Ion transport mechanisms in the passive film formed on 304L stainless steel studied by ToF-SIMS with 18O isotopic tracer
Source abstract
Abstract
Abstract The ion transport in the pre-formed passive film on 304L stainless steel surface has been investigated by in situ ToF-SIMS with isotopic tracer. The passive film, formed electrochemically in sulfuric acid, has a bilayer structure with outer iron oxide and inner chromium oxide layers. Further exposure of the passive film to 18O2 gas (isotopic tracer) at 300 °C reveals that outward cation diffusion is the governing ion transport mechanism for the oxide growth. The parabolic rate constant for the oxide growth was determined. The cation diffusion coefficient is found to be markedly higher than the oxygen diffusion coefficient.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Current developments of nanoscale insight into corrosion protection by passive oxide films10.1016/j.cossms.2018.05.004 ↗
2. Nanoscale morphology and atomic structure of passive films on stainless steel10.1149/2.067306jes ↗
3. Passive films at the nanoscale10.1016/j.electacta.2012.03.158 ↗
4. Davis · 1994
5. Corrosion behavior of 304 stainless steel in high temperature, hydrogenated water10.1016/S0010-938X(02)00004-5 ↗
6. The mechanism of oxide film formation on austenitic stainless steels in high temperature water10.1016/S0010-938X(97)00140-6 ↗
7. Effects of molybdenum on the composition and nanoscale morphology of passivated austenitic stainless steel surfaces10.1039/C4FD00231H ↗
8. Passivation-induced physicochemical alterations of the native surface oxide film on 316L austenitic stainless steel10.1149/2.0321911jes ↗
9. XPS and ToF-SIMS characterization of the surface oxides on lean duplex stainless steel – global and local approaches10.1016/j.corsci.2019.04.039 ↗
10. Comparative study of the surface oxide films on lean duplex and corresponding single phase stainless steels by XPS and ToF-SIMS10.1016/j.corsci.2018.08.009 ↗
11. Mechanisms of Cr and Mo enrichments in the passive oxide film on 316L austenitic stainless steel10.3389/fmats.2019.00232 ↗
12. Comparative study of the native oxide on 316L stainless steel by XPS and ToF-SIMS10.1116/1.4927319 ↗
13. XPS and SEM studies of chromium oxide films chemically formed on stainless steel 316 L10.1016/S0254-0584(00)00249-2 ↗
14. Investigation of oxide film formation on 316L stainless steel in high-temperature aqueous environments10.1016/j.electacta.2011.04.127 ↗
15. Oxide film growth kinetics on metals and alloys I. Physical model10.1149/2.036306jes ↗
16. The role of oxygen transport in oxidation of Fe-Cr alloys10.1080/14786437308228001 ↗
17. Oxide film growth kinetics on metals and alloys II. Numerical simulation of transient behavior10.1149/2.037306jes ↗
18. Investigating the transport mechanisms governing the oxidation of Hastelloy BC-1 by in situ ToF-SIMS10.1016/j.corsci.2019.108138 ↗
19. Anion transport in growing Cr2O3 scales
20. Theoretical analysis of the diffusion processes determining the oxidation rate of alloys10.1149/1.2779605 ↗
21. Oxidation of iron‐molybdenum and nickel‐molybdenum alloys10.1149/1.2429990 ↗
22. Use of 18O/SIMS and electrochemical techniques to study the reduction and breakdown of passive oxide films on iron10.1149/1.2095629 ↗
23. Volatilization and transport mechanisms during Cr oxidation at 300 °C studied in situ by ToF-SIMS10.1007/s11085-017-9756-y ↗
24. On high temperature oxidation of chromium II. Properties of and the oxidation mechanism of chromium10.1149/1.2129481 ↗
25. Kofstad · 1972
26. Atomic transport mechanisms in thin oxide films grown on zirconium by thermal oxidation, as-derived from 18O-tracer experiments10.1016/j.actamat.2011.08.035 ↗
27. Oxide layer growth on nickel-base alloy surfaces in high temperature water and in O2 studied by ToF-SIMS with isotopic tracers10.1016/j.corsci.2018.10.009 ↗
28. Diffusion of cations in chromia layers grown on iron-base alloys10.1007/BF00665632 ↗
29. Relation between the oxidation growth rate of chromia scales and self-diffusion in Cr2O310.1007/BF01166020 ↗
30. Oxide scale formation of Fe–Cr alloys and oxygen diffusion in the scale10.1016/j.ssi.2004.09.045 ↗
31. Ion diffusion study in the oxide layers due to oxidation of AISI 439 ferritic stainless steel10.1007/s11085-013-9451-6 ↗
32. Study of ion diffusion in oxidation films grown on a model Fe–15%Cr alloy10.1016/j.ssi.2015.03.027 ↗
33. About the role of chromium and oxygen ion diffusion on the growth mechanism of oxidation films of the AISI 304 austenitic stainless steel10.1007/s11085-012-9301-y ↗
34. Thermal stability of the passive film formed on 316L stainless steel surface studied by ToF-SIMS
35. ToF-SIMS study of oxide films thermally grown on nickel-base alloys10.1016/j.corsci.2018.06.043 ↗
36. National Research Council · 1970