High temperature oxidation of irons without and with 0.06 wt.% Sn in dry and humidified oxygen
Source abstract
Abstract
Abstract Irons without and with 0.06 wt.% Sn were oxidised in oxygen at 700–900 °C. The oxidation rates were parabolic with a reduced rate for the iron having higher Sn content. Oxidation rates of each studied material in dry and humidified oxygen were similar at 700 °C. However, the rate in humidified oxygen tended to be higher at higher temperatures. The Arrhenius relations for oxidation of the studied materials in both atmospheres were reported.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Metallurgical Processes and Thermodynamics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Oxidation of simulated recycled steels with 0.23 and 1.03 wt.% Si in Ar-20% H2O at 900 ºC10.1016/j.corsci.2014.06.018 ↗
2. Adhesion of thermal oxide scales on hot-rolled conventional and recycled steels10.1007/s11085-012-9356-9 ↗
3. Copper and tin in steel scrap recycling
4. Ginzgurg · 2009
5. Effects of TMCP schedule on precipitation, microstructure and properties of Ti-microalloyed high strength steel10.1016/S1006-706X(16)30093-0 ↗
6. Case study of severe strip breakage in rolling mill of Thin Slab Casting and Rolling (TSCR) shop of TATA steel, Jamshedpur10.1016/j.csefa.2015.11.002 ↗
7. Oxidation kinetics, mechanical adhesion and pickling behaviour of thermal oxide scales on hot-rolled conventional and recycled steels
8. The role of tin in the hot-ductility deterioration of a low-carbon steel10.1007/s11661-003-0306-7 ↗
9. Influence of Cu and Sn on hot ductility of steels with various C content10.2355/isijinternational.37.255 ↗
10. Characteristics of hot ductility in steels subjected to the melting and solidification10.2355/isijinternational1966.22.48 ↗
11. Effects of residual elements arsenic, antimony, and tin on surface hot shortness10.1007/s11663-011-9528-z ↗
12. Barin · 1989
13. Thermodynamic evaluation of the In-Sn-O system10.1016/j.jallcom.2005.11.083 ↗
14. Kubaschewski · 1993
15. Oxide-Scale Structures formed on commercial hot-rolled steel strip and their formation mechanisms10.1023/A:1010395419981 ↗
16. Review of the high-temperature oxidation of iron and carbon steels in air or oxygen10.1023/A:1023685905159 ↗
17. High temperature oxidation of micro-alloyed steel and its scale adhesion10.1007/s11085-017-9712-x ↗
18. Effects of carbon and coiling temperature on the adhesion of thermal oxide scales to hot-rolled carbon steels10.1016/j.corsci.2016.11.014 ↗
19. Effects of Si and its content on the scale formation on hot-rolled steel strips10.1016/j.matchemphys.2008.06.021 ↗
20. Comparison between the oxidation of iron in oxygen and in steam at 650–750 C10.1016/j.corsci.2013.06.014 ↗
21. Rates of scale formation on iron and a few of its alloys
22. The oxidation of pure iron
23. On the mechanism and kinetics of the scaling of iron
24. The kinetics of the air oxidation of iron in the range 700–1250°C10.1016/0001-6160(58)90006-3 ↗
25. Temperature dependence of scaling of pure iron in oxygen10.1002/srin.195802678 ↗
26. Kofstad · 1988
27. Young · 2016
28. Sarrazin · 2008
29. Observation on isothermal reactive diffusion between solid Fe and liquid Sn10.2320/matertrans.M2012060 ↗
30. The Fe-O-Sn-Zn (iron-oxygen-tin-zinc)10.1007/s11669-010-9722-8 ↗
31. Einfluss von wasserdampf und kohlendioxyd auf die oxydation von eisen in sauerstoff bei hohen temperaturen10.1016/S0010-938X(65)90500-7 ↗
32. The oxidation of iron at 950 ºC in oxygen/water vapour mixtures10.1016/S0010-938X(69)80056-9 ↗
33. Effects of the presence of water vapour on the oxidation behaviour of low carbon-low silicon steel in 1% O2–N2 at 1073 K10.1007/s11085-012-9314-6 ↗
34. High temperature oxidation behaviour of Fe-15.7 wt.% Cr-8.5 wt.% Mn in oxygen without and with water vapour at 700 ºC
35. Effects of process parameters on mechanical adhesion of thermal oxide scales on hot-rolled low carbon steels10.1007/s11085-013-9370-6 ↗
36. Oxidation in steam and steam/hydrogen environments