journal article·2016-04

Improved oxide scale adherence of low-Pt/Hf co-doped β-NiAlCrSi coating on superalloy IC21 at 1200°C

Zimin Zhou, Hui Peng, Lei Zheng, Hongbo Guo, Shengkai Gong

Corrosion Science· Volume 105
Publisher page

Abstract

Abstract Low-Pt/Hf co-doped β-NiAlCrSi and Hf single-doped β-NiAlCrSi coatings were produced onto advanced single crystal (SC) superalloy IC21 containing Mo, respectively. The cyclic oxidation and interdiffusion behaviour of the coatings at 1200 °C were investigated. As compared to the single-doped coating, the co-doped coating revealed suppressed interdiffusion and delayed β–γ′ phase transformation. Simultaneously, the interfacial voids formation and scale rumpling were inhibited. As a result, the thermally grown oxide (TGO) grown on the co-doped coating exhibited improved adherence and the roles of Pt and Hf in low-Pt/Hf co-doped coating were discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Cyclic behaviour of EB-PVD thermal barrier coating systems with modified bond coats10.1016/j.surfcoat.2008.08.056 ↗
2. In-situ SEM study of cavity growth during high temperature oxidation of β-(Ni, Pd)Al10.1016/S1359-6462(01)00959-9 ↗
3. NiAl bond coats made by a directed vapour deposition approach10.1016/j.msea.2004.11.017 ↗
4. Martensitic transformation in CVD NiAl and (Ni, Pt)Al bond coatings10.1016/S0257-8972(02)00585-6 ↗
5. Cyclic oxidation and interdiffusion behaviour of a NiAlDy/RuNiAl coating on a Ni-based single crystal superalloy10.1016/j.corsci.2011.04.025 ↗
6. Comparison of the cyclic oxidationbehaviour of β-NiAl, β-NiPtAl and γ–γ′ NiPtAlcoatings onvarious superalloys10.1016/j.surfcoat.2007.06.039 ↗
7. Effect of co-doping of two reactive elements on alumina scale growth of β-NiAl at 1200°C10.1016/j.corsci.2014.07.036 ↗
8. Effect of different B contents on the mechanical properties and cyclic oxidation behaviour of β-NiAlDy coatings10.1016/j.jallcom.2014.10.116 ↗
9. Cyclic oxidation of β-NiAl with various reactive element dopants at 1200°C10.1016/j.corsci.2012.09.010 ↗
10. Effect of Sm, Gd, Yb, Sc and Nd as reactive elements on oxidation behaviour of β-NiAl at 1200°C10.1016/j.corsci.2013.10.021 ↗
11. Partition of alloying elements between γ (A1), γ′ (L12), and β (B2) phases in Ni–Al base systems10.1007/BF02651589 ↗
12. Influences of chromium and hafnium additions on the microstructures of β-NiAl coatings on superalloy substrates10.1016/j.intermet.2011.06.020 ↗
13. The role of Cr and Si in affecting high-temperature oxidation behaviour of minor Dy doped NiAl alloys10.1016/j.corsci.2013.08.020 ↗
14. Cyclic-oxidation behaviour of multilayered Pt/Ru-modified aluminide coating10.1016/S1005-0302(11)60063-7 ↗
15. On the interfacial degradation mechanism of thermal barrier coating system: effects of bond coat composition10.1016/j.actamat.2010.06.027 ↗
16. Influence of Pt on the metal-oxide interface during high temperature oxidation of NiAl bulk materials10.1016/j.corsci.2008.12.016 ↗
17. Surface and interface segregation in β-NiAl with and without Pt addition10.1016/j.scriptamat.2005.10.065 ↗
18. J. Angenete, Aluminide diffusion coatings for Ni based superalloys: coating and oxide microstructure. Ph.D. thesis. Gӧeborg, Sweden: Department of Experimental Physics, Chalmers University of Technology, Gӧeborg University; 2002.
19. Microstructures and cyclic oxidation behaviour of Pt-free and low-Pt NiAl coatings on the Ni-base superalloy Rene-8010.1016/j.corsci.2011.10.037 ↗
20. Degradation of the platinum aluminide coating on CMSX-4 at 1100°C10.1016/S0257-8972(96)03117-9 ↗
21. The effect of silicon on the oxidation behavior of NiAlHf coating system10.1016/j.apsusc.2013.01.189 ↗
22. Rhys-Jones TN, Role of platinum in aluminide coatings10.1016/0257-8972(91)90022-O ↗
23. Comparative thermal stability characteristics and isothermal oxidation behaviour of an aluminized and a Pt-aluminized Ni-base superalloy10.1016/0956-716X(95)00388-C ↗
24. Effect of zirconium addition on cyclicoxidation behaviour of platinum-modifiedaluminide coating on nickel-based superalloy10.1016/j.intermet.2009.12.012 ↗
25. The effect of an oxide dispersion on the critical Al content in Fe–Al alloys10.1023/A:1018862404800 ↗
26. Comparison of inward and outward grown Pt modified aluminide diffusion coatings on a Ni based single crystal superalloy10.1016/S0257-8972(01)01544-4 ↗
27. Effect of Pt and Al content on the long-term, high temperature oxidation behaviour and interdiffusion of a Pt-modified aluminide coating deposited on Ni-base superalloys10.1016/j.surfcoat.2006.07.246 ↗
28. Rumpling of CVD (Ni,Pt)Al diffusion coatings under intermediate temperature cycling10.1016/j.surfcoat.2009.04.016 ↗
29. Effect of prealuminizing diffusion treatment on microstructural evolution of high-activity Pt-aluminide coatings10.1007/s11661-000-0231-y ↗
30. Formation of secondary reaction zones in diffusion aluminide-coated Ni-base single-crystal superalloys containing ruthenium10.1007/s11661-008-9534-1 ↗
31. Platinum and the oxidation behaviour of a nickel based superalloy10.1007/BF00656576 ↗
32. Use of platinum and rhodium to improve oxide adherence on Ni-8Cr-6Al alloys10.1007/BF00611696 ↗
33. Effect of Al content on microstructure and cyclic oxidation performance of Pt-aluminide coatings10.1023/A:1014822217982 ↗
34. The influence of grain-boundary segregation of Y in Cr2O3 on the oxidation of Cr metal10.1007/BF00665014 ↗
35. The oxidation behavior of Y2O3-dispersed-NiAl10.1023/B:OXID.0000025335.62402.79 ↗
36. Improved cyclic oxidation resistance of electron beam physical vapour deposited nano-oxide dispersed β-NiAl coatings for Hf-containing superalloy10.1016/j.corsci.2010.01.009 ↗
37. Evolution of a diffusion aluminide bond coat for thermal barrier coatings during thermal cycling10.1016/S1359-6454(03)00014-4 ↗
38. Effect of temperature on rumpling and thermally grown oxide stress in an EB-PVD thermal barrier coating10.1016/j.surfcoat.2006.07.212 ↗
39. Surface rumpling of a (Ni, Pt)Al bond coat induced by cyclic oxidation10.1016/S1359-6454(00)00156-7 ↗
40. Deformation and phase transformations during the cyclic oxidation of Ni–Al and Ni–Pt–Al
41. NiAlHf/Ru: promising bond coat materials in thermal barrier coatings for advanced single crystal superalloys10.1016/j.corsci.2013.10.013 ↗