journal article·2020-04

Hydrogen embrittlement of 718 under cathodic polarization

Ramgopal Thodla, Ashwini Chandra, Xiaoji Li, Christopher D. Taylor, Huibin Ke, Narasi Sridhar

Corrosion Science· Volume 165
Publisher page

Abstract

Abstract High strength nickel based alloys are extensively used in both O&G and Navy applications. 718 is one of the most commonly used alloys in these applications. Applied cathodic potential had a significant effect on the crack growth rate (CGR) of various grades of 718. Crevice geometry was used to estimate the crack tip pH and potential conditions under cathodic polarization. Density functional theory (DFT) modelling was performed to estimate the water coverage on fresh metal surfaces of 718 under the crack tip conditions. The CGR was related to the estimated water adsorption on fresh metal surfaces in the measured crack tip conditions.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. Understanding Field failures of alloy 718 forging materials in HPHT wells
2. Study of the effect of δ phase on hydrogen embrittlement of Inconel 718 by notch tensile tests10.1016/j.corsci.2004.06.008 ↗
3. On the role of precipitates in hydrogen trapping and hydrogen embrittlement of a nickel-based superalloy10.1016/j.corsci.2018.10.019 ↗
4. Tensile mechanical properties and fracture behaviors of nickel-based superalloy 718 in the presence of hydrogen10.1016/j.ijhydene.2018.08.179 ↗
5. Hydrogen-assisted failure in Ni-based superalloy 718 studied under in situ hydrogen charging: the role of localized deformation in crack propagation10.1016/j.actamat.2017.02.059 ↗
6. Effects of precipitation phases on the hydrogen embrittlement sensitivity of Inconel 71810.1016/S1468-6996(02)00039-6 ↗
7. Effect of microstructure and alloy chemistry on hydrogen embrittlement of precipitation-hardened Ni-Based alloys10.1007/s11661-018-4483-9 ↗
8. Hydrogen assisted crack initiation and propagation in a nickel-based superalloy10.1016/j.actamat.2016.05.003 ↗
9. High strength fasteners for subsea applications
10. Development of test methodology to evaluate High strength nickel based alloys under cathodic protection
11. Cathodic hydrogen embrittlement in alloy 71810.1016/S0921-5093(99)00167-7 ↗
12. Effect of trapping and temperature on the hydrogen embrittlement susceptibility of alloy 71810.1016/j.msea.2014.06.015 ↗
13. Turnbull · 1983
14. Experimental determination of the electrochemistry in corrosion fatigue cracks in structural steel in artificial seawater10.5006/1.3582026 ↗
15. Measurement and modeling of hydrogen environment-assisted cracking in Monel K-50010.1007/s11661-014-2324-z ↗
16. Refilming kinetics of scraped steel electrodes in simulated corrosion fatigue crack-tip environments10.1016/0010-938X(89)90046-2 ↗
17. Predicting the kinetics of hydrogen generation at the tips of corrosion fatigue cracks10.1007/BF02645148 ↗
18. 2015
19. 2015
20. S. M. Bruemmer, M. B. Toloczko, and M. J. Olszta, "Pacific Northwest National Laboratory Investigation of the Stress Corrosion Cracking in Nickel-Base Alloys, Volume 1," Pacific Northwest National Lab.(PNNL), Richland, WA (United States).
21. Andresen · 1998
22. ASTM E1681-03(2013) · 2013
23. Combining rigorously controlled crevice geometry and computational modeling for study of crevice corrosion scaling factors10.1149/1.1753581 ↗
24. Crevice scaling laws to investigate local hydrogen uptake in rescaled model occluded sites
25. Investigation of local hydrogen uptake in rescaled model occluded sites using crevice scaling laws
26. Predictions of surface electrochemistry of saturated and alkaline NH4Cl solutions interacting with Fe (110) from ab initio calculations10.5006/0411 ↗
27. First-principles investigation of surface properties and adsorption of oxygen on Ni-22Cr and the role of molybdenum10.1016/j.corsci.2018.02.017 ↗
28. Oxidation versus salt-film formation: competitive adsorption on a series of metals from first-principles10.1016/j.electacta.2018.02.150 ↗
29. Chloride susceptibility index (CSI): an Ab initio based corrosion resistance indicator
30. Hydrogen Embrittlement Study of Three Heats of UNS N07718 In Subsea Applications
31. Environmentally assisted cracking of High strength nickel based alloys under cathodic protection
32. In-situ observation of hydrogen induced crack initiation in a nickel-based superalloy10.1016/j.scriptamat.2017.07.006 ↗
33. Deformation behaviour of γ″ strengthened inconel 71810.1016/0001-6160(88)90139-3 ↗
34. Gamma double prime precipitation kinetic in Alloy 71810.1016/j.msea.2007.08.046 ↗
35. Hydrogen trapping in some advanced high strength steels10.1016/j.corsci.2016.05.046 ↗
36. Effect of strain rate on the fatigue and static crack growth rate of UNS N07718 under cathodic polarization
37. Hydrogen-enhanced cracking of superalloys10.1007/BF02660868 ↗
38. Lillard · 1998
39. The effect of microstructural variation on the hydrogen environment-assisted cracking of monel K-50010.1007/s11661-016-3486-7 ↗
40. Measurement and modeling of temperature dependent internal hydrogen assisted cracking in Cr-Mo steel
41. Hydrogen diffusion coefficients through Inconel 718 in different metallurgical conditions10.1016/j.corsci.2013.11.002 ↗
42. Hydrogen permeation and diffusion in inconel 718 and incoloy 90310.1007/BF02646873 ↗
43. Strain gradient plasticity-based modeling of hydrogen environment assisted cracking10.1016/j.actamat.2016.07.022 ↗