Effect of brief thermal aging on stress corrosion cracking susceptibility of LDSS 2101 in the presence of chloride and thiosulphate ions

F. Zanotto, V. Grassi, A. Balbo, C. Monticelli, C. Melandri, F. Zucchi

Corrosion Science· Volume 130

Abstract

Abstract In this paper, the effect of brief aging within the 650–850 °C temperature range on the resistance of lean duplex stainless steel (LDSS) 2101 to stress corrosion cracking (SCC) was discussed. The thermal aging induced a decrease in Vickers microhardness and an increase in alloy ductility. This behaviour was connected to depletion of interstitial nitrogen in austenite. LDSS 2101 was found to suffer SCC in NACE TM-0177 solution, particularly under specific thermal aging and in the presence of thiosulphate ions (S2O32−) at 10−4 and 10−3 M. Crack nucleation and propagation were linked to microstructural variations connected to thermal aging.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (62)

Show source-provided references
1. The history of duplex developments, nowadays DSS properties and duplex market future trends
2. Duplex –a new generation of stainless steels for desalination plants10.1016/j.desal.2006.02.051 ↗
3. Influence of chemical composition on the pitting corrosion resistance of non-standard low-Ni high- Mn–N duplex stainless steels10.1016/S0010-938X(02)00154-3 ↗
4. Application of the modified electrochemical potentiodynamic reactivation method to detect susceptibility to intergranular corrosion of a newly developed lean duplex stainless steel LDX 210110.1016/j.corsci.2009.11.020 ↗
5. Study of mechanical and corrosion properties of a Fe-21.4Cr-6Mn-1.5Ni-0.24N-0.6Mo duplex stainless steel10.1016/j.msea.2008.07.062 ↗
6. Effect of intermetallic precipitations on the properties of duplex stainless steel10.1016/j.matchar.2006.03.015 ↗
7. Influence of microstructure on the corrosion resistance of the duplex stainless steel UNS S3180310.1016/j.matchar.2007.09.002 ↗
8. Infuence of σ-phase on mechanical properties and corrosion resistance of duplex stainless steels10.1016/S0010-938X(99)00009-8 ↗
9. Application of double loop electrochemical potentiodynamic reactivation test to austenitic and duplex stainless steels10.1016/S0921-5093(97)00008-7 ↗
10. Microstructural evolution and localized corrosion resistance of an aged superduplex stainless steel10.1016/j.corsci.2003.09.024 ↗
11. The influence of solution treatment temperature on microstructure and corrosion behavior of high temperature ageing in 25% Cr duplex stainless steel10.1016/j.jallcom.2011.06.099 ↗
12. The effect of large heat input on the microstructure and corrosion behavior of simulated heat affected zone in 2205 duplex stainless steel10.1016/j.corsci.2011.07.022 ↗
13. Evaluation of aged duplex stainless steel UNS S32750 susceptibility to intergranular corrosion by optimized double loop electrochemical potentiokinetic reactivation method10.1016/j.corsci.2012.11.024 ↗
14. Influence of cold work and sigma phase on the pitting corrosion behavior of 25 chromium super duplex stainless steel in 3.5% sodium chloride solution10.1002/maco.200905312 ↗
15. Evaluation of intergranular corrosion susceptibility of UNS S31803 duplex stainless steel with an optimized double loop electrochemical potentiokinetic reactivation method10.1016/j.electacta.2010.03.086 ↗
16. Effect of ageing on precipitation and impact energy of 2101 economical duplex stainless steel10.1016/j.matchar.2008.07.002 ↗
17. Structural evolution of LDX 2101® (EN 1.4162) during isothermal ageing at 600–850°C
18. Lean duplex stainless steel within the oli and gas industry, vol. 4
19. Role of nitrogen in the pitting resistance of cast duplex CF-type stainless steels10.5006/1.3577829 ↗
20. The influence of nitrogen on the passivation of stainless steels10.1016/0010-938X(96)00018-2 ↗
21. On the behaviour of nitrogen in a low-Ni high-Mn super duplex stainless steel10.1016/j.matdes.2010.11.021 ↗
22. The influence of nitrogen content on corrosion fatigue crack growth behavior of duplex stainless steel10.1016/S0921-5093(02)00404-5 ↗
23. Cleavage-Like fracture of austenite in duplex stainless steel10.1016/0956-716X(93)90300-H ↗
24. Effect of nitrogen partitioning on yield strength in nitrogen-Alloyed duplex stainless steel during annealing10.1007/s11661-014-2210-8 ↗
25. Chloride-induced stress corrosion cracking of Duplex stainless steels. Models, test methods and experience
26. Effects of processing and manufactruring of high nitrogen-containing stainless steels on their mechanical, corrosion and wear properties10.1016/S0924-0136(01)00804-4 ↗
27. Estimating localized corrosion resistance of low alloy stainless steels: comparison of pitting potentials and critical pitting temperatures measured on lean duplex stainless steel LDX 2101 after sensitization10.1179/174327808X286347 ↗
28. Effect of aging on the corrosion of 2101 lean duplex stainless steel10.1016/j.matchar.2009.08.009 ↗
29. Investigation of selective corrosion resistance of aged lean duplex stainless steel 2101 by non-destructive electrochemical techniques10.1016/j.electacta.2009.05.039 ↗
30. Effect of brief heat treatments performed between 650 and 850°C on corrosion behaviour of a lean duplex stainless steel10.1016/j.corsci.2015.01.035 ↗
31. Effect of hydrogen concentrationon the embrittlement of a duplex stainless steel10.1016/j.corsci.2004.07.036 ↗
32. Stress corrosion cracking resistance of 22 duplex stainless steel in simulated sour environments10.5006/1.3584990 ↗
33. Sterss corrosion cracking of duplex and super duplex stainless steels in sour environments10.1016/S0010-938X(98)00022-5 ↗
34. Influence of dynamic straining on hydrogen embrittlement of UNS-G41300 and UNS-S31803 steels in a low H2S concentration environment10.1016/j.corsci.2004.07.033 ↗
35. Investigation of hydrogen induced cracking in 2205 duplex stainless steel in wet H2S environments after isothermal treatment at 675, 750 and 900°C10.1016/j.matchar.2005.11.024 ↗
36. Stress corrosion cracking of 2205 duplex stainless steel in H2S–CO2 environment10.1007/s10853-009-3520-x ↗
37. Corrosion behavior of 25 Pct Cr duplex stainless steel in CO2–H2S–Cl–environments10.1007/BF02833508 ↗
38. Stress corrosion cracking susceptibility of duplex stainless steels in sour gas environments10.1007/BF02833502 ↗
39. Stress corrosion cracking of duplex stainless steel weldments in sour conditions
40. Stress corrosion cracking of LDX 2101® duplex stainless steel in chloride solutions in the presence of thiosulphate10.1016/j.corsci.2013.11.028 ↗
41. Alternative for evaluating sour gas resistance of low-alloy steels and corrosion-resistant alloys10.5006/1.3316068 ↗
42. An alternative test method for evaluating the sour gas resistance of low-alloy steels and CRAs
43. Role of thiosulfate in the corrosion of steels: a review10.5006/1709 ↗
44. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
45. 1988 · vol. 13
46. 1990
47. Effect of nitrogen content on grain refinement and mechanical properties of a reversion-treated Ni-free 18Cr-12 Mn austenitic stainless steel10.1007/s11661-014-2595-4 ↗
48. Effect of hydrogen on the hardness of different phases in super duplex stainless steel10.1016/j.ijhydene.2015.10.106 ↗
49. Measurements of thermal residual elastic strains in ferrite-austenite Fe-Cr-Ni alloys by neutron and X-ray diffractions10.1016/S1359-6454(98)00300-0 ↗
50. Thermally induced microstructural changes of ferritic-austenitic stainless steels and their influence on residual stress
51. Evolution of the residual stress state in a duplex stainless steel during loading10.1016/S1359-6454(99)00149-4 ↗
52. Marcus · 1995
53. Effects of nitrogen and tensile direction on stress corrosion cracking susceptibility of Ni-free feCrMnC-Based duplex stainless steels
54. On the depassivation mechanism of lean duplex stainless steels and influence of the partitioning of the alloying elements10.5006/1173 ↗
55. Effect of nitrogen content on the environmentally-assisted cracking susceptibility of duplex stainless steels10.1007/s11661-003-0211-0 ↗
56. Microstructure and stress corrosion cracking in simulated heat-affected zone of duplex stainless steels10.1016/S0010-938X(02)00068-9 ↗
57. Determination of susceptibility to intergranular corrosion and electrochemical reactivation behaviour of AISI 316L type stainless steel10.1016/j.corsci.2006.01.003 ↗
58. Stress corrosion cracking of sensitized Type 304 stainless steel in thiosulphate solution. II. Dynamics of fracture10.1016/j.corsci.2005.06.010 ↗
59. Hydrogen transport and degradation of a commercial duplex stainless steel10.1016/S0010-938X(01)00143-3 ↗
60. The hydrogen content of austenite after cathodic charging10.1016/0036-9748(81)90047-8 ↗
61. Hydrogen embrittlement of 22-5 duplex stainless steel10.1179/bcj.1998.33.1.49 ↗
62. Effect of heat treatment on susceptibility of duplex stainless steel to embrittlement by hydrogen10.1179/026708300101508162 ↗