High-Temperature Phase Transitions Preceding the Decomposition of Mixed Valence Aluminum Titanate Pseudobrookite
Source abstract
Abstract
Dark blue single crystals of Al 1.75 3+ Ti 1.0 4+ Ti 0.25 3+ O 5 were grown with a novel synthesis method based on the reaction of a Ti 3+ /Ti 4+ -containing langbeinite melt and porous α-alumina crucible. The obtained needles crystallize in the pseudobrookite structure and, upon heating, undergo two reversible phase transitions, from orthorhombic Cmcm to C 2/ m first and subsequently to C2 symmetry. Like the known aluminum titanate pseudobrookites, anisotropic thermal expansion is observed. The temperature evolution of the crystal structure reveals insights into the mechanism leading to the decomposition of the pseudobrookites above 725 °C. The magnetic and electrical properties are discussed and compared to other reported aluminum titanate pseudobrookites.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Nuclear materials and radiation effects · Ferroelectric and Piezoelectric Materials · Advanced Condensed Matter Physics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Laboratory of Quantum Magnetism, Institute of Physics, Ecole Polytechnique Fédérale de Lausanne−EPFL, Lausanne CH-1006, Switzerland
Crystal Growth Facility, Institute of Physics, Ecole Polytechnique Fédérale de Lausanne−EPFL, Lausanne CH-1006, Switzerland
Funding
Schweizerischer Nationalfonds zur Förderung der Wissenschaftlichen Forschung · Hrvatska Zaklada za Znanost
References (34)
Show source-provided references
1. 10.1007/BF0299329210.1007/BF02993292 ↗
2. Pellache C. · Am. Mineral. · 1934 · 19 · 16
3. 10.1524/zkri.1928.68.1.23910.1524/zkri.1928.68.1.239 ↗
4. 10.1524/zkri.1930.73.1.9710.1524/zkri.1930.73.1.97 ↗
5. Ottemann J. · Schweizerische Mineral. und Petrogr. Mitteilungen · 1965 · 45 · 819
6. 10.1016/j.lithos.2006.07.00910.1016/j.lithos.2006.07.009 ↗
7. 10.1515/znb-1974-9-100210.1515/znb-1974-9-1002 ↗
8. 10.1002/zaac.1982494011210.1002/zaac.19824940112 ↗
9. 10.1103/PhysRevB.99.06440310.1103/PhysRevB.99.064403 ↗
10. 10.1103/PhysRevB.100.09440110.1103/PhysRevB.100.094401 ↗
11. 10.1002/anie.19650241310.1002/anie.196502413 ↗
12. 10.1021/ja073355s10.1021/ja073355s ↗
13. 10.1246/cl.2002.73610.1246/cl.2002.736 ↗
14. 10.1006/jssc.1997.748110.1006/jssc.1997.7481 ↗
15. 10.1016/j.ceramint.2012.03.04410.1016/j.ceramint.2012.03.044 ↗
16. 10.1107/S056774087200368110.1107/S0567740872003681 ↗
17. 10.1016/j.jeurceramsoc.2008.05.03710.1016/j.jeurceramsoc.2008.05.037 ↗
18. 10.1016/0022-5088(71)90091-910.1016/0022-5088(71)90091-9 ↗
19. 10.4416/JCST2011-0004910.4416/JCST2011-00049 ↗
20. 10.1007/s11663-021-02061-510.1007/s11663-021-02061-5 ↗
21. 10.1007/s11167-005-0487-510.1007/s11167-005-0487-5 ↗
22. 10.1103/PhysRevMaterials.4.07440110.1103/PhysRevMaterials.4.074401 ↗
23. 10.1016/j.jpcs.2018.12.02910.1016/j.jpcs.2018.12.029 ↗
24. 10.1016/0022-4596(89)90101-110.1016/0022-4596(89)90101-1 ↗
25. Rigaku O. D. · 2015
26. 10.1107/S002188980804272610.1107/S0021889808042726 ↗
27. 10.1107/S205327331402637010.1107/S2053273314026370 ↗
28. Putz, H.; Brandenburg, K. Diamond - Crystal and Molecular Structure Visualization; Crystal Impact.1996.
29. 10.1016/0921-4526(93)90108-I10.1016/0921-4526(93)90108-I ↗
30. Goldberg D. · Rev. Int. Hautes. Temp. Refract. · 1968 · 5 · 181
31. The melting point of K1.8Ti2(PO4)3 was determined during a Laser-Heating Floating Zone Growth Process. During the growth, the temperature is measured by Infrared camera and liquid K1.8Ti2(PO4)3 was observed from 1250°C.
32. Dhanaraj G. · 201010.1007/978-3-540-74761-1 ↗
33. 10.1002/anie.20221578210.1002/anie.202215782 ↗
34. 10.1107/S056773947600155110.1107/S0567739476001551 ↗