j.msea.2012.12.041 ↗
9. Significant enhancement of the age-hardening response in Mg–10Sn–3Al–1Zn alloy by Na microalloying10.1016/j.scriptamat.2013.01.032 ↗
10. A high-strength Mg–Sn–Zn–Al alloy extruded at low temperature10.1016/j.scriptamat.2008.07.042 ↗
11. Heat-treatable Mg–Sn–Zn wrought alloy10.1016/j.scriptamat.2009.03.014 ↗
12. Microstructure and mechanical properties of binary Mg–Sn alloys subjected to indirect extrusion10.1016/j.msea.2010.03.031 ↗
13. Improving tensile properties of Mg–Sn–Zn magnesium alloy sheets using pre-tension and ageing treatment10.1016/j.jallcom.2017.11.220 ↗
14. Effect of extrusion conditions on microstructure and mechanical properties of microalloyed Mg–Sn–Al–1Zn alloys10.1016/j.msea.2013.09.050 ↗
15. Effect of cold pre-forging on the microstructure and mechanical properties of extruded Mg–8Sn–1Al–1Zn alloy10.1016/j.msea.2014.06.053 ↗
16. Strong and ductile heat-treatable Mg–Sn–Zn–Al wrought alloys10.1016/j.actamat.2015.06.060 ↗
17. Low-temperature superplasticity of extruded Mg–Sn–Al–Zn alloy10.1016/j.scriptamat.2011.04.005 ↗
18. Superplasticity and load relaxation behavior of extruded Mg–8Sn–3A–l1Zn alloy at 25010.1016/j.msea.2016.01.014 ↗
19. Influence of alloyed Al on the microstructure and corrosion properties of extruded Mg–8Sn–1Zn alloys10.1016/j.corsci.2015.03.007 ↗
20. Improved corrosion resistance of extruded Mg–8Sn–1Zn–1Al alloy by microalloying with Mn10.1016/j.scriptamat.2015.07.013 ↗
21. Understanding magnesium corrosion10.1002/adem.200310405 ↗
22. Grain refinement and reduced yield asymmetry of extruded Mg–5Sn–1Zn alloy by Al addition10.1016/j.jallcom.2015.11.133 ↗
23. Influences of the quantity of Mg2Sn phase on the corrosion behavior of Mg–7Sn magnesium alloy10.1016/j.electacta.2010.12.030 ↗
24. Influences of metallurgical factors on the corrosion behaviour of extruded binary Mg–Sn alloys10.1016/j.corsci.2014.01.035 ↗
25. Role of hydrogen evolution rate in determining the corrosion rate of extruded Mg–5Sn–(1–4 wt%)Zn alloys10.1016/j.corsci.2014.09.011 ↗
26. Corrosion mechanism applicable to biodegradable magnesium implants10.1016/j.mseb.2010.12.017 ↗
27. The Al-rich region of the Al–Fe–Mn alloy system10.1016/j.jallcom.2014.08.232 ↗
28. The stability of aluminum-manganese intermetallic phases under the microgalvanic coupling conditions anticipated in magnesium alloys10.1002/maco.201508349 ↗
29. Fundamentals and advances in magnesium alloy corrosion10.1016/j.pmatsci.2017.04.011 ↗
30. Corrosion and passivation of magnesium alloys10.1016/j.corsci.2016.05.041 ↗
31. Role of Sn in corrosion and passive behavior of extruded Mg–5wt% Sn alloy10.1016/j.corsci.2015.10.028 ↗
32. Limitations in the use of the potentiodynamic polarisation curves to investigate the effect of Zn on the corrosion behaviour of as-extruded Mg–Zn binary alloy10.1016/j.corsci.2013.06.027 ↗
33. Poisoning the corrosion of magnesium10.1016/j.elecom.2013.07.021 ↗
34. New insights into the corrosion of magnesium alloys – the role of aluminum10.1016/j.scriptamat.2016.01.008 ↗
35. Effect of alloyed Ca on the microstructure and corrosion properties of extruded AZ61 Mg alloy10.1016/j.corsci.2016.07.011 ↗
36. Role of alloyed Y in improving the corrosion resistance of extruded Mg–Al–Ca-based alloy10.1016/j.corsci.2017.01.022 ↗
37. Classification of bulk metallic glasses by atomic size difference, heat of mixing and period of constituent elements and its application to characterization of the main alloying element10.2320/matertrans.46.2817 ↗
38. Effect of alloying and impurity elements in magnesium alloy cast anodes10.5006/0010-9312-10.6.182 ↗
39. Effect of Mn additions on the corrosion behavior of mould-cast magnesium ASTM AZ9110.5006/1.3583151 ↗
40. Effect of impurity Fe on corrosion behavior of AM50 and AM60 magnesium alloys10.1016/j.corsci.2012.09.021 ↗
41. Self-diffusion in calcium and diffuse of barely soluble impurities in magnesium and calcium