journal article·2018-09Open access

Atmospheric chloride-induced stress corrosion cracking of laser engraved type 316L stainless steel

Benjamin Krawczyk, Paul Cook, Jeff Hobbs, Dirk L. Engelberg

Corrosion Science· Volume 142

Abstract

The influence of aqua blasting and laser engraving on the atmospheric chloride-induced stress corrosion cracking (AISCC) resistance of type 316L stainless steel has been elucidated by using MgCl2-laden droplet deposits as the test medium. Aqua blasted surfaces showed no evidence of AISCC. Laser engraving resulted in tensile residual stresses, and led to AISCC within two weeks of exposure, with crack growth rates similar to U-bend samples. Introducing compressive residual stresses via peening inhibited crack nucleation, whereas oxide layer removal of engraved surfaces had no effect on AISCC. Strategies to reduce the likelihood of AISCC of laser engraved components are discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Welding Techniques and Residual Stresses · Hydrogen embrittlement and corrosion behaviors in metals · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Effects of laser peening on stress corrosion cracking (SCC) of ANSI 304 austenitic stainless steel10.1016/j.corsci.2012.03.044 ↗
2. Effects of surface preparation on pitting resistance, residual stress, and stress corrosion cracking in austenitic stainless steels
3. Performance optimization of cold rolled type 316L stainless steel by sand blasting and surface linishing treatment10.1007/s11665-016-1943-5 ↗
4. Influence of peening on the corrosion properties of AISI 304 stainless steel10.1016/j.corsci.2009.08.008 ↗
5. Morphological and structural characterizations of different oxides formed on the stainless steel by Nd:YAG pulsed laser irradiation10.1016/j.apsusc.2008.04.020 ↗
6. Mechanical and electromechanical behavior of oxide coatings grown on stainless steel 304L by nanosecond pulsed laser irradiation10.1016/j.surfcoat.2013.09.013 ↗
7. Thermal effects of laser marking on microstructure and corrosion properties of stainless steel10.1364/AO.55.000D35 ↗
8. Effects of laser-induced oxidation on the corrosion resistance of AISI 304 stainless steel10.2351/1.4948726 ↗
9. Influence of femtosecond laser marking on the corrosion resistance of stainless steels10.1016/j.apsusc.2005.07.161 ↗
10. Environmental resistance of oxide tags fabricated on 304L stainless steel via nanosecond pulsed laser irradiation10.1016/j.surfcoat.2015.11.021 ↗
11. Nanosecond laser surface modification of AISI 304L stainless steel: influence the beam overlap on pitting corrosion resistance10.1016/j.apsusc.2013.09.086 ↗
12. Effect of microstructure and chemical composition on localized corrosion resistance of a AISI 304L stainless steel after nanopulsed-laser surface melting10.1016/j.apsusc.2015.08.015 ↗
13. Pitting corrosion of 304 stainless steel after laser surface melting in argon and nitrogen atmospheres10.1016/S0010-938X(00)00114-1 ↗
14. Effect of residual stress induced by pulsed-laser irradiation on initiation of chloride stress corrosion cracking in stainless steel10.1016/j.msea.2013.10.066 ↗
15. Residual stress. Part 1 – measurement techniques10.1179/026708301101509980 ↗
16. Corrosion behavior of aqua-blasted and laser-engraved type 316L stainless steel10.1007/s11665-017-3053-4 ↗
17. Superficial severe plastic deformation of 316 LVM stainless steel through grit blasting: effects on its microstructure and subsurface mechanical properties10.1016/j.surfcoat.2010.07.126 ↗
18. Corrosion reactivity of laser-peened steel surfaces10.1361/105994900770345520 ↗
19. Effect of chloride deposition on stress corrosion cracking of 316L stainless steel used for intermediate level radioactive waste containers10.1179/1743278210Y.0000000004 ↗
20. Assessing the risk of under-deposit chloride-induced stress corrosion cracking in austenitic stainless steel nuclear waste containers10.1179/1743278214Y.0000000204 ↗
21. Effect of aqua blasting, sandblasting and laser engraving on the corrosion resistance of type 316 stainless steel10.1007/s00501-016-0446-x ↗
22. Atmospheric pitting corrosion of 304L stainless steel: the role of highly concentrated chloride solutions10.1039/C4FD00246F ↗
23. Influence of shot peening pressure on stress corrosion susceptibility of 304 austenitic stainless steel10.4028/www.scientific.net/AMR.486.524 ↗
24. Stress corrosion cracking of austenitic stainless steel under compressive stress10.5006/1.3581957 ↗
25. Direct observations of stress corrosion crack tips of type 304 stainless steel in a boiling 42% MgCl2 solution10.5006/1.3577275 ↗
26. Mechanism of brittle fracture in a ductile 316 alloy during stress corrosion10.1016/0956-7151(90)90203-S ↗
27. Y. Mukai, M. Watanabe, M. Murata, Fractographic Observation of Stress-Corrosion Cracking of AISI 304 Stainless Steel in Boiling 42 Percent Magnesium-Chloride Solution, in: Fractography Fail. Anal., ASTM International, 100 Barr Harbor Drive, PO Box C700, West Conshohocken, PA 19428-2959, n.d.: pp. 164-164–12. doi:https://doi.org/10.1520/STP38091S.10.1520/STP38091S ↗
28. The crystallography of stress corrosion cracking in face centered cubic single crystals10.1016/0010-938X(84)90123-9 ↗
29. Studies of the orientations of fracture surfaces produced in austenitic stainless steels by stress-corrosion cracking and hydrogen embrittlement10.1007/BF02654520 ↗
30. Low-temperature stress corrosion cracking of stainless steels in the atmosphere in the presence of chloride deposits10.5006/1.3319115 ↗
31. Investigation into composition and deposition of artificially produced marine aerosols on austenitic stainless steels10.1179/1743278214Y.0000000179 ↗
32. Corrosion control of stainless steels in indoor atmospheres—laboratory measurements under MgCl2 deposits at constant relative humidity (Part 1)10.5006/1437 ↗
33. Low-temperature stress corrosion cracking of Austenitic and duplex stainless steels under chloride deposits10.5006/1242 ↗