Abstract

High-quality Li 4 Ti 5 O 12 crystals were successfully grown at a holding temperature of 800 °C and a solute concentration of 50 mol % using the NaCl flux cooling method. Idiomorphic, highly crystalline, and single-phase Li 4 Ti 5 O 12 crystals were first grown from the NaCl flux; therefore, the method is very low cost and environmentally friendly (i.e., safe for the environment and humans). On the basis of the powder X-ray diffraction data, the lattice parameter of the crystals was determined to be a = 0.838 nm. This value is in good agreement with that from the literature ( a = 0.836 nm). The average crystal size was about 2.6 μm. Transmission electron microscope images indicated that the Li 4 Ti 5 O 12 crystals had very good crystallinity. In addition, the crystal phase, crystallinity, shape, and size of the flux-grown Li 4 Ti 5 O 12 crystals were obviously dependent on the growth conditions, such as the holding temperature and solute concentration.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Ferroelectric and Piezoelectric Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Environmental Science and Technology, Faculty of Engineering, Shinshu University, Nagano 380-8553, Japan

Institute for Materials Research, Tohoku University, Sendai 980-8577, Japan

Battery Research Division, Toyota Motor Corporation, 1200 Mishuku, Susono, Shizuoka 410-1193, Japan

References (27)

Show source-provided references
1. Scrosati B. · J. Power Sources · 2010 · 195 · 241910.1016/j.jpowsour.2009.11.048 ↗
2. Megahed S. · J. Power Sources · 1995 · 54 · 15510.1016/0378-7753(94)02059-C ↗
3. Nakano H. · Electrochem. Commun. · 2007 · 9 · 201310.1016/j.elecom.2007.05.020 ↗
4. Kitaura H. · J. Power Sources · 2009 · 189 · 14510.1016/j.jpowsour.2008.10.005 ↗
5. Koga C. · Electrochim. Acta · 2010 · 55 · 256110.1016/j.electacta.2009.12.034 ↗
6. Ge H. · J. Phys. Chem. C · 2009 · 113 · 632410.1021/jp9017184 ↗
7. Kanamura K. · Chem. Lett. · 1997 · 26 · 4510.1246/cl.1997.45 ↗
8. Wang G. X. · J. Power Sources · 1999 · 83 · 15610.1016/S0378-7753(99)00290-6 ↗
9. Leonidov I. A. · Phys. Solid State · 2003 · 45 · 218310.1134/1.1626760 ↗
10. Matsui E. · J. Am. Ceram. Soc. · 2008 · 91 · 152210.1111/j.1551-2916.2008.02269.x ↗
11. Lin C.-Y. · J. Alloys Compd. · 2011 · 509 · 368210.1016/j.jallcom.2010.12.160 ↗
12. Chen J. · Electrochim. Acta · 2010 · 55 · 659610.1016/j.electacta.2010.06.015 ↗
13. Tang Y. F. · Electrochem. Commun. · 2008 · 10 · 151310.1016/j.elecom.2008.07.049 ↗
14. Li Y. · J. Alloys Compd. · 2008 · 455 · 47110.1016/j.jallcom.2007.01.168 ↗
15. Lee D. K. · Nanoscale Res. Lett. · 2010 · 5 · 158510.1007/s11671-010-9680-4 ↗
16. Venkateswarlu M. · J. Power Sources · 2005 · 146 · 20410.1016/j.jpowsour.2005.03.016 ↗
17. Hao Y.-J. · J. Power Sources · 2005 · 94 · 382
18. Lee S. · CrystEngComm · 2009 · 11 · 232610.1039/b905870b ↗
19. Lee S. · CrystEngComm · 2010 · 12 · 287110.1039/b921092j ↗
20. Teshima K. · Cryst. Growth Des. · 2011 · 11 · 99510.1021/cg100932k ↗
21. Kataoka K. · J. Phys. Chem. Solids · 2008 · 69 · 145410.1016/j.jpcs.2007.10.134 ↗
22. Teshima K. · Cryst. Growth Des. · 2010 · 10 · 447110.1021/cg100705d ↗
23. Teshima K. · Cryst. Growth Des. · 2010 · 10 · 253310.1021/cg901229d ↗
24. Teshima K. · Cryst. Growth Des. · 2008 · 8 · 259510.1021/cg070432m ↗
25. Teshima K. · Cryst. Growth Des. · 2008 · 8 · 46510.1021/cg070341p ↗
26. Teshima K. · Cryst. Growth Des. · 2006 · 6 · 159810.1021/cg050673z ↗
27. Teshima K. · CrystEngComm · 2011 · 13 · 119010.1039/C0CE00080A ↗