journal article·2019-11

The roles of thermal mechanical treatment and δ phase in the stress corrosion cracking of alloy 718 in primary water

M. Wang, M. Song, G.S. Was, J.L. Nelson

Corrosion Science· Volume 160
Publisher page

Abstract

Abstract Eleven variants of the precipitation-hardened alloy 718 were tested for stress corrosion cracking (SCC) resistance in a simulated pressurized water reactor primary water environment. The optimized grade had the lowest SCC susceptibility, while more traditional thermal-mechanical treatment exhibited the highest. The high susceptibility was attributed primarily to δ phase formation at grain boundaries (GBs), with localized deformation playing a secondary role. Intergranular cracks initiated most often at GBs decorated with either the high temperature δ phase, which aligned with respect to the slip planes intersecting the GB, or the low temperature δ phase, which is a film on the GB.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Nuclear Materials and Properties · High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. 2013
2. SCC properties of modified alloy 718 in BWR plant
3. Inconel alloy 718 · 1978
4. Application of alloy 718 in GE aircraft engines: past, present and next five years
5. The initial years of alloy 718 – a GE perspective
6. 2004
7. 2013
8. The effect of thermal treatment on SCC of alloy 718: a structure – properties study.
9. Creep crack growth in alloy 718
10. 1996
11. 1999
12. 1994
13. Precipitation in alloy 718: a combined AEM and APFIM investigation
14. TEM study of high-temperature precipitation of delta phase in Inconel 718 alloy10.1155/2011/940634 ↗
15. Isolation and determination for δ, γ′ and γ′′ phases in Inconel 718 alloy10.1016/S1359-6462(02)00041-6 ↗
16. The effect of microstructure on the SCC behavior of alloy 718
17. Deleume · 2007
18. Delta phase precipitation in Inconel 71810.1016/j.matchar.2004.07.004 ↗
19. Modelling of δ-phase dissolution during preheating of Inconel 718 turbine disks
20. Metallurgical stability of Inconel alloy 718
21. Grain boundary δ-phase morphologies, carbides and notch rupture sensitivity of case alloy 718.
22. Creep crack growth in alloy 71810.1007/BF02661754 ↗
23. Stress corrosion of chemistry and heat treat variants of alloy 718, part 1: stress corrosion test results
24. Stress corrosion of chemistry variants of alloy 718, part 2: microstructural characterization
25. Stress corrosion cracking of alloy 718 in pressurized water reactor primary water.
26. Delta (Ni3Nb) and IGSCC degradation in alloy 718 and derivatives
27. Deformability of austenitic stainless steels and Ni-base alloys in the core of a boiling and a pressurized water reactor
28. Influence of phase precipitation on the stress corrosion cracking resistance of alloy 718 in PWR primary water10.1016/j.jnucmat.2008.09.018 ↗
29. Radiation tolerance of commercial and advanced alloys for core internals: a comprehensive microstructural characterization10.1016/j.jnucmat.2018.08.035 ↗
30. Irradiation assisted stress corrosion cracking of commercial and advance alloys for light water reactor core internals10.1016/j.jnucmat.2018.12.015 ↗
31. Characterization of alloy 718 subjected to different thermomechanical treatment10.1016/j.msea.2017.03.045 ↗
32. Was · 2015
33. Was · 2017
34. Standard specification for precipitation-hardening and cold worked nickel alloy bars, forgings, and forging stock for moderate or high temperature service. ASTM B637-16, 2016.
35. Eiselstein · 1965 · 62
36. A current T-T-T diagram for wrought alloy 718
37. TTT diagram of a newly developed nickel-base superalloy – Allvac® 718Plus™
38. Precipitation of the δ-Ni3Nb phase in two nickel base superalloys10.1007/BF02649259 ↗
39. Delta phase in Inconel 718: mechanical properties and forging process requirements
40. Short term precipitation kinetics of delta phase in strain free Inconel 718 alloy10.1179/026708304225019830 ↗
41. Dissolution kinetics of δ phase and its influence on the notch sensitivity of Inconel 71810.1016/j.matchar.2006.04.020 ↗
42. Stress corrosion cracking behavior of alloy 718 subjected to various thermal mechanical treatments in primary water
43. Was · 2017
44. Impact of localized deformation on IASCC in austenitic stainless steels10.1016/j.jnucmat.2010.10.087 ↗
45. The role of irradiated microstructure in the localized deformation of austenitic stainless steels10.1016/j.jnucmat.2010.07.006 ↗
46. Strain localization at dislocation channel-grain boundary intersections in irradiated stainless steel10.1016/j.ijplas.2014.01.001 ↗
47. Quantitative analysis of localized stresses in irradiated stainless steels using high resolution electron backscatter diffraction and molecular dynamics modeling10.1016/j.scriptamat.2016.01.017 ↗
48. Quantitative linkage between the stress at dislocation channel – grain boundary interaction sites and irradiation assisted stress corrosion crack initiation10.1016/j.actamat.2019.02.032 ↗
49. Influence of localized deformation on A-286 austenitic stainless steel stress corrosion cracking in PWR primary water10.1016/j.jnucmat.2007.01.001 ↗
50. Deformation behaviour of γ ″strengthened Inconel 71810.1016/0001-6160(88)90139-3 ↗
51. High temperature oxidation of Nb, NbC and Ni3Nb and oxygen enhanced crack growth10.1016/S1359-6462(99)00336-X ↗