journal article·2011-02

High temperature oxidation of AZ91D magnesium alloy granule during in-situ melting

Hassan Jafari, Mohd Hasbullah Idris, Ali Ourdjini

Corrosion Science· Volume 53· Issue 2
Publisher page

Abstract

Abstract Oxidation behaviour of AZ91D was investigated by heating the alloy granules in a ceramic mould between 650 and 800 °C, for 30 and 60 min. The granules failed to melt in unprotected environment even when the temperature was increased to 800 °C. Raising the temperature increased the oxides thickness linearly, however, oxidation enhanced beyond 750 °C with severe mould–metal reaction and selective oxidation. Heating duration showed more pronounced effect on oxide formation compared to heating temperature. MgO was found to be the dominant compound in oxidation products. Aluminium participated during severe oxidation or combustion to some extent whilst no zinc oxide was detected.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Y. Kojima, T. Aizawa, K. Higashi, S. Kamado, Magnesium Alloys 2003, Proceedings of the Second Osaka International Conference on Platform Science and Technology for Advanced Magnesium Alloys 2003, Osaka, Japan, in: Materials Science Forum, 2003, pp. 419–422.10.4028/www.scientific.net/MSF.419-422.3 ↗
2. Effect of thermomechanical treatment on microstructure and hardness behavior of AZ63 magnesium alloy10.1016/S1006-7191(08)60115-5 ↗
3. Microstructures and properties of die casting components with various thicknesses made of AZ91D alloy10.1016/j.jmatprotec.2008.07.034 ↗
4. Film formation in the second step of micro-arc oxidation on magnesium alloys10.1016/j.corsci.2009.12.025 ↗
5. Microstructure and mechanical properties of AZ31B magnesium alloy recycled by solid-state process from different size chips10.1016/j.jmatprotec.2009.04.002 ↗
6. Effect of chip size on mechanical property and microstructure of AZ91D magnesium alloy prepared by solid state recycling10.1016/j.matchar.2007.02.002 ↗
7. Enhanced corrosion properties of pure Mg and AZ31 Mg alloy recycled by solid-state process10.1016/j.msea.2006.07.019 ↗
8. Effect of heat treatment on the microstructure and mechanical properties of the consolidated Mg alloy AZ91D machined chips10.1016/j.jmatprotec.2008.11.001 ↗
9. Effect of yttrium addition and the powder size on oxide film and powder ignition temperature of AZ91D magnesium alloy10.1016/j.jallcom.2009.02.132 ↗
10. Effect of Ce addition on ignition point of AM50 alloy powder10.1016/j.matlet.2006.02.086 ↗
11. Ignition-proof mechanism of ZM5 magnesium alloy added with rare earth10.1007/s11771-010-0006-6 ↗
12. Effect of Ca and Y additions on oxidation behaviour of AZ91 alloy at elevated temperatures10.1016/S1003-6326(08)60268-X ↗
13. Newly developed magnesium alloys for powertrain applications10.1007/s11837-003-0206-8 ↗
14. Review on research and development of magnesium alloys10.1016/S1006-7191(08)60054-X ↗
15. Magnesium technology 2002, Part I: Primary production, environmental issues, high-temperature alloys10.1007/BF02711861 ↗
16. Interactive effect of cerium and aluminum on the ignition point and the oxidation resistance of magnesium alloy10.1016/j.corsci.2008.06.025 ↗
17. Oxidation behaviour of molten magnesium and AZ91D magnesium alloy in 1,1,1,2-tetrafluoroethane/air atmospheres10.1016/j.corsci.2008.10.011 ↗
18. Oxidation resistance of cast magnesium alloys10.1007/s11085-009-9141-6 ↗
19. Characterisation of fresh surface oxidation films formed on pure molten magnesium in different atmospheres10.1016/j.corsci.2010.02.003 ↗
20. Combustion of AZ61A under different gases10.1016/S0254-0584(01)00412-6 ↗
21. F. Czerwinski, The oxidation of magnesium alloys in solid and semisolid state, in: H.I. Kaplan (Ed.), Magnesium Technology 2003, TMS 2003, pp. 39–42.
22. The oxidation behaviour of an AZ91D magnesium alloy at high temperatures10.1016/S1359-6454(02)00094-0 ↗
23. Combustion of magnesium alloys in air10.1016/j.matchemphys.2004.01.036 ↗
24. Effect of alloying elements on the ignition resistance of magnesium alloys10.1016/S1359-6462(03)00263-X ↗
25. Ignition of magnesium and magnesium–aluminum alloy by impinging hot-air stream10.1080/00102208008946924 ↗
26. The early stage oxidation and evaporation of Mg–9%Al–1%Zn alloy10.1016/S0010-938X(03)00151-3 ↗
27. The effects of cerium implantation on the oxidation behavior of AZ31 magnesium alloys10.1016/j.jallcom.2007.02.048 ↗
28. Structure analysis of oxidation film of ignition-inhibition AZ91D magnesium alloy added with cerium
29. Behaviour of surface oxidation on molten Mg–9AAl–0.5Zn–0.3Be alloy10.1016/S0921-5093(00)01798-6 ↗
30. Birks · 2006
31. Pilling–Bedworth ratio for oxidation of alloys10.1007/s100190050008 ↗
32. Ignition of magnesium and its alloys10.1007/BF00775738 ↗
33. Corrosion and high temperature oxidation of AM60 magnesium alloy